Simple Processing of ZnO from Solution: Homoepitaxial Film and Bulk Single Crystal
Source abstract
Abstract
The system LiCl−ZnCl 2 −K 2 CO 3 is employed to fabricate homoepitaxial (0001) ZnO films by liquid phase epitaxy (LPE). The effect of ZnO concentration in the solution on the microstructure of the film is analyzed. Transition of growth modes was observed, evolving from island growth at <2 mmol of ZnO per 1 mol of LiCl over columnar growth (free-standing columns at 2.5 ± 0.5 mmol, porous film at 3.5 ± 0.5 mmol, and fully coalesced film at 5 mmol of ZnO) to step-flow growth at 12 ± 0.5 mmol of ZnO. Single-crystalline films, X-ray full-width half-maximum (FWHM) of 25 arcsec for (0002) reflection, with steps propagating over macroscopic dimensions were fabricated in the concentration range 12.5−14 mmol of ZnO. A structural quality factor (SQF) was introduced for joint description of both surface roughness and X-ray crystallinity. SQF is highest for films grown at 13 mmol of ZnO. Doping with bi-, tri- and tetravalent cationic additives yields ZnO films, the luminescent characteristics of which are investigated in comparison to low-alkaline hydrothermal ZnO. Hydrothermal synthesis under subcritical conditions at ≤150 °C has been investigated as a fast tool for doping of thermodynamically stable ZnO. Low-temperature luminescence is compared to hydrothermal bulk ZnO crystal grown under supercritical conditions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: ZnO doping and properties · Ga2O3 and related materials · Copper-based nanomaterials and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Multidisciplinary Research for Advanced Materials, Tohoku University, 2-1-1 Katahira, Aoba-ku, Sendai 980-8577, Japan, Mitsubishi Gas Chemical Co., Inc., 6-1-1 Niijuku, Katsushika-ku, Tokyo 125-0051, Japan, Murata Mfg. Co., Ltd., 2-26-10 Tenjin, Nagaokakyo, Kyoto 617-8555, Japan, Department of Geology, University of Mysore, Manasagangothri, Mysore 570 006, India, Center for Interdisciplinary Research, Tohoku University, Aramaki aza Aoba 6-3, Aoba-ku, Sendai 980-8578, Japan, and Rigaku Corp.,...
References (29)
Show source-provided references
1. Zu P. · Solid State Commun. · 1997 · 103 · 45910.1016/S0038-1098(97)00216-0 ↗
2. Tsukazaki A. · Nat. Mater. · 2005 · 4 · 4210.1038/nmat1284 ↗
3. Pearton S. J. · Prog. Mater. Sci. · 2005 · 50 · 29310.1016/j.pmatsci.2004.04.001 ↗
4. Dietl T. · Science (Washington, DC) · 2000 · 287 · 101910.1126/science.287.5455.1019 ↗
5. Simpson P. J. · Nucl. Instrum. Methods Phys. Res., Sect. A · 2003 · 505 · 8210.1016/S0168-9002(03)01025-8 ↗
6. Kadota M. · Jpn. J. Appl. Phys., Part 1 · 1992 · 11 · 301310.1143/JJAP.31.3013 ↗
7. Ballato A. · Proc. IEEE Int. Freq. Control Symp. · 1994 · 22
8. Yoshimura M. · MRS Bull. · 2000 · 25 · 1710.1557/mrs2000.175 ↗
9. Byrappa K. · Prog. Cryst. Growth Charact. Mater. · 2007 · 53 · 11710.1016/j.pcrysgrow.2007.04.001 ↗
10. Ehrentraut D. · J. Cryst. Growth · 2006 · 287 · 36710.1016/j.jcrysgro.2005.11.046 ↗
11. Sato H. · Jpn. J. Appl. Phys., Part 1 · 2006 · 45 · 19010.1143/JJAP.45.190 ↗
12. Schmidt O. · Appl. Phys. A: Mater. Sci. Process. · 2007 · 88 · 7110.1007/s00339-007-3949-1 ↗
13. Kaiya K. · Chem. Mater. · 2001 · 13 · 195210.1021/cm0006594 ↗
14. Stringfellow G. B. · J. Cryst. Growth · 1991 · 115 · 110.1016/0022-0248(91)90706-B ↗
15. Scheel H. J. · Appl. Phys. Lett. · 1994 · 65 · 90110.1063/1.112195 ↗
16. Chernov A. A. · J. Cryst. Growth · 1995 · 149 · 18710.1016/0022-0248(95)00014-3 ↗
17. Scheel H. J. · Appl. Phys. Lett. · 1980 · 37 · 7010.1063/1.91705 ↗
18. Sato H. · J. Electrochem. Soc. · 2007 · 154 · H14210.1149/1.2409483 ↗
19. Ohshima E. · J. Cryst. Growth · 2004 · 260 · 16610.1016/j.jcrysgro.2003.08.019 ↗
20. Communication with.Ohtomo, A.; Tsukazaki, A. (0002) FWHM ≈30 arcsec and RMS ≈0.15 nm for best films grown at 900−1000 °C at a growth rate of 3 nm min−1by L-MBE on ScAlMgO4substrate with an Mg0.15Zn0.85O buffer layer. The buffer layer required annealing around 650 °C prior deposition of the ZnO film.
21. Ehrentraut D. · J. Mater. Chem. · 2006 · 16 · 336910.1039/b608023e ↗
22. Romanyuk Y. E. · J. Cryst. Growth · 2004 · 269 · 37710.1016/j.jcrysgro.2004.05.049 ↗
23. Ehrentraut D. · Prog. Cryst. Growth Charact. Mater. · 2006 · 52 · 28010.1016/j.pcrysgrow.2006.09.002 ↗
24. Kawaguchi T. · J. Cryst. Growth · 1995 · 152 · 8710.1016/0022-0248(95)00081-X ↗
25. In doped ZnO bulk crystal was grown under similar conditions to the ZnO substrates reported in ref19. The source for the In dopant was In2O3.
26. von Wenckstern H. · Appl. Phys. Lett. · 2007 · 91 · 02291310.1063/1.2757097 ↗
27. Meyer B. K. · Phys. Status Solidi B · 2004 · 241 · 23110.1002/pssb.200301962 ↗
28. Measured at spots where the In doped ZnO crystal from the (0001) and (0001̅) faces grew together. Since the growth of In doped ZnO into the ⟨0001⟩ direction is very much reduced to the favor of the growth toward the ⟨101̅0⟩ direction, this sample practically demonstrates a free-standing, In doped ZnO crystal.
29. Byrappa, K.,unpublished.