Effects of Crystal Orientation on the Crack Propagation of Sapphire by Sequential Indentation Testing
Source abstract
Abstract
Single-crystal sapphire (α-Al2O3) is a hard and brittle material. Due to its highly crystalline nature, the fracture behavior of sapphire is strongly related to its crystal structure, and understanding the effects of crystal structure on the crack propagation of sapphire is essential for the successful application of this important material (e.g., as wafers in the electronics industry). In the present work, crack propagation that is induced by sequential indentation was investigated on the A-plane and C-plane of sapphire using a Vickers indenter on a micrometer scale. It was found that increasing indentation depth obviously increases the rate of crack propagation on the A-plane, but this effect is not so obvious on the C-plane because of the different slip systems induced by indentation on the different crystal planes of sapphire. Moreover, some parallel linear traces along the A-plane, which fracture with increasing indentation depth, are observed from the residual indentation on the A-plane. The fracture toughness of both A-plane and C-plane sapphire is smaller after indentation testing than that obtained using conventional testing methods. The subsurface damage was detected by transmission electron microscopy (TEM).
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Manufacturing Engineering, Huaqiao University, Xiamen 361021, China
MOE Engineering Research Center for Brittle Materials Machining, Huaqiao University, Xiamen 361021, China
College of Mechanical Engineering and Automation, Huaqiao University, Xiamen 361021, China
Funding
National Natural Science Foundation of China · Graduates Cultivation Project of Huaqiao University for Research and Innovation Ability
References (29)
Show source-provided references
1. Controlled wet erosive wear of sapphire10.1016/j.jeurceramsoc.2004.08.018 ↗
2. Nanoscale elastic–plastic deformation and stress distributions of the c plane of sapphire single crystal during nanoindentation10.1016/j.jeurceramsoc.2011.04.012 ↗
3. Dobrovinskaya, E.R., Lytvynov, L.A., and Pishchik, V. (2009). Sapphire Material, Manufacturing, Applications, Springer Science+Business Media.
4. Influence of mosaicity on the fracture behavior of sapphire10.1016/j.actamat.2013.12.004 ↗
5. Armstrong, R.W., Walley, S.M., and Elban, W.L. (2017). Crystal Indentation Hardness. Crystals, 7.10.3390/cryst7010021 ↗
6. Galanov, B.A., Milman, Y.V., Chugunova, S.I., Goncharova, I.V., and Voskoboinik, I.V. (2017). Application of the Improved Inclusion Core Model of the Indentation Process for the Determination of Mechanical Properties of Materials. Crystals, 7.10.3390/cryst7030087 ↗
7. Ruestes, C.J., Alhafez, I.A., and Urbassek, H.M. (2017). Atomistic Studies of Nanoindentation—A Review of Recent Advances. Crystals, 7.10.3390/cryst7100293 ↗
8. Nanoindentation study of pop-in phenomenon characteristics and mechanical properties of sapphire 10 1 ¯ 2 crystal10.1111/j.1551-2916.2012.05405.x ↗
9. Influence of loading rate on nanohardness of sapphire10.1016/j.ceramint.2016.05.091 ↗
10. Indentation-induced damage in GaN epilayers10.1063/1.1436280 ↗
11. Peculiar surface deformation of sapphire Numerical simulation of nanoindentation10.1063/1.1635983 ↗
12. Dislocation cross-slip in GaN single crystals under nanoindentation10.1063/1.3593381 ↗
13. Understanding the friction and wear of KDP crystals by nanoscratching10.1016/j.wear.2014.11.032 ↗
14. Deformation of sapphire induced by a spherical indentation on the 10 1 ¯ 0 plane10.1063/1.115713 ↗
15. Indentation fracture and soft impresser fatigue in sapphire and polycrystalline alumina10.1016/S0263-4368(98)00041-9 ↗
16. Static and dynamic indentation response of basal and prism plane sapphire10.1016/j.jeurceramsoc.2011.03.006 ↗
17. Ultrasonic vibration-assisted scratch-induced characteristics of c-plane sapphire with a spherical indenter10.1016/j.ijmachtools.2012.07.009 ↗
18. Analysis of interacting cracks due to sequential indentations on sapphire10.1016/j.actamat.2011.02.026 ↗
19. Investigation into the microstructure evolution caused by nanoscratch-induced room temperature deformation in M-plane sapphire10.1016/j.actamat.2011.04.054 ↗
20. An experimental and theoretical investigation on the brittle ductile transition and cutting force anisotropy in cutting KDP crystal10.1016/j.ijmachtools.2016.04.009 ↗
21. Strength dependent design method for the crystal orientation of diamond berkovich indenter10.1016/j.matdes.2015.10.062 ↗
22. Distribution of residual strain around nanoindentations in silicon10.1016/j.matlet.2014.06.004 ↗
23. Elastic/plastic indentation damage in ceramics the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
24. In situ observation of fracture sequence of physical vapor deposited tin film on 1120 sapphire10.1557/JMR.2005.0201 ↗
25. A critical evaluation of indentation techniques for measuring fracture toughness i, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
26. High-temperature fracture toughness of sapphire10.1111/j.1151-2916.1994.tb04542.x ↗
27. Molecular dynamics-simulations of the fracture toughness of sapphire
28. Residual stress effects in sharp contact cracking10.1007/BF00551043 ↗
29. Initial stages of contact-induced plasticity in sapphire. I. Surface traces of slip and twinning10.1080/14786430701618464 ↗