Heat Treatment Post-Processing for the Improved Mechanical Properties of Scalmalloy® Processed via Directed Energy Deposition
Source abstract
Abstract
As high-strength aluminum alloys present several processability issues with additive manufacturing (AM), Scalmalloy®, an Al-Mg-Sc-Zr-based alloy, has been developed. This alloy is age-hardenable, allowing it to precipitate out a strengthening precipitate phase, Al3(Sc,Zr). The manufacturer recommends a single-stage aging treatment at 325 °C for 4 h; however, the majority of the literature studies utilize a powder bed processing known as selective laser melting (SLM) over powder-fed processing directed energy deposition (DED). This study addresses the lack of information on heat treatments for DED fabrication by exploring the application of artificial aging temperatures of 300–400 °C for 2, 4, and 6 h to: 1. determine the impact on the microstructural evolution and mechanical performance and 2. determine whether the recommended treatment for Scalmalloy® is appropriate for DED fabrication. Tensile testing determined that low-temperature treatments exhibited no visible dependence on time (2–6 h); however, time becomes influential at higher temperatures starting at 350 °C. The temperature plays a considerable role in the mechanical and microstructural behaviors of DED Scalmalloy®. The highest tensile strength was noted at 300 °C (384 MPa, 21.6% increase), but all heat-treated cases resulted in an improvement over the as-built case. This investigation established that increasing the treatment temperature resulted in a decreasing trend for the tensile strength that held over time. Elongation at 2 h displayed a near parabolic trend that peaks at 350 °C (20%) and falls with higher temperatures. At the 4 h treatment, a slight decreasing trend was noticed for elongation. No visible change was observed for elongation at 6 h, with elongation values remaining fairly consistent. The microstructural evolution, including micron-sized and nano-sized Al3(Sc,Zr) and grain size, was examined, and coarsening effects were noted with the increase in the temperature. It is recommended that treatment be conducted at 300 °C to achieve the precipitation of the strengthening Al3(Sc,Zr) phase while minimizing coarsening.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical Engineering, Missouri University of Science and Technology, Rolla, MO 65409, USA
Funding
DoEdu GAANN · NSF · Product Innovation and Engineering, LLC.
References (45)
Show source-provided references
1. Challenges in additive manufacturing of high-strength aluminium alloys and current developments in hybrid additive manufacturing
2. Defects control of aluminum alloys and their composites fabricated via laser powder bed fusion: A review10.1016/j.jmatprotec.2023.118064 ↗
3. Dixit, S., and Liu, S. (2022). Laser Additive Manufacturing of High-Strength Aluminum Alloys: Challenges and Strategies. J. Manuf. Mater. Process., 6.10.3390/jmmp6060156 ↗
4. Rajendrachari, D.S. (2023). Additively Manufactured High-Strength Aluminum Alloys: A Review. Recent Advancements in Aluminum Alloys, IntechOpen.10.5772/intechopen.103993 ↗
5. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
6. Excellent strength–ductility balance of Sc-Zr-modified Al–Mg alloy by tuning bimodal microstructure via hatch spacing in laser powder bed fusion10.1016/j.matdes.2022.110976 ↗
7. Microstructural features of Sc- and Zr-modified Al-Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
8. SLM-processed Sc- and Zr-modified Al-Mg alloy: Mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
9. Effect of the heat treatment on the mechanical properties and microstructure of Scalmalloy® manufactured by Selective Laser Melting (SLM) under certified conditions10.1016/j.matchar.2022.112549 ↗
10. Deformation and fatigue behaviour of additively manufactured Scalmalloy® with bimodal microstructure10.1016/j.ijfatigue.2023.107592 ↗
11. Kuo, C.N., Peng, P.C., Liu, D.H., and Chao, C.Y. (2021). Microstructure evolution and mechanical property response of 3d-printed scalmalloy with different heat-treatment times at 325 °C. Metals, 11.10.3390/met11040555 ↗
12. (2024, June 18). Carpenter Additive Scalmalloy Datasheet. Available online: https://www.carpenteradditive.com/hubfs/Resources/Data%20Sheets/Scalmalloy_Datasheet.pdf.
