journal article·2023-10-26Open access

Grain Boundary Wetting Transition in the Mg-Based ZEK 100 Alloy

Boris Straumal, Natalya Khrapova, Aleksandr Druzhinin, Kristina Tsoy, Gregory Davdian, Valery Orlov, Gregory Gerstein, Alexander Straumal

Crystals· Volume 13· Issue 11

Abstract

Modern magnesium-based alloys are broadly used in various industries as well as for biodegradable medical implants due to their exceptional combination of light weight, strength, and plasticity. The studied ZEK100 alloy had a nominal composition of 1 wt.% zinc, 0.1 wt.% zirconium, and 0.1 wt.% rare earth metals (REMs) such as Y, Ce, Nd, and La, with the remainder being Mg. It has been observed that between the solidus (Ts = 529.5 ± 0.5 °C) and liquidus temperature (Tl = 645 ± 5 °C), the Mg/Mg grain boundaries can contain either the droplets of a melt (incomplete or partial wetting) or the continuous liquid layers separating the abutting Mg grains (complete wetting). With the temperature increasing from Ts to Tl, the transformation proceeds from incomplete to complete grain boundary wetting. Below 565 °C, all grain boundaries are partially wetted by the melt. Above 565 °C, the completely wetted Mg/Mg grain boundaries appear. Their portion grows quickly with an increasing temperature until reaching 100% at 622 °C. Above 622 °C, all the solid Mg grains are completely surrounded by the melt. After rapid solidification, the REM-rich melt forms brittle intermetallic compounds. The compression strength as well as the compression yield strength parameter σ02 strongly depend on the morphology of the grain boundary layers. If the hard and brittle intermetallic phase has the shape of separated particles (partial wetting), the overall compression strength is about 341 MPa and σ02 = 101 MPa. If the polycrystal contains the continous intergarnular layers of the brittle intermetallic phase (complete wetting), the overall compression strength drops to 247 Mpa and σ02 to 40 Mpa. We for the first time observed, therefore, that the grain boundary wetting phenomena can strongly influence the mechanical properties of a polycrystal. Therefore, grain boundary wetting can be used for tailoring the behavior of materials.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Osipyan Institute of Solid State Physics, The Russian Academy of Sciences, Ac. Osipyan Str. 2, 142432 Chernogolovka, Russia

Department of Physical Chemistry, National University of Science and Technology MISiS, Leninskiy Ave. 4, 119049 Moscow, Russia

Institute for Material Science, Leibniz Universität Hannover, An der Universität 2, 30823 Garbsen, Germany

Department of Materials for Agrotechnology, Cotton Breeding, Seed Production and Agrotechnologies Research Institute, University Str. 3, Salar, Tashkent 702147, Uzbekistan

References (100+)

