journal article·2025-09-30Open access

Investigation of Process and Properties of Cu-Mn-Al Alloy Cladding Deposited on 27SiMn Steel via Cold Metal Transfer

Jin Peng, Shihua Xie, Junhai Xia, Xingxing Wang, Zenglei Ni, Pei Wang, Nannan Chen

Crystals· Volume 15· Issue 10

Abstract

This study systematically investigates the effects of welding current on the macro-morphology, microstructure, mechanical properties, and corrosion resistance of Cu-Mn-Al alloy coatings deposited on 27SiMn steel substrates using Cold Metal Transfer (CMT) technology. The 27SiMn steel is widely applied in coal mining, geology, and engineering equipment due to its high strength and toughness, but its poor corrosion and wear resistance significantly limits service life. To address this issue, a Cu-Mn-Al alloy (high-manganese aluminum bronze) was selected as a cladding material because of its superior combination of mechanical strength, toughness, and excellent corrosion resistance in saline and marine environments. Compared with conventional cladding processes, CMT technology enables low-heat-input deposition, reduces dilution from the substrate, and promotes defect-free coating formation. To the best of our knowledge, this is the first report on the fabrication of Cu-Mn-Al coatings on 27SiMn steel using CMT, aiming to optimize process parameters and establish the relationship between welding current, phase evolution, and coating performance. The experimental results demonstrate that the cladding layer width increases progressively with welding current, whereas the layer height remains relatively stable at approximately 3 mm. At welding currents of 120 A and 150 A, the cladding layer primarily consists of α-Cu, κII, β-Cu3Al, and α-Cu + κIII phases. At higher welding currents (180 A and 210 A), the α-Cu + κIII phase disappears, accompanied by the formation of petal-shaped κI phase. The peak shear strength (509.49 MPa) is achieved at 120 A, while the maximum average hardness (253 HV) is obtained at 150 A. The 120 A cladding layer demonstrates optimal corrosion resistance. These findings provide new insights into the application of CMT in fabricating Cu-Mn-Al protective coatings on steel and offer theoretical guidance for extending the service life of 27SiMn steel components in aggressive environments.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metallurgy and Material Science · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, North China University of Water Resources and Electric Power, Zhengzhou 450045, China

Henan Engineering Research Center on Special Materials and Applications of Water Conservancy and Hydropower Engineering, Zhengzhou 450045, China

Henan Key Laboratory of High Performance Carbon Fiber Reinforced Composites, Institute of Carbon Matrix Composites, Henan Academy of Sciences, Zhengzhou 450046, China

School of Materials Science and Engineering, Shanghai Jiao Tong University, No. 800, Dong Chuan Road, Shanghai 200240, China

Funding

Key Scientific Research Projects of Higher Education Institutions in Henan Province · Key R & D and Promotion Project of the Henan Province

References (35)

