High-Durability Concrete with Supplementary Cementitious Admixtures Used in Corrosive Environments

Shiming Liu, Miaomiao Zhu, Xinxin Ding, Zhiguo Ren, Shunbo Zhao, Mingshuang Zhao, Juntao Dang

Crystals· Volume 11· Issue 2

Abstract

Durability of concrete is of great significance to prolong the service life of concrete structures in corrosive environments. Aiming at the economical and environment-friendly production of concrete by comprehensive utilization of the supplementary cementitious materials made of industrial byproducts, the resistances to chloride penetration, sulfate attack, and frost of high-performance concrete were studied in this paper. Fifteen concretes were designed at different water–binder ratio with the changes of contents of fly ash (FA), silica fume (SF), ground granulated blast-furnace slag (GGBS), and admixture of sulfate corrosion-resistance (AS). The compressive strength, the total electric flux of chloride penetrability, the sulfate resistance coefficient, and the indices of freezing and thawing were measured. Results indicate that, depending on the chemical composition, fineness, and pozzolanic activity, the supplementary cementitious admixtures had different effects on the compressive strength and the durability of concrete; despite having a higher fineness and pozzolanic activity, the GGBS gave out a negative effect on concrete due to a similar chemical composition with cement; the SF and FA presented beneficial effects on concrete whether they were used singly with GGBS or jointly with GGBS; the AS improved the compressive strength and the sulfate corrosion resistance of concrete. In general, the grade of durability was positively related to the compressive strength of concrete. Except for the concretes admixed only with GGBS or with GGBS and FA, others had super durability with the compressive strength varying from 70 MPa to 113 MPa. The concretes with water to binder ratio of 0.29 and total binders of 500 kg/m3 admixed with 7% FA + 8% SF + 8% GGBS or 7% FA + 8% SF + 8% GGBS + (10~12)% AS presented the highest grades of resistances specified in China codes to chloride penetration, sulfate corrosion, and frost, while the compressive strength was about 100 MPa.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Concrete Corrosion and Durability · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

International Joint Research Lab for Eco-Building Materials and Engineering of Henan, School of Civil Engineering and Communications, North China University of Water Resources and Electric Power, Zhengzhou 450045, China

Collaborative Innovation Center of New Urban Building Technology of Henan, North China University of Water Resources and Electric Power, Zhengzhou 450045, China

Zhuzhou China Railway Electrical Materials Co. LTD., Zhuzhou 412001, China

Funding

Key Scientific and Technological Research Project of University in Henan, China · Postgraduate Innovation Project of NCWU · State Key Research and Development Plan, China · Innovative Sci-Tech Team of Eco-building Material and Structural Engineering of Henan, China

References (49)