Show source-provided references
1. Improvement of Strength and Ductility of an EZ Magnesium Alloy by Applying Two Different ECAP Concepts to Processable Initial States10.1016/j.msea.2018.09.070 ↗
2. Effect of High-Pressure Torsion on Grain Refinement, Strength Enhancement and Uniform Ductility of EZ Magnesium Alloy10.1016/j.matlet.2017.10.113 ↗
3. Grain Boundary Wetting and Material Performance in an Industrial EZ33a Mg Cast Alloy10.24425/amm.2019.129463 ↗
4. Straumal, A., Mazilkin, I., Tzoy, K., Straumal, B., Bryła, K., Baranchikov, A., and Eggeler, G. (2020). Bulk and Surface Low Temperature Phase Transitions in the Mg-Alloy EZ33A. Metals, 10.10.3390/met10091127 ↗
5. Designing a Magnesium Alloy with High Strength and High Formability10.1038/s41467-018-04981-4 ↗
6. Oshida, Y. (2021). Magnesium Materials. From Mountain Bikes to Degradable Bone Grafts, De Gruyter Publishing.10.1515/9783110676945 ↗
7. Atrens, A., Dietzel, W., Srinivasan, P.B., Winzer, N., and Kannan, M.B. (2011). Stress Corrosion Cracking: Theory and Practice, Woodhead Publishing.
8. In Vitro and In Vivo Degradation Behavior of Mg-0.45Zn-0.45Ca (ZX00) Screws for Orthopedic Applications
9. The Strain Rate Sensitive and Anisotropic Behavior of Rare-Earth Magnesium Alloy ZEK100 Sheet10.1016/j.jma.2021.06.010 ↗
10. Sheet Texture Modification in Magnesium-Based Alloys by Selective Rare Earth Alloying10.1016/j.msea.2011.01.080 ↗
11. Patel, M., Paudel, Y., Mujahid, S., Rhee, H., and El Kadiri, H. (2023). Self-Consistent Crystal Plasticity Modeling of Slip-Twin Interactions in Mg Alloys. Crystals, 13.10.3390/cryst13040653 ↗
12. Effect of Bending and Tension Deformation on the Texture Evolution and Stretch Formability of Mg–Zn–RE–Zr Alloy10.1007/s12613-021-2398-8 ↗
13. The Influence of Strain Path on Rare Earth Recrystallization Textures in a Magnesium-Zinc-Rare Earth Alloy10.1007/s11661-017-4404-3 ↗
14. Anisotropy, Tension-Compression Asymmetry and Texture Evolution of a Rare-Earth-Containing Magnesium Alloy Sheet, ZEK100, at Different Strain Rates and Temperatures: Experiments and Modeling10.1016/j.ijplas.2017.04.006 ↗
15. A Reduced-Order Crystal Model for HCP Metals: Application to Mg10.1016/j.mechmat.2016.04.009 ↗
16. Characterization of Heat Transfer Coefficient for Non-isothermal Elevated Temperature Forming of Metal Alloys10.1007/s12289-019-01478-3 ↗
17. Warm and Hot Deformation Behavior of As-delivered ZEK100 Magnesium Alloy10.1007/s11340-015-0094-1 ↗
18. Experimental Fracture Characterisation of an Anisotropic Magnesium Alloy Sheet in Proportional and Non-proportional Loading Conditions10.1016/j.ijsolstr.2018.04.010 ↗
19. Fracture Characterization of Rolled Sheet Alloys in Shear Loading: Studies of Specimen Geometry, Anisotropy, and Rate Sensitivity10.1007/s11340-016-0211-9 ↗
20. The Effect of Microstructure on Damage and Fracture in AZ31B and ZEK100 Magnesium Alloys10.1016/j.msea.2016.01.103 ↗
21. Improving the Corrosion Resistance of ZEK100 Magnesium Alloy by Combining High-pressure Torsion Technology with Hydroxyapatite Coating10.1016/j.matdes.2019.107933 ↗
22. Spatio-temporal Characteristics of Propagative Plastic Instabilities in a Rare Earth Containing Magnesium Alloy10.1016/j.ijplas.2014.02.004 ↗
23. Effects of Calcium and Rare-earth Elements on the Microstructure and Tension–Compression Yield Asymmetry of ZEK100 Alloy10.1016/j.msea.2014.09.023 ↗
24. A Constitutive Law for the Thermo-mechanical Modelling of Magnesium Alloy Extrusion10.1007/s12289-011-1055-6 ↗
25. On the Effect of the Extrusion Speed on Microstructure and Plastic Deformation of ZE10 and ZEK100 Magnesium Alloys—An Acoustic Emission Study10.12693/APhysPolA.122.593 ↗
26. Effect of Hot Rolling on Microstructure and Properties of the ZEK100 Alloy10.1016/j.jma.2019.02.001 ↗
