Room Temperature Corrosion Behavior of Selective Laser Melting (SLM)-Processed Ni-Fe Superalloy (Inconel 718) in 3.5% NaCl Solution at Different pH Conditions: Role of Microstructures
Source abstract
Abstract
Inconel 718 (UNS N07718) is a nickel-base superalloy containing iron that is used at cryogenic temperatures (arctic pipe components) and at high temperatures (gas turbines). This alloy is also used in off-shore oil drilling due to its high overall strength and resistance to corrosion. Inconel 718 components are created by a selective laser melting (SLM) additive manufacturing route and result in isotropic fine-grained microstructures with metastable phases (such as Laves phases) that are not usually present in conventional manufacturing processes. In this work, SLM Inconel 718 alloy specimens were investigated in four different conditions: (1) As-manufactured (AS-AM), (2) Additively manufactured and hot isostatically pressed (AM-HIP), (3) As-manufactured and heat-treated (solution annealing followed by two-step aging), and 4) AM-HIP and heat-treated. Localized corrosion behavior was evaluated at room temperature in a 3.5% NaCl solution at three different pH conditions (pH 1.25, 6.25, and 12.25). Electrochemical tests, including linear polarization, cyclic polarization, potentiostatic conditioning, electrochemical impedance spectroscopy, and Mott–Schottky analyses, were used to compare the corrosion behaviors of the SLM specimens with that of the conventionally wrought IN718 samples. The results showed that the additively manufactured specimens showed better corrosion resistance than the wrought material in the acidic chloride solution, and the AM-HIP specimens exhibited superior corrosion resistance to the as-manufactured ones. Hot isostatic pressing resulted in the visible elimination of the dendritic structure, indicating compositional homogeneity as well as a significant decrease in porosity. In addition, the deleterious secondary phases, such as Laves and δ phases, were not observed in the microstructure of the HIPed samples. The AM-HIP material showed the highest corrosion resistance in all the pH conditions. The two-step aging treatment, in general, resulted in the deterioration of corrosion resistance, which could be attributed to the formation of γ′ and γ″ precipitates that increased the cathodic reaction catalytic activities. In the additively manufactured samples, the presence of the Laves phase was more detrimental to corrosion resistance than any other phases and MC carbide and grain boundary δ phase increased the susceptibility to corrosion in wrought materials.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Nuclear Engineering and Industrial Management, University of Idaho, Idaho Falls, ID 83402, USA
Funding
Idaho Department of Commerce
References (44)
Show source-provided references
1. Sims, C.T., and Hagel, W.C. (1972). The Superalloys, John Wiley & Sons.
2. Microstructural evolution and corrosion behaviors of Inconel 718 alloy produced by selective laser melting following different heat treatments
3. An Investigation on high-temperature oxidation and hot corrosion resistance behavior of coated TLP (Transient Liquid Phase)-bonded IN738-LC10.1007/s12666-018-1390-0 ↗
4. Morphology of γ′ and γ″ precipitates and thermal stability of inconel 718 type alloys10.1007/BF02649604 ↗
5. High temperature deformation of Inconel 71810.1016/j.jmatprotec.2006.04.072 ↗
6. Microstructure and mechanical properties of Inconel 718 electron beam welds10.1179/174328405X62260 ↗
7. Grain boundary niobium carbides in Inconel 71810.1016/S1359-6462(97)00373-4 ↗
8. (2020, November 14). INCONEL®alloy 718 (UNS N07718/W.Nr. 2.4668), Technical Brochure, Special Metals. Available online: www.specialmetals.com.
9. (2004). Specification of Nickel Base Alloy 718 (UNS N07718) for Oil and Gas Drilling and Production Equipment (Standard No. API SPEC 6A718-2004).
10. The influence of heat treatments on the corrosion behavior of nickel-based alloy 71810.1016/j.jallcom.2019.151781 ↗
11. Influence of surface modifications on pitting corrosion behavior of nickel-base alloy 718. Part 1: Effect of machine hammer peening10.1016/j.corsci.2013.08.007 ↗