13. Perander, L. Effect of Heat Treatment on the Microstructure and Mechanical Properties of LB-PBF AlSi10Mg and Scalmalloy. Proceedings of the Light Metals 2021.
14. Effect of aging treatment on the microstructure and mechanical properties of Al-3.02Mg-0.2Sc-0.1Zr alloy printed by selective laser melting10.1016/j.matdes.2019.107668 ↗
15. Deng, C., Li, R., Yuan, T., Niu, P., and Wang, Y. (2021). Microstructure and Mechanical Properties of a Combination Interface between Direct Energy Deposition and Selective Laser Melted Al-Mg-Sc-Zr Alloy. Metals, 11.10.3390/met11050801 ↗
16. Awd, M., Tenkamp, J., Hirtler, M., Siddique, S., Bambach, M., and Walther, F. (2017). Comparison of Microstructure and Mechanical Properties of Scalmalloy® Produced by Selective Laser Melting and Laser Metal Deposition. Mater, 11.10.3390/ma11010017 ↗
17. Gao, B., Zhao, H., Peng, L., and Sun, Z. (2022). A Review of Research Progress in Selective Laser Melting (SLM). Micromachines, 14.10.3390/mi14010057 ↗
18. Gokuldoss, P.K., Kolla, S., and Eckert, J. (2017). Additive Manufacturing Processes: Selective Laser Melting, Electron Beam Melting and Binder Jetting-Selection Guidelines. Materials, 10.10.3390/ma10060672 ↗
19. Materials and manufacturing renaissance: Additive manufacturing of high-entropy alloys10.1557/jmr.2020.140 ↗
20. Controls and process planning strategies for 5-axis laser directed energy deposition of Ti-6Al-4V using an 8-axis industrial robot and rotary motion
21. Gouveia, J.R., Pinto, S.M., Campos, S., Matos, J.R., Sobral, J., Esteves, S., and Oliveira, L. (2022). Life Cycle Assessment and Cost Analysis of Additive Manufacturing Repair Processes in the Mold Industry. Sustainability, 14.10.3390/su14042105 ↗
22. Directed energy deposition (DED) additive manufacturing: Physical characteristics, defects, challenges and applications10.1016/j.mattod.2021.03.020 ↗
23. Dass, A., and Moridi, A. (2019). State of the Art in Directed Energy Deposition: From Additive Manufacturing to Materials Design. Coatings, 9.10.3390/coatings9070418 ↗
24. Review of selective laser melting: Materials and applications10.1063/1.4935926 ↗
25. Directed Energy Deposition (DED) Process: State of the Art10.1007/s40684-020-00302-7 ↗
26. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
27. Froes, F., and Boyer, R. (2019). Review of Additive Manufacturing Technologies and Applications in the Aerospace Industry. Additive Manufacturing for the Aerospace Industry, Elsevier.
28. Boillat-Newport, R., Isanaka, S.P., Kelley, J., and Liou, F. (2024). Heat Treatments for Minimization of Residual Stresses and Maximization of Tensile Strengths of Scalmalloy® Processed via Directed Energy Deposition. Materials, 17.10.3390/ma17061333 ↗
29. Boillat, R., Isanaka, S.P., and Liou, F. (2021). The Effect of Nanostructures in Aluminum Alloys Processed Using Additive Manufacturing on Microstructural Evolution and Mechanical Performance Behavior. Crystals, 11.10.3390/cryst11050524 ↗
30. Kelley, J. (2024, June 18). Influence of Alloy Composition on the Process Robustness of Steels Consolidated via Laser-Directed Energy Deposition, Missouri University of Science and Technology. Available online: https://repositories.lib.utexas.edu/items/63015677-378b-4f1e-adbf-76d56a5ab816.
31. A Comparative Study on Representativeness and Stochastic Efficacy of Miniature Tensile Specimen Testing10.1520/MPC20210136 ↗
32. Caballero, F.G. (2022). Multiscale Data Driven Methodology for Accelerating Qualification and Certification of Additively Manufactured Parts. Encyclopