journal article·2013-07-17Open access

Corrosion Study and Intermetallics Formation in Gold and Copper Wire Bonding in Microelectronics Packaging

Chwee Goh, Wee Chong, Teck Lee, Christopher Breach

Crystals· Volume 3· Issue 3

Abstract

A comparison study on the reliability of gold (Au) and copper (Cu) wire bonding is conducted to determine their corrosion and oxidation behavior in different environmental conditions. The corrosion and oxidation behaviors of Au and Cu wire bonding are determined through soaking in sodium chloride (NaCl) solution and high temperature storage (HTS) at 175 °C, 200 °C and 225 °C. Galvanic corrosion is more intense in Cu wire bonding as compared to Au wire bonding in NaCl solution due to the minimal formation of intermetallics in the former. At all three HTS annealing temperatures, the rate of Cu-Al intermetallic formation is found to be three to five times slower than Au-Al intermetallics. The faster intermetallic growth rate and lower activation energy found in this work for both Au/Al and Cu/Al as compared to literature could be due to the thicker Al pad metallization which removed the rate-determining step in previous studies due to deficit in Al material.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Technical Education, 2 Ang Mo Kio Drive, 567720, Singapore

Promat Consultants, 160 Lentor Loop, #08-05, Tower 6, 789094, Singapore

References (19)

Show source-provided references
1. Harmon, G. (1997). Wire Bonding in Microelectronics: Materials, Processes, Reliability and Yield, McGraw-Hill. [2nd ed.].
2. England, L., and Jiang, T. (2007, January 29). Reliability of Cu Wire Bonding to Al Metallization. Proceedings of IEEE Electronic Component Technology Conference, Reno, NV, USA.10.1109/ECTC.2007.374009 ↗
3. Effects of Cu/Al intermetallic compound (IMC) on copper wire and aluninum pad bondability10.1109/TCAPT.2003.815121 ↗
4. Kurtz, J., Cousens, D., and Dufour, M. (1984, January 14–16). Copper wire ball bonding. Proceedings of the 34th Electron Component Conference, New Orleans, LA, USA.
5. Mori, S., Yoshida, H., and Uchiyama, N. (1988, January 9–11). The development of new copper ball bonding wire. Proceedings of the 38th Elentron Component Conference, Los Angeles, CA, USA.
6. Na, S.H., Hwang, T.Y., Park, J.S., Kim, J.Y., Yoo, H.Y., and Lee, C.H. (June, January 31). Characterization of intermetallic compound (IMC) growth in Cu wire ball bonding on Al pad metallization. Proceedings of the 61st Electronic Components and Technology Conference, Lake Buena Vista, FL, USA.
7. Grains, deformation substructures and slip bands observed in thermosonic copper ball bonding10.1016/S1044-5803(03)00102-5 ↗
8. Optimization of copper wire bonding on Al-Cu metallization10.1109/95.390327 ↗
9. Corrosion study at the Cu-Al interface in microelectronics packaging10.1016/S0169-4332(02)00150-2 ↗
10. Growth behaviour of Cu/Al intermetallic compounds and cracks in copper ball bonds during isothermal aging10.1016/j.microrel.2007.06.008 ↗
11. Lee, C.C., and Higgins, L.M. (2010, January 1–4). Challenges of Cu wire bonding on low-k/Cu wafers with BOA structures. Proceedings of the 60th Electronic Components and Technology Conference, Las Vega, NV, USA.
12. Boettcher, T., Rother, M., Liedtke, S., Ulrich, M., Bollmann, M., Pinkernelle, A., Gruber, D., Funke, H.-J., Kaiser, M., and Lee, K. (2010, January 8–10). On the intermetallic corrosion of Cu-Al wire bonds. Proceedings of the 12th Electronics Packaging Technology Conference, Singapore.10.1109/EPTC.2010.5702706 ↗
13. Facility for the Analysis of Chemical Thermodynamics. Available online:http://www.crct.polymtl.ca/factweb.php.
14. The chemical nature of Al corrosion—V. Energy transfer in Al dissolution10.1149/1.2123881 ↗
15. Beverskog, B., and Puigdomenech, I. SKI Rapport 98:19. Pourbaix diagrams for the system copper-chlorine at 5–100 °C. Available online:http://www.stralsakerhetsmyndigheten.se/global/ publikationer/ski_import/010803/04318226039/98-19.pdf.
16. Bromine and chlorine induced degradation of the Au–Al bonds10.1007/s11664-004-0112-z ↗
17. Schrapler, L., Muller, T., Knoll, H., and Petzold, M. (2006, January 5–7). Influence of intermetallic phases on bonding reliability in thermosonic Au–Al wire bonding. Proceedings of the 1st Electronic System Integration Technology Conference, Dresden, Germany.
18. A transmission electron microscopy study of intermetallic formation in Al-Cu thin film couples10.1016/0022-0248(80)90164-5 ↗
19. Thermal and ion beam induced thin film reactions in Cu-Al bilayers10.1016/0168-583X(92)95451-V ↗