27. Warm Forming Limits of Rare Earth-magnesium Alloy ZEK100 Sheet10.1007/s12289-015-1267-2 ↗
28. Applications of Neuber’s and Glinka’s Notch Plasticity Correction Rules to Asymmetric Magnesium Alloys Under Cyclic Load10.1016/j.tafmec.2019.102431 ↗
29. Fatigue of ZEK100-F Magnesium Alloy: Characterisation and Modelling10.1016/j.ijfatigue.2019.04.001 ↗
30. Pseudoelastic and Corrosion Behaviors of Mg ZEK100 Alloy under Cyclic Loading10.1016/j.ijfatigue.2017.06.028 ↗
31. Cyclic Deformation and Anelastic Behavior of ZEK100 Magnesium Alloy: Effect of Strain Ratio10.1016/j.msea.2015.05.110 ↗
32. Strain-controlled Low Cycle Fatigue Properties of a Rare-earth Containing ZEK100 Magnesium Alloy10.1016/j.matdes.2014.11.058 ↗
33. Anelastic Behavior and Phenomenological Modeling of Mg ZEK100-O Alloy Sheet under Cyclic Tensile Loading–Unloading10.1016/j.msea.2012.11.009 ↗
34. Three-point Bending Behavior of a ZEK100 Mg Alloy at Room Temperature10.1016/j.msea.2013.10.030 ↗
35. Evaluation of the VDA 238–100 Tight Radius Bend Test for Plane Strain Fracture Characterization of Automotive Sheet Metals10.1007/s11340-020-00597-2 ↗
36. Characterization and Modeling of {1012} Twin Banding in Magnesium10.1016/j.actamat.2019.11.020 ↗
37. Forming Limits of Mg alloy ZEK100 Sheet in Preform Annealing Process10.1016/j.matdes.2013.07.082 ↗
38. Analytical Method for Forming Limit Diagram Prediction with Application to a Magnesium ZEK100-O Alloy10.1007/s11665-013-0582-3 ↗
39. Forming-Limit Diagrams for Magnesium AZ31B and ZEK100 Alloy Sheets at Elevated Temperatures10.1007/s11665-013-0623-y ↗
40. Temperature-Dependent Constitutive Modeling of a Magnesium Alloy ZEK100 Sheet Using Crystal Plasticity Models Combined with In Situ High-Energy X-ray Diffraction Experiment10.1016/j.jma.2021.09.007 ↗
41. Multi-Island Genetic-Algorithm-Based Approach to Uniquely Calibrate Polycrystal Plasticity Models for Magnesium Alloys10.1007/s11837-021-04614-0 ↗
42. Mechanism-Based Constitutive Modeling of ZEK100 Magnesium Alloy with Crystal Plasticity and In-Situ HEXRD Experiment10.1016/j.ijplas.2018.09.005 ↗
43. Abedini, A., Butcher, C., and Worswick, M.J. (2018). Application of an Evolving Non-Associative Anisotropic-Asymmetric Plasticity Model for a Rare-Earth Magnesium Alloy. Metals, 8.10.3390/met8121013 ↗
44. Thermodynamically-Consistent Constitutive Modeling of Hardening Asymmetry Including Isotropic Ductile Damage for Mg Alloys10.1016/j.euromechsol.2018.08.002 ↗
45. Constitutive Characterization of a Rare-Earth Magnesium Alloy Sheet (ZEK100-O) in Shear Loading: Studies of Anisotropy and Rate Sensitivity10.1016/j.ijmecsci.2017.04.013 ↗
46. An Elasto-Plastic Constitutive Model for Evolving Asymmetric/anisotropic Hardening Behavior of AZ31B and ZEK100 Magnesium Alloy Sheets Considering Monotonic and Reverse Loading Paths10.1016/j.ijplas.2015.03.004 ↗
47. Sharma, S.K., Saxena, K.K., Malik, V., Mohammed, K.A., Prakash, C., Buddhi, D., and Dixit, S. (2022). Significance of Alloying Elements on the Mechanical Characteristics of Mg-Based Materials for Biomedical Applications. Crystals, 12.10.3390/cryst12081138 ↗
48. In Vitro and in Vivo Degradation and Mechanical Properties of ZEK100 Magnesium Alloy Coated with Alginate, Chitosan and Mechano-growth Factor10.1016/j.msec.2016.02.073 ↗
49. Degradation of Bioabsorbable Mg-Based Alloys: Assessment of the Effects of Insoluble Corrosion Products and Joint Effects of Alloying Components on Mammalian Cells10.1016/j.msec.2015.08.043 ↗
50. Reifenrath, J., Marten, A.-K., Angrisani, N., Eifler, R., and Weizbauer, A. (2015). In Vitro and In Vivo Corrosion of the Novel Magnesium Alloy Mg–La–Nd–Zr: Influence of the Measurement Technique and in vivo Implant Location. Biomed. Mater., 10.10.1088/1748-6041/10/4/045021 ↗