Show source-provided references
1. China Academy of Railway Sciences (2011). Code for Durability Design on Concrete Structure of Railway, China Railway Publishing House. TB 10005-2010.
2. Mechanical properties of non-uniformly corroded steel bars based on length characterization
3. Analysis of corrosion risk due to chloride diffusion for concrete structures in marine environment10.1016/j.marstruc.2020.102804 ↗
4. Sulfate attack expansion mechanisms10.1016/j.cemconres.2013.07.005 ↗
5. Experimental study of the deterioration mechanism of concrete under sulfate attack in wet-dry cycles
6. Durability of concrete containing fly ash and silica fume against combined freezing-thawing and sulfate attack10.1016/j.conbuildmat.2017.04.172 ↗
7. Li, Y., Zhai, Y., Liang, W.B., Li, Y.B., Dong, Q., and Meng, F.D. (2020). Dynamic mechanical properties and visco-elastic damage constitutive model of freeze–thawed concrete. Materials, 13.10.3390/ma13184056 ↗
8. Long term durability performance and mechanical properties of highperformance concretes with combined use of supplementary cementing materials10.1016/j.conbuildmat.2016.02.224 ↗
9. Efficiency of mineral admixtures in concrete: Microstructure, compressive strength and stability of hydrate phases10.1016/j.clay.2013.08.021 ↗
10. Optimization of ternary cementitious mortar blends using factorial experimental plans10.1007/BF02483137 ↗
11. Mechanical and durability properties of high performance concretes containing supplementary cementitious materials10.1016/j.conbuildmat.2009.08.045 ↗
12. Enhanced hydration model of fly ash in blended cement and application of extensive modeling for continuous hydration to pozzolanic micro-pore structures10.1016/j.cemconcomp.2020.103733 ↗
13. Mechanism of fly ash in hydration of composite cementitious materials
14. Compressive strength and chloride resistance of self-compacting concrete containing high level fly ash and silica fume10.1016/j.matdes.2014.07.042 ↗
15. Sulfate resistance of plain and blended cements exposed tovarying concentrations of sodium sulfate10.1016/S0958-9465(02)00083-5 ↗
16. Strength and drying shrinkage properties of self-compacting concretes incorporating multi-system blended mineral admixtures10.1016/j.conbuildmat.2010.04.015 ↗
17. Performances evaluation of binary concrete designed with silica fumeand metakaolin10.1016/j.conbuildmat.2018.01.138 ↗
18. Influence of hydration environment on the characteristics of ground granulated blast furnace slag hydration products
19. Influence of mineral admixtures on impermeability and frost resistance of high performance concrete
20. Experimental research about sulfate resistance performance of high performance concrete
21. Yang, B.J. (2011). Experimental Study on the Sulfate Corrosion-Resistance Admixturefor Concrete. [Master’s Thesis, Qingdao Technological University].
22. Effect and mechanism of sulfate corrosion-resistance admixture on concrete performance
23. Influence of anticorrosion agent and curing regimes on pore structure feature and moisture loss of concrete
24. Liang, R. (2018). Compounding of High Durability Concrete and Application in Strong Corrosive Environment. [Master’s Thesis, Harbin Institute of Technology].
25. Ministry of Housing and Urban-Rural Construction of the People’s Republic of China (2009). Standard for Test Methods of Long-Term Performance and Durability of Ordinary Concrete, China Building Industry Press. GB 50082-2009.
26. Ministry of Housing and Urban-Rural Construction of the People’s Republic of China (2009). Standard for Inspection and Assessment of Concrete Durability, China Building Industry Press. JGJ/T 193-2009.
27. Deterioration mechanisms of sulfate attack on concrete under alternate action10.1007/s11595-010-2355-2 ↗
28. Sossa, V., Pérez-Gracia, V., González-Drigo, R., and Rasol, M.A. (2019). Lab non-destructive test to analyze the effect of corrosion on ground penetrating radar scans. Remote Sens., 11.10.3390/rs11232814 ↗
29. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China (2007). Common Portland Cement, China Standard Press. GB 175-2007.
30. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China (2017). Fly Ash Used for Cement and Concrete, China Standard Press. GB/T 1596-2017.
31. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China (2011). Silica Fume Cement Mortar and Concrete, China Standard Press. GB/T 27690-2011.
32. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China (2008). Ground Granlated Blast Furnace Slag Used for Cement, Mortar and Concrete, China Standard Press. GB/T 18046-2017.
33. National Development and Reform Commission of the People’s Republic of China (2006). Sulfate Corrosion-resistance Admixtures for Concrete, China Building Materials Industry Press. JC/T 1011-2006.
34. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China (2011). Sand for Construction, China Standard Press. GB/T 14684-2011.
35. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China (2011). Pebble and Crushed Stone for Construction, China Standard Press. GB/T 14685-2011.
36. Ministry of Housing and Urban Rural Development of the People’s Republic of China (2011). Specification for Mix Proportion Design of Ordinary Concrete, China Building Industry Press. JGJ 55-2011.
37. Ministry of Construction of the People’s Republic of China (2002). Standard for Test Methods on Mechanical Properties of Ordinary Concrete, China Building Industry Press. GB/T 50081-2002.
38. American Society for Testing and Materials (2019). Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration, ASTM International. ASTM C1202-19.
39. Numerical analysis of mix proportion of self-compacting concrete compared to ordinary concrete10.4028/www.scientific.net/KEM.789.69 ↗
40. Ding, X.X., Zhao, M.L., Zhou, S.Y., Fu, Y., and Li, C.Y. (2019). Statistical analysis and preliminary study on the mix proportion design of self-compacting steel fiber reinforced concrete. Materials, 12.10.3390/ma12040637 ↗
41. Li, C.Y., Shang, P.R., Li, F.L., Feng, M., and Zhao, S.B. (2020). Shrinkage and mechanical properties of self-compacting SFRC with calcium sulfoaluminate expansive agent. Materials, 13.10.3390/ma13030588 ↗
42. Durability performance of concrete incorporating Class F and Class C fly ashes10.1016/j.conbuildmat.2012.02.075 ↗
43. Experimental study on autogenous and drying shrinkage of lightweight-aggregate concrete reinforced by steel fibers10.1155/2016/2589383 ↗
44. Experimental study on long-term compressive strength of concrete with manufactured sand10.1016/j.conbuildmat.2016.01.028 ↗
45. Li, C.Y., Wang, F., Deng, X.S., Li, Y.Z., and Zhao, S.B. (2019). Testing and prediction of the strength development of recycled-aggregate concrete with large particle natural aggregate. Materials, 12.10.3390/ma12121891 ↗
46. Concrete deterioration mechanisms under combined sulfate attack and flexural loading10.1061/(ASCE)MT.1943-5533.0000538 ↗
47. Deterioration mechanisms of sulfate attack on concrete under the action of compound factors
48. Mu, R. (2000). Durability and Service Life Prediction of Concrete Subjected to the Combined Action of Freezing-Thawing, Sustained External Flexural Stress and Salt Solution. [Master’s Thesis, Southeast University].
49. Development of steel fiber-reinforced expanded-shale lightweight concrete with high freeze-thaw resistance10.1155/2018/9573849 ↗