Reduced Sintering Temperatures of Li+ Conductive Li1.3Al0.3Ti1.7(PO4)3 Ceramics
Source abstract
Abstract
All-solid-state batteries (ASSB) are considered promising candidates for future energy storage and advanced electric mobility. When compared to conventional Li-ion batteries, the substitution of Li-ion conductive, flammable liquids by a solid electrolyte and the application of Li-metal anodes substantially increase safety and energy density. The solid electrolyte Li1.3Al0.3Ti1.7(PO4)3 (LATP) provides high Li-ion conductivity of about 10−3 S/cm and is considered a highly promising candidate for both the solid electrolyte-separator and the ionically conductive part of the all-solid state composite cathode, consisting of the cathode material, the solid electrolyte, and an electron conductor. Co-sintering of the composite cathode is a sophisticated challenge, because temperatures above 1000 °C are typically required to achieve the maximum ionic conductivity of LATP but provoke reactions with the cathode material, inhibiting proper electrochemical functioning in the ASSB. In the present study, the application of sintering aids with different melting points and their impact on the sinterability and the conductivity of LATP were investigated by means of optical dilatometry and impedance spectroscopy. The microstructure of the samples was analyzed by SEM. The results indicate that the sintering temperature can be reduced below 800 °C while maintaining high ionic conductivity of up to 3.6 × 10−4 S/cm. These insights can be considered a crucial step forward towards enable LATP-based composite cathodes for future ASSB.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Fraunhofer IKTS, Fraunhofer Institute for Ceramic Technologies and Systems IKTS, Winterbergstrasse 28, 01277 Dresden, Germany
Funding
Bundesministerium für Bildung, Wissenschaft und Forschung
References (27)
Show source-provided references
1. A solid future for battery development10.1038/nenergy.2016.141 ↗
2. Lithium battery chemistries enabled by solid-state electrolytes10.1038/natrevmats.2016.103 ↗
3. Zhao, Q., Stalin, S., Zhao, C.-Z., and Archer, L.A. (2020). Designing solid-state electrolytes for safe, energy-dense batteries. Nat. Rev. Mater.10.1038/s41578-019-0165-5 ↗
4. Mindemark, J., Lacey, M.J., Bowden, T., and Brandell, D. (2018). Beyond PEO–Alternative host materials for Li+-conducting solid polymer electrolytes. Prog. Polym. Sci., 114–143.10.1016/j.progpolymsci.2017.12.004 ↗
5. Capacity Fade in Solid-State Batteries: Interphase Formation and Chemomechanical Processes in Nickel-Rich Layered Oxide Cathodes and Lithium Thiophosphate Solid Electrolytes10.1021/acs.chemmater.7b00931 ↗
6. A Novel Sol-Gel Method for Large-Scale Production of Nanopowders: Preparation of Li1.5Al0.5Ti1.5(PO4)3 as an Example10.1111/jace.13997 ↗
7. Preparation and characterization of sol-gel derived high lithium ion conductive NZP-type ceramics Li1+xAlxTi2−x(PO4)310.1016/j.ssi.2015.03.009 ↗
8. Inada, R., Yasuda, S., Hosokawa, H., Saito, M., Tojo, T., and Sakurai, Y. (2018). Formation and Stability of Interface between Garnet-Type Ta-doped Li7La3Zr2O12 Solid Electrolyte and Lithium Metal Electrode. Batteries, 4.10.3390/batteries4020026 ↗
9. An explanation of the microcrack formation in Li1.3Al0.3Ti1.7(PO4)3 ceramics10.1016/j.jeurceramsoc.2016.02.042 ↗
10. First priniciples study on electrochemical and chemical stability of solid electrolyte-electrode interfaces in all-solid-state Li-ion batteries10.1039/C5TA08574H ↗
11. A garnet structure-based all-solid-state Li battery without interface modification: Resolving incompatibility issues on positive electrodes10.1039/C8SE00436F ↗
12. Understanding interface stability in solid-state batteries10.1038/s41578-019-0157-5 ↗
13. About the Compatibility between High Voltage Spinel Cathode Materials and Solid Oxide Electrolytes as a Function of Temperature10.1021/acsami.6b09059 ↗
14. A microcontact impedance study on NASICON type Li1+xAlxTi2−x(PO4)3 (0 ≤ x ≤ 0.5) single crystals10.1039/C5TA08545D ↗
15. Synthesis and sintering of Li1.3Al0.3Ti1.7(PO4)3 (LATP) electrolyte for ceramics with improved Li+ conductivity10.1016/j.jallcom.2019.153237 ↗
16. Dense on porous solid LATP electrolyte system: Preparation and conductivity measurement10.1111/jace.14451 ↗
17. Optimization of Al2O3 and Li3BO3 Content as Sintering Additives of Li7−xLa2.95Ca0.05ZrTaO12 at Low Temperature10.1007/s11664-016-4924-4 ↗
18. Electrical property and sinterability of LiTi2(PO4)3 mixed with lithium salt (Li3PO4 or Li3BO3)10.1016/0167-2738(91)90247-9 ↗
19. Ionic conductivity enhancement in LiTi2(PO4)3-based composite electrolyte by the addition of lithium nitrate10.1016/S0378-7753(97)02520-2 ↗
20. Solid lithium ion conducting composites based on LiTi2(PO4)3 and Li2.9B0.9S0.1O3.1 glass10.1016/j.ssi.2018.05.007 ↗
21. The Li+ conducting composite based on LiTi2(PO4)3 and Li3BO3 glass10.1016/j.jssc.2018.06.028 ↗
22. Influence of the secondary phase LiTiOPO4 on the properties of Li1+xAlxTi2−x(PO4)3 (x = 0; 0.3)10.1016/j.ssi.2016.10.008 ↗
23. Lithium-ion conducting solid electrolytes of Li1.4Al0.4Ge0.2Ti1.4(PO4)3 and MOx (M=Al, Ti, and Zr) composites10.1016/j.ssi.2018.06.016 ↗
24. Insight into the Microstructure and Ionic Conductivity of Cold Sintered NASICON Solid Electrolyte for Solid-State Batteries10.1021/acsami.9b08132 ↗
25. The devitrification of lithium metaborate: Polymorphism and glass formation
26. Effect of microcracking on ionic conductivity in LATP10.1016/j.jpowsour.2012.06.081 ↗
27. Electroceramics: Characterization by Impedance Spectroscopy10.1002/adma.19900020304 ↗