51. Biodegradable Behaviour and Fatigue Life of ZEK100 Magnesium Alloy in Simulated Physiological Environment10.1111/ffe.12262 ↗
52. Magnesium-based Bone Implants: Immunohistochemical Inalysis of Peri-implant Osteogenesis by Evaluation of Osteopontin and Osteocalcin Expression10.1002/jbm.a.34828 ↗
53. Comparative in vitro Study and Biomechanical Testing of Two Different Magnesium Alloys10.1177/0885328213506758 ↗
54. Long-term in vivo Degradation Behaviour and Biocompatibility of the Magnesium Alloy ZEK100 for use as a Biodegradable Bone Implant10.1016/j.actbio.2012.08.028 ↗
55. Reifenrath, J., Angrisani, N., Erdmann, N., Lucas, A., Waizy, H., Seitz, J.M., Bondarenko, A., and Meyer-Lindenberg, A. (2013). Degrading Magnesium Screws ZEK100: Biomechanical Testing, Degradation Analysis and Soft-tissue Biocompatibility in a Rabbit Model. Biomed. Mater., 8.10.1088/1748-6041/8/4/045012 ↗
56. Bauer, M., Biskup, C., Schilling, T., Haverich, A., Bach, F.W., Maier, H.J., and Hassel, T. (2013). Influence of Shot Peening on Surface Rougness and in vitro Load Cycles of Magnesium Alloys. Biomed. Tech., 58.10.1515/bmt-2013-4060 ↗
57. Weidling, M., Besdo, S., Schilling, T., Bauer, M., Hassel, T., Haverich, A., and Wriggers, P. (2013). Finite Element Simulation of Myocardial Stabilising Structures and Development of New Designs. Biomed. Tech., 58.10.1515/bmt-2013-4061 ↗
58. Phantomuntersuchungen an einem Hochauflösenden CT zur Ex-vivo-Darstellung von Degradierbaren Magnesiumimplantaten und Simulierten Periimplantären Knochenschichten in Kaninchentibiae10.1055/s-0031-1299293 ↗
59. In Vivo Corrosion of Two Novel Magnesium Alloys ZEK100 and AX30 and Their Mechanical Suitability as Biodegradable Implants10.3390/ma4061144 ↗
60. Huehnerschulte, T.A., Reifenrath, J., von Rechenberg, B., Dziuba, D., Seitz, J.M., Bormann, D., Windhagen, H., and Meyer-Lindenberg, A. (2012). In Vivo Assessment of the Host Reactions to the Biodegradation of the Two Novel Magnesium Alloys ZEK100 and AX30 in an Animal Model. BioMed. Eng. OnLine, 11.10.1186/1475-925X-11-14 ↗
61. The Manufacture of Resorbable Suture Material from Magnesium—Drawing and Stranding of Thin Wires10.1002/adem.201100152 ↗
62. The Manufacture of Resorbable Suture Material from Magnesium10.1002/adem.201000191 ↗
63. Corrosion Inhibition of Mg Alloy ZEK100 Sheet Metal by Dissolved Lithium Carbonate10.1149/1945-7111/ac1cc5 ↗
64. Temporal Evolution of Corrosion Film Nano-Porosity and Magnesium Alloy Hydrogen Penetration in NaCl Solution10.1149/1945-7111/abbdd0 ↗
65. Magnesium Alloy Effects on Plasma Electrolytic Oxidation Electro-Ceramic and Electro-Coat Formation and Corrosion Resistance10.1149/2.0531914jes ↗
66. Physical and Electrochemical Evidence for the Role of a Mg Hydride Species in Mg Alloy Corrosion10.5006/2918 ↗
67. Advanced Characterization Study of Commercial Conversion and Electrocoating Structures on Magnesium Alloys AZ31B and ZE10A10.1016/j.surfcoat.2016.03.066 ↗
68. Determination of the Local Corrosion Rate of Magnesium Alloys Using a Shear Force Mounted Scanning Microcapillary Method10.1039/C4FD00276H ↗
69. The Influence of Microstructure on the Corrosion of Magnesium Alloy ZEK10010.5006/1387 ↗
70. Waizy, H., Weizbauer, A., Modrejewski, C., Witte, F., Windhagen, H., Lucas, A., Kieke, M., Denken, B., Behrens, P., and Meyer-Lindenberg, A. (2012). In Vitro Corrosion of ZEK100 Plates in Hank’s Balanced Salt Solution. BioMed. Eng. OnLine, 11.10.1186/1475-925X-11-12 ↗
71. Geometric Adaption of Resorbable Myocardial Stabilizing Structures Based on the Magnesium Alloys LA63 and ZEK100 for the Support of Myocardial Grafts on the Left Ventricle10.1515/bmt-2012-4214 ↗