Show source-provided references
1. 316L Stainless Steel Repaired Layers by Weld Surfacing and Laser Cladding on a 27SiMn Steel: A Comparative Study of Microstructures, Corrosion, Hardness and Wear Performances10.1016/j.jmrt.2023.01.162 ↗
2. Lu, X., Zhang, Z., Lv, M., Li, X., Song, B., and Fang, M. (2022). Evolution of Non-Metallic Inclusions in 27SiMn Steel. Metals, 12.10.3390/met12050718 ↗
3. Industrial Experiment of the Online Accelerated Cooling for 27SiMn Seamless Steel Pipe10.1002/srin.202400822 ↗
4. Study on Dynamic Solidification Characteristics and Microstructure of Laser Cladded Coatings on the Surface of 27SiMn Alloy Structural Steel10.1016/j.mtcomm.2025.112309 ↗
5. Elucidation of Dissimilar Material Joining Phenomena on Steel and Aluminum Alloy Using Hot-Wire Laser Brazing10.1007/s40194-023-01667-4 ↗
6. High-Speed Laser Surface Structuring for Thermal Spray Coating Preparation10.1002/pssa.202300710 ↗
7. Microstructure and Properties of Ni-ZrB2; Gradient Composite Coating on the 27SiMn Steel Surface by Laser Cladding10.1016/j.mtcomm.2025.111657 ↗
8. Hardfacing Using Ferro-Alloy Powder Mixtures by Submerged Arc Welding10.1016/j.surfcoat.2014.08.076 ↗
9. A Novel Amorphous Alloy Coating for Elevating Corrosion Resistance of X70 Pipeline Steel10.1007/s11666-024-01778-4 ↗
10. Ding, Y., Bi, W., Zhong, C., Wu, T., and Gui, W. (2022). A Comparative Study on Microstructure and Properties of Ultra-High-Speed Laser Cladding and Traditional Laser Cladding of Inconel625 Coatings. Materials, 15.10.3390/ma15186400 ↗
11. Al-Si-Mn Alloy Coating on Aluminum Substrate Using Cold Metal Transfer (CMT) Welding Technique10.1007/s11837-014-0970-7 ↗
12. Recent Developments in Cladding and Coating Using Cold Metal Transfer Technology10.1007/s11665-023-08940-z ↗
13. A Review on Wire Arc Additive Manufacturing Based on Cold Metal Transfer10.1080/10426914.2024.2323441 ↗
14. Comprehensive Analysis of Experimental Studies in Cold Metal Transfer Welding10.1007/s42452-025-07065-3 ↗
15. Cold Metal Transfer (CMT) Technology—An Overview10.1016/j.dt.2017.08.002 ↗
16. Cold Metal Transfer Technology—A Review of Recent Research Developments10.1016/j.rineng.2024.102423 ↗
17. Sliding Wear Behavior of Cold Metal Transfer Cladded Stellite 12 Hardfacings on Martensitic Stainless Steel10.1007/s40194-022-01390-6 ↗
18. Enhancing Corrosion Resistance of AZ31B Magnesium Alloy Substrate in 3.5% NaCl Solution with Al-Si Coating Prepared by Cold Metal Transfer-Based Wire Arc Additive Manufacturing10.1016/j.ijoes.2024.100763 ↗
19. Microstructural Evolution and Mechanical Properties of Ti Alloy/Stainless Steel Lap Joints during Cold Metal Transfer Technique with CuSi3 Filler Wire10.1007/s11665-020-05053-9 ↗
20. Comparative Study on Microstructure and Oxidation Resistance of Inconel 625 Superalloy Coatings on 12CrMoV Steel Surfaces Prepared by CMT and MIG Cladding10.1016/j.jmrt.2024.01.293 ↗
21. Cavitation Erosion and Corrosion Behavior of Copper–Manganese–Aluminum Alloy Weldment10.1016/j.msea.2004.04.032 ↗
22. Effect of Filler Metal on Microstructure and Mechanical Properties of Manganese–Aluminum Bronze Repair Welds10.1016/S1003-6326(17)60057-8 ↗
23. Nickel-Aluminum Bronze (NAB) Alloy Design under Two-Steps Casting and Submerged Friction Stir Processing10.1016/j.msea.2023.145960 ↗
24. Micro- and Nanostructural Evolution of Copper Bronze CuAl10Ni5Fe5 during Cooling from Solution Treatments10.1016/j.matchar.2025.114795 ↗
25. Microstructural Evolution and Mechanical Behavior of Nickel Aluminum Bronze Cu-9Al-4Fe-4Ni-1Mn Fabricated through Wire-Arc Additive Manufacturing
26. Microstructure and Corrosion Resistance of an Al-Bronze Coating Prepared by Cold Metal Transfer on 27SiMn Steel10.1016/j.surfcoat.2024.130493 ↗
27. Corrosion Behavior of Cu−Al−Mn−Zn−Zr Shape Memory Alloy in NaCl Solution10.1016/S1003-6326(21)65557-7 ↗
28. Mechanical, Friction and Wear Behaviors of a Novel High-Strength Wear-Resisting Aluminum Bronze10.1016/0043-1648(95)06890-2 ↗
29. Uncovering the Effects of Neutralizing Elements (Co, Mn and Cr) on the Fe-Rich Intermetallic Formation in Al-Si-Cu Alloys10.1016/j.msea.2022.144090 ↗
30. The Influence of Ultrasonic Vibration on Micro-Arc Oxidation Behaviour of Manganese Aluminium Bronze10.1016/j.jmrt.2024.09.038 ↗
31. Wire Arc Additive Manufactured CuMn13Al7 High-Manganese Aluminium Bronze10.1186/s10033-022-00716-1 ↗
32. Corrosion and Cavitation Erosion Behaviors of the Manganese-Aluminum-Bronze Cladding Layer Prepared by MIG in 3.5% NaCl Solution10.1016/j.mtcomm.2022.103566 ↗
33. Elucidating Different Selective Corrosion Behavior of Two Typical Marine Aluminum Bronze Alloys from the Perspective of Constituent Phases10.1016/j.corsci.2024.112167 ↗
34. Effects of Solder Dimension on the Interfacial Shear Strength and Fracture Behaviors of Cu/Sn–3Cu/Cu Joints10.1016/j.scriptamat.2012.07.024 ↗
35. Corrosion Behavior of Wire-Arc Additive Manufactured and as-Cast Ni-Al Bronze in 3.5 Wt% NaCl Solution10.1016/j.corsci.2023.111048 ↗