The Effect of Thermocycling and Surface Treatments on the Surface Roughness and Microhardness of Three Heat-Pressed Ceramics Systems
Source abstract
Abstract
Dental ceramic restorations are widely used in restorative dentistry. However, these restorations can be affected once cemented in the oral cavity by several factors. How can conventional surface treatments, such as glazing and mechanical polishing, diminish the effects of aging? The purpose of this in vitro study was to evaluate the effect of thermocycling and conventional surface treatments on the surface roughness and microhardness of three types of glass-ceramics by using a profilometer, scanning electron microscopy (SEM), atomic force microscopy (AFM), and a microhardness tester. Three types of ceramic systems (zirconia reinforced lithium silicate glass-ceramic, lithium disilicate glass-ceramic, and feldspathic glass-ceramic) (n = 48) were prepared. The samples were subjected to thermocycling for 10,000 cycles. Surface roughness was evaluated numerically using a profilometer and visually by using SEM and AFM. Microhardness was performed using a microhardness tester. The data were interpreted using the ANOVA test, and the results were correlated using Pearson’s correlation formula (r). Significant differences were found before and after thermocycling for the Ra (p < 0.01) and Rz (p < 0.05) parameters. As well, differences between glazed and polished surfaces were significant before and after thermocycling for surface roughness and microhardness (p < 0.05). A correlation was made between average surface roughness and microhardness (r = −460) and for the maximum surface roughness and microhardness (r = −606). Aging increases the roughness and decreases in time the microhardness. The tested ceramic systems behaved differently to the aging and surface treatments. Surface treatments had a significant impact on the microhardness and surface characteristics. The glazed groups were reported with higher surface roughness and lower microhardness when compared to the polished groups before and after thermocycling. The measuring roughness techniques determine the scale-dependent values for the Ra (Sa) and Rz (Sq) parameters. Thermocycling almost doubled the surface roughness for all the tested samples. Microhardness decreased only for the Celtra glazed samples. Nano-roughness increased the values for Vita and slightly for Emax. Thermocycling had little effect on Emax ceramic and a more significant impact on Celtra Press ceramic.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Research and COVID-19
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Dental Prostheses Technology, Universitatea de Medicină si Farmacie Victor Babeș, Timișoara, 300041 Timisoara, Romania
Department of Oral Rehabilitation, Universitatea de Medicină si Farmacie Victor Babeș, Timișoara, 300041 Timișoara, Romania
National Institute for Research and Development in Electrochemistry and Condensed Matter, 300569 Timișoara, Romania
Departamentul Ingineria Materialelor şi Fabricaţiei, Universitatea Politehnică Timişoara, Bd. Mihai Viteazul nr.1, 300222 Timişoara, Romania
References (65)
Show source-provided references
1. The effect of surface roughness on ceramics used in dentistry: A review of the literature10.4103/1305-7456.143646 ↗
2. Porcelain materials10.1177/08959374880020011601 ↗
3. The use of confocal microscopy to assess surface roughness of two milled CAD-CAM ceramics following two polishing techniques10.1016/j.dental.2006.06.012 ↗
4. The influence of surface roughness and surface-free energy on supra-and subgingival plaque formation in man. A review of the literature10.1111/j.1600-051X.1995.tb01765.x ↗
5. The influence of surface free energy and surface roughness on early plaque formation. An in vivo study in man10.1111/j.1600-051X.1990.tb01077.x ↗