72. Ratcheting Behavior of ZEK100 Magnesium Alloy with Various Loading Conditions and Different Immersing Time10.1557/jmr.2017.104 ↗
73. Strong and Tough Magnesium Wire Reinforced Phosphate Cement Composites for Load-bearing Bone Replacement10.1016/j.jmbbm.2012.12.012 ↗
74. Microstructure and Mechanical Properties of Mg-to-Al Dissimilar Welded Joints with an Ag Interlayer using Ultrasonic Spot Welding10.1016/j.jma.2020.04.001 ↗
75. Ultrasonic Spot Welding of a Rare-Earth Containing ZEK100 Magnesium Alloy: Effect of Welding Energy10.1007/s11661-016-3355-4 ↗
76. Microstructures and Properties of Mg alloy/DP600 Steel Dissimilar Refill Friction Stir Spot Welds10.1179/1362171815Y.0000000033 ↗
77. Microstructure, Texture, and Mechanical Properties of Friction Stir Spot Welded Rare-Earth Containing ZEK100 Magnesium Alloy Sheets10.1016/j.msea.2014.09.010 ↗
78. Ultrasonic Spot Welding of Magnesium-to-Aluminum Alloys with a Copper Interlayer: Microstructural Evolution and Tensile Properties10.1016/j.jmapro.2018.11.008 ↗
79. Peng, H., Jiang, X., Bai, X., Li, D., and Chen, D. (2018). Microstructure and Mechanical Properties of Ultrasonic Spot Welded Mg/Al Alloy Dissimilar Joints. Metals, 8.10.3390/met8040229 ↗
80. Ultrasonic Spot Welding of Rare-Earth Containing ZEK100 Magnesium Alloy to 5754 Aluminum Alloy10.1016/j.msea.2016.04.060 ↗
81. Microstructure and Texture Evolution of Magnesium Alloys During Electropulse Treatment10.1007/s11661-014-2735-x ↗
82. Laser Welding/Brazing of 5182 Aluminium Alloy to ZEK100 Magnesium Alloy Using a Nickel Interlayer10.1080/13621718.2018.1425182 ↗
83. Influence of Ni Interlayer Width on Interfacial Reactions and Mechanical Properties in Laser Welding/Brazing of Al/Mg Lap Joint10.1080/13621718.2019.1607487 ↗
84. Critical Point Wetting10.1063/1.434402 ↗
85. New Phase-Transition Phenomena in Thin Argon Films10.1103/PhysRevLett.38.1486 ↗
86. Faceting of Σ3 and Σ9 grain boundaries in copper10.1023/A:1015174921561 ↗
87. Transformation of Σ17 special tilt boundaries to general boundaries in tin10.1016/0001-6160(88)90225-8 ↗
88. Experimental and Theoretical Constraints on Melt Distribution in Crustal Sources: The Effect of Crystalline Anisotropy on Melt Interconnectivity10.1016/0009-2541(95)00052-N ↗
89. Wetting and premelting phase transitions in 38° [100] tilt grain boundaries in (Fe–12at.%Si) Zn alloy in the vicinity of the A2–B2 bulk ordering in Fe–12at.%Si alloy10.1016/0956-7151(91)90042-Y ↗
90. Grain boundary segregation in the Cu–Bi system10.4028/www.scientific.net/DDF.156.135 ↗
91. Observation of Short-Range Critical Wetting10.1038/23425 ↗
92. Tie lines of the grain boundary wetting phase transition in the Zn-rich part of the Zn–Sn phase diagram
93. Grain Boundaries: Phase Transitions and Critical Phenomena10.1142/S0217979291001176 ↗
94. Review: Liquid Phase Sintering10.1007/s10853-008-3008-0 ↗
95. Pressure influence on the grain boundary wetting phase transition in Fe–Si alloys10.1016/S1359-6454(96)00332-1 ↗
96. “Wetting” Phase Transitions by the Second Solid Phase for Linear Defects (Grain Boundary Triple Junctions)10.1134/S0021364020160031 ↗
97. Apparently Complete Grain Boundary Wetting in Cu–In Alloys10.1007/s10853-012-6773-8 ↗
98. Grain Boundary Transition Associated Intergranular Failure Analysis at TMAZ/SZ Interface of Dissimilar AA7475-AA2198 Joints by Friction Stir Welding10.1016/j.matlet.2020.128557 ↗
99. Jandaghi, M.R., Pouraliakbar, H., Saboori, A., Hong, S.I., and Pavese, M. (2021). Comparative Insight into the Interfacial Phase Evolutions during Solution Treatment of Dissimilar Friction Stir Welded AA2198-AA7475 and AA2198-AA6013 Aluminum Sheets. Materials, 14.10.3390/ma14051290 ↗
100. The Effect of Pressure on Migration of the [001] Tilt Grain Boundaries in the Tin Bicrystals10.1016/0036-9748(84)90509-X ↗