journal article·2017-12-12Open access

Vickers Hardness of Diamond and cBN Single Crystals: AFM Approach

Sergey Dub, Petro Lytvyn, Viktor Strelchuk, Andrii Nikolenko, Yurii Stubrov, Igor Petrusha, Takashi Taniguchi, Sergey Ivakhnenko

Crystals· Volume 7· Issue 12

Abstract

Atomic force microscopy in different operation modes (topography, derivative topography, and phase contrast) was used to obtain 3D images of Vickers indents on the surface of diamond and cBN single crystals with high spatial resolution. Confocal Raman spectroscopy and Kelvin probe force microscopy were used to study the structure of the material in the indents. It was found that Vickers indents in diamond has no sharp and clear borders. However, the phase contrast operation mode of the AFM reveals a new viscoelastic phase in the indent in diamond. Raman spectroscopy and Kelvin probe force microscopy revealed that the new phase in the indent is disordered graphite, which was formed due to the pressure-induced phase transformation in the diamond during the hardness test. The projected contact area of the graphite layer in the indent allows us to measure the Vickers hardness of type-Ib synthetic diamond. In contrast to diamond, very high plasticity was observed for 0.5 N load indents on the (001) cBN single crystal face. Radial and ring cracks were absent, the shape of the indents was close to a square, and there were linear details in the indent, which looked like slip lines. The Vickers hardness of the (111) synthetic diamond and (111) and (001) cBN single crystals were determined using the AFM images and with account for the elastic deformation of the diamond Vickers indenter during the tests.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Force Microscopy Techniques and Applications · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute for Superhard Materials of NASU, 2 Avtozavodskaya Str., 04074 Kyiv, Ukraine

Institute of Semiconductor Physics of NASU, 41 Nauky Pr., 03028 Kyiv, Ukraine

National Institute for Materials Sciences, 1-1 Namiki, Tsukuba, Ibaraki 305-0044, Japan

References (46)

Show source-provided references
1. Hardness measurement of CVD diamond coatings on SiC substrates10.1016/j.surfcoat.2004.08.131 ↗
2. Materials: Ultrahard polycrystalline diamond from graphite10.1038/421599b ↗
3. Indentation hardness of nano-polycrystalline diamond prepared from graphite by direct conversion10.1016/j.diamond.2004.03.002 ↗
4. Mechanical properties of high purity polycrystalline cBN synthesized by direct conversion sintering method10.1023/A:1004780218732 ↗
5. Nanotwinned diamond with unprecedented hardness and stability10.1038/nature13381 ↗
6. Superhard nanocomposite of dense polymorphs of boron nitride: Noncarbon material has reached diamond hardness10.1063/1.2711277 ↗
7. Creation of nanostuctures by extreme conditions: High-pressure synthesis of ultrahard nanocrystalline cubic boron nitride10.1002/adma.201104361 ↗
8. Ultrahard nanotwinned cubic boron nitride10.1038/nature11728 ↗
9. Elasticity and hardness of nano-polycrystalline boron nitrides: The apparent Hall-Petch effect10.1063/1.4894377 ↗
10. Elastic and mechanical softening in boron-doped diamond10.1038/srep42921 ↗
11. Real indentation hardness of nano-polycrystalline cBN synthesized by direct conversion sintering under HPHT10.1016/j.diamond.2014.06.009 ↗
12. Ultrahardness: Measurement and enhancement10.1021/acs.jpcc.5b00017 ↗
13. Fracture of synthetic diamond10.1063/1.360060 ↗
14. Mechanical properties of cubic BC2N, a new superhard phase10.1016/S0925-9635(01)00513-1 ↗
15. Elastic moduli and hardness of cubic silicon nitride10.1111/j.1151-2916.2002.tb00044.x ↗
16. Mechanical properties of polycrystalline cBN obtained from pyrolytic gBN by direct transformation technique10.1080/08957950600764239 ↗
17. Theoretical shear strength and the onset of plasticity in nanodeformation of cubic boron nitride10.3103/S1063457617020034 ↗
18. Nanoindentation of diamond, graphite and fullerene films10.1016/S0925-9635(00)00188-6 ↗
19. Nanoindentation of natural diamond10.1080/01418610208235696 ↗
20. Superior wear resistance of aggregated diamond nanorods10.1021/nl0602084 ↗
21. Comparative nanoindentation of single crystals of hard and superhard oxides10.3103/S1063457614040017 ↗
22. Pressure-induced phase transformations in diamond10.1063/1.368198 ↗
23. Transformation of diamond to graphite10.1038/44323 ↗
24. Change of dislocations density in single crystals of various types diamonds depending on the growth temperature and rate10.15407/fm23.04.378 ↗
25. Large-volume high-pressure devices for physical investigations10.1070/PU2008v051n10ABEH006615 ↗
26. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
27. Fractured polymer/silica fiber surface studied by tapping mode atomic force microscopy10.1016/0039-6028(93)90582-5 ↗
28. Imaging viscoelasticity by force modulation with the atomic force microscope10.1016/S0006-3495(93)81433-4 ↗
29. Phase imaging and stiffness in tapping-mode atomic force microscopy10.1016/S0039-6028(96)01591-9 ↗
30. Kelvin probe force microscopy10.1063/1.105227 ↗
31. Effect of phase transformations on the shape of unloading curve in the nanoindentation of silicon10.1063/1.126300 ↗
32. Electron affinity and work function of differently oriented and doped diamond surfaces determined by photoelectron spectroscopy10.1016/S0039-6028(98)00718-3 ↗
33. Resistivity and electronic work function of very thin film carbon
34. Incipient plasticity of diamond during nanoindentation10.1039/C7RA05721K ↗
35. First-principles, UV Raman, X-ray diffraction and TEM study of the structure and lattice dynamics of the diamond—Lonsdaleite system10.1016/j.diamond.2011.05.013 ↗
36. Raman identification of lonsdaleite in Popigai impactites10.1002/jrs.4457 ↗
37. Shock induced splitting of the triply degenerate Raman line in diamond10.1103/PhysRevLett.71.3497 ↗
38. Raman spectra of shocked diamond single crystals10.1103/PhysRevB.66.014107 ↗
39. Fracture toughness of diamond single crystals
40. Mechanical properties of diamond at 1200 °C10.1016/0925-9635(94)90080-9 ↗
41. Identification of slip systems in cubic boron nitride10.1080/01418618308245250 ↗
42. Investigation of mechanical properties of high-hardness materials by indentation
43. The effect of the indenter load on the nanohardness of ductile metals: An experimental study on polycrystalline work-hardened and annealed oxygen-free copper10.1080/01418619908212037 ↗
44. Dub, S.N. (1984). Fracture Toughness Determination of Superhard Single Crystals by Indentation. [Ph.D. Thesis, Institute for Superhard Materials of the Academy of Sciences of Ukraine].
45. Hardness and fracture toughness of CVD diamond film10.1016/0925-9635(95)00346-0 ↗
46. Microhardness and fracture toughness of cubic boron nitride single crystals