6. Tooth Polishing: The Current Status10.4103/0972-124X.154170 ↗
7. Glazing and Finishing Dental Porcelain: A Literature Review
8. McLean, J.W. (1979). The Science and Art of Dental Ceramics, Quintessence Publishing.
9. Effects of porcelain on occluding surface of restored teeth10.1016/0022-3913(89)90360-0 ↗
10. Refinishing of porcelain by using a refinishing kit10.1016/0022-3913(91)90229-P ↗
11. Efficacy of a porcelain refinishing system in restoring surface finish after grinding with fine and extra-fine diamond burs10.1016/0022-3913(92)90400-5 ↗
12. Clinical discrimination between auto glazed and polished porcelain surfaces10.1016/0022-3913(90)90284-J ↗
13. Application of heat-pressed ceramics for single-tooth restorations
14. The influence of oral environment on the optical properties of heat-pressed ceramics10.37358/MP.19.1.5164 ↗
15. Effects of six surface treatment methods on the surface roughness of a low-fusing and an ultra low-fusing feldspathic ceramic material10.1111/j.1532-849X.2008.00410.x ↗
16. Mechanics of distributed cracking10.1115/1.3143724 ↗
17. Analysis of stresses and strains near the end of a crack transversing a plate10.1115/1.4011547 ↗
18. Failure analysis of various monolithic posterior aesthetic dental crowns using the finite element method10.1088/1742-6596/885/1/012003 ↗
19. Vicker’s microhardness and energy dispersive X-ray analysis of fluoride leucite fluorapatite ceramics clinically immersed in acid agents10.2334/josnusd.51.443 ↗
20. Evaluation of different pH solutions on the mechanical behavior of two hot pressed dental ceramics10.1088/1757-899X/416/1/012012 ↗
21. Experimental analyses for the mechanical behavior of pressed all-ceramic molar crowns with anatomical design10.1051/matecconf/201710802001 ↗
22. Multifunctional uses of a novel ceramic-lithium disilicate10.1111/j.1708-8240.2010.00362.x ↗
23. Clinical outcomes of lithium disilicate single crowns and partial fixed dental prostheses: A systematic review10.1016/j.prosdent.2014.01.005 ↗
24. Fracture loads of all-ceramic crowns under wet and dry fatigue conditions10.1111/j.1532-849X.2009.00498.x ↗
25. Heat transfer and thermal stress analysis of a mandibular molar restored by different indirect restorations using a three-dimensional finite element method
26. Effect of artificial accelerated aging on surface roughness and color stability of different ceramic restorations
27. Effect of thermocycling on the roughness of nanofilm, microfilm, and micro-hybrid composites10.3109/00016357.2014.971868 ↗
28. Vasiliu, R.D., Porojan, S.D., Birdeanu, M.I., and Porojan, L. (2020). Effect of thermocycling, surface treatments and microstructure on the optical properties and roughness of CAD-CAM and heat-pressed glass-ceramics. Materials, 13.10.3390/ma13020381 ↗
29. Thermal cycling for restorative materials does a standardised protocol exist in laboratory testing? A literature review10.1016/j.jmbbm.2013.09.013 ↗
30. Temperature extremes produced orally by hot and cold liquids10.1016/0022-3913(92)90239-7 ↗
31. Effect of critical thermal cycling on the flexural strength of resin composites10.2334/josnusd.57.137 ↗
32. Thermal cycling procedures for laboratory testing of dental restorations
33. Mechanical properties of resin-ceramic CAD-CAM materials after accelerated aging10.1016/j.prosdent.2017.08.016 ↗
34. Mechanical properties of composite resin blocks for CAD/CAM10.4012/dmj.2014-208 ↗
35. Improving shear bond strength between feldspathic porcelain and zirconia substructure with lithium disilicate glass-ceramic liner10.4012/dmj.2014-319 ↗
36. Nesrin, S., Pinar, G., Volkan, T., Gokhan, A., and Deniz, S. (2018). Evaluation of five CAD/CAM materials by microstructural characterization and mechanical tests: A comparative in vitro study. BMC Oral Health, 18.10.1186/s12903-017-0458-2 ↗