12. Effect of carbides on sensitivity of pitting corrosion in Inconel 718 alloy10.1108/ACMM-10-2018-2025 ↗
13. Edward, J.L. (1991). Superalloys 718,625 and Various Derivatives, The Minerals, Metals & Materials Society.
14. The formation and control of Laves phase in superalloy 718 welds10.1023/A:1018541915113 ↗
15. Decomposition of the Laves phase in the fusion zone of the Inconel 718/ATI 718Plus® welded joint during isothermal holding at a temperature of 649 °C10.1016/j.matchar.2022.112560 ↗
16. The formation and dissolution mechanisms of Laves phase in Inconel 718 fabricated by selective laser melting compared to directed energy deposition and cast10.1016/j.compositesb.2022.109994 ↗
17. Strengthening mechanisms in selective laser-melted Inconel718 superalloy10.1016/j.msea.2021.141145 ↗
18. Dissolution kinetics of Laves phase during homogenization heat treatment of additively manufactured Inconel 718 superalloy10.1016/j.jmrt.2023.04.013 ↗
19. Corrosion of Additively Manufactured Alloys: A Review10.5006/2926 ↗
20. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
21. Electrochemical Removal of Different Phases from Laser Solid Formed Inconel 71810.1149/2.0951707jes ↗
22. Electrochemical behavior of Inconel 718 fabricated by laser solid forming on different sections10.1016/j.corsci.2017.12.021 ↗
23. Effects of Solution Heat Treatment on Laves Phase and Corrosion Behaviors in Selective Laser Melted Inconel 718 Alloy10.1088/1757-899X/677/2/022081 ↗
24. Influence of build orientation on microstructure, mechanical and corrosion behavior of Inconel 718 processed by selective laser melting10.1016/j.msea.2019.05.013 ↗
25. Microstructural evolution and mechanical properties of IN718 alloy fabricated by selective laser melting following different heat treatments10.1016/j.jallcom.2018.09.200 ↗
26. Tribocorrosion Behavior of Inconel 718 Fabricated by Laser Powder Bed Fusion-Based Additive Manufacturing10.3390/coatings11020195 ↗
27. Understanding the corrosion behaviour of laser directed energy deposition-based additive manufacturing built Inconel 718 under acidic environments10.1007/s40964-021-00176-4 ↗
28. Corrosion Behaviors of Selective Laser Melted Inconel 718 Alloy in NaOH Solution
29. Synergistic effect of transpassive film and gamma double prime phase on the electrochemical dissolution behavior of Inconel 718 manufactured by laser directed energy deposition10.1016/j.matchar.2023.113207 ↗
30. Passive behavior of laser directed energy deposited Inconel 718 after homogenization and aging heat treatment10.1016/j.corsci.2022.110439 ↗
31. Influence of SLM process parameters on the surface finish, porosity rate and fatigue behavior of as-built Inconel 625 parts10.1016/j.jmatprotec.2017.12.043 ↗
32. Influence of processing parameters on the evolution of melt pool, porosity, and microstructures in Ti-6Al-4V alloy parts fabricated by selective laser melting10.1007/s40964-017-0030-2 ↗
33. Influence of laser processing parameters on porosity in Inconel 718 during additive manufacturing10.1007/s00170-019-03655-9 ↗
34. On The Corrosion and Metastable Pitting Characteristics of 316L Stainless Steel Produced by Selective Laser Melting10.1149/2.0551706jes ↗
35. Koizumi, M. (1992). Hot Isostatic Pressing Theory and Applications, International Conference on Hot Isostatic Pressing, Elsevier Applied Science.10.1007/978-94-011-2900-8 ↗
36. Improvement in the Microstructure and Tensile Properties of Inconel 718 Superalloy by HIP Treatment10.2320/matertrans.47.2877 ↗
37. Effect of heat treatment on the modification of microstructure of selective laser melted (SLM) IN718 and its consequences on mechanical behavior10.1557/jmr.2020.129 ↗
38. Impact of heat treatment on mechanical behaviour of Inconel 718 processed with tailored microstructure by selective laser melting10.1016/j.matdes.2017.05.065 ↗
39. Corrosion behavior of wire arc additive manufactured Inconel 718 superalloy10.1016/j.jallcom.2020.154455 ↗
40. Anion redox chemistry in the cobalt free 3d transition metal oxide intercalation electrode Li[Li0.2Ni0.2Mn0.6]O210.1021/jacs.6b05111 ↗
41. Effects of dissolved oxygen on passive behavior of stainless alloys10.1016/j.corsci.2005.05.048 ↗
42. Influence of micro-structure on corrosion behavior of a Ni-based superalloy in 3.5% NaCl10.1016/j.electacta.2007.05.043 ↗
43. Semiconducting properties of surface oxide films of pure iron, nickel and chromium metals in pure water at 288 °C10.1023/A:1025787328084 ↗
44. Pitting corrosion of SLM Inconel 718 sample under surface and heat treatments10.1016/j.apsusc.2019.06.043 ↗