37. Effects of different glaze treatments on the optical properties and roughness of lithium disilicate ceramics10.7126/cumudj.500975 ↗
38. Color change of CAD-CAM materials and composite resin cements after thermocycling10.1016/j.prosdent.2017.12.003 ↗
39. Effect of etching time and resin bond on theflexural strength of IPS e.max Press glass ceramic10.1016/j.dental.2014.08.373 ↗
40. The influence of ceramic re-pressing on surface properties, bond strength, and color stability of leucite ceramic
41. Alp, G., Subasi, M.G., Johnston, W.M., and Yilmaz, B. (2018). Effect of surface treatments and coffee thermocycling on the color and translucency of CAD-CAM monolithic glass-ceramic. J. Prosthet. Dent.10.1016/j.prosdent.2017.10.024 ↗
42. Failure of all-ceramic fixed partial dentures in vitro and in vivo: Analysis and modeling10.1177/00220345950740060301 ↗
43. Influence of polishing procedures on the surface roughness of dental ceramics made by different techniques
44. Surface treatment of feldspathic porcelain: Scanning electron microscopy analysis10.4047/jap.2014.6.5.387 ↗
45. The use of environmental scanning electron microscopy for imaging wet and insulating materials10.1038/nmat898 ↗
46. Surface roughness of a dental ceramic after polishing with different vehicles and diamond pastes10.1590/S0103-64402006000300003 ↗
47. Surface roughness in ceramics with different finishing techniques using atomic force microscope and profilometry10.2341/05-54 ↗
48. Influence of the finishing technique on surface roughness of dental porcelain with different microstructure10.2341/05-104 ↗
49. Effect finishing and polishing procedures on the surface roughness of IPS Empress 2 ceramic10.3109/00016357.2012.690570 ↗
50. The surface roughness of enamel to enamel contact areas compred with the intrinsic roughness of dental resin composites10.1177/00220345910700091301 ↗
51. The in vivo perception of roughnes of restorations10.1038/sj.bdj.4810881 ↗
52. Effect of finishing and polishing on the surface roughness of four ceramic materials after occlusal adjustment10.1111/jerd.12222 ↗
53. The effect of porcelain polishing systems on the color and surface texture of feldspathic porcelain10.1016/j.prosdent.2006.05.009 ↗
54. Wear resistance and abrasiveness of CAD-CAM solid materials10.1016/j.prosdent.2018.05.011 ↗
55. Adhesion to Y-TZP ceramic: A study of silica nanofilm coating on the surface of Y-TZP10.1002/jbm.b.33184 ↗
56. Comparison of surface roughness of oral hard materials to the threshold surface roughness for bacterial plaque retention: A review of the literature10.1016/S0109-5641(97)80038-3 ↗
57. Mechanical and optical properties of monolithic CAD-CAM restorative materials10.1016/j.prosdent.2017.06.012 ↗
58. Evaluation of mechanical and optical behavior of current aesthetic dental restorative CAD/CAM composites10.1016/j.jmbbm.2015.10.004 ↗
59. Mechanical and thermal cycling effects on the flexural strength of glass ceramics fused to titanium10.4012/dmj.27.7 ↗
60. Does artificial aging affect the mechanical properties of CAD/CAM composite materials?10.1016/j.jpor.2017.06.001 ↗
61. A statistical approach to the mechanical testing of dental materials10.1016/S0109-5641(86)80021-5 ↗
62. Wang, F., Chai, Z., Deng, Z., Gao, J., Wang, H., and Chen, J. (2015). Effect of heat- pressing temperature and holding time on the microstructure and flexural strength of lithium Disilicate glass-ceramics. PLoS ONE, 10.10.1371/journal.pone.0130919 ↗
63. Bradt, R.C., Evans, A.G., Hasselman, D.P.H., and Lange, F.F. (1983). Surface flaws, statics, and microcracking. Fracture Mechanics of Ceramics, Plenunm Press.10.1007/978-1-4613-3488-0 ↗
64. Correlation between fracture toughness and leucite content in dental porcelains10.1016/j.jdent.2005.02.001 ↗
65. Slow crack growth and reliability of dental ceramics10.1016/j.dental.2010.10.025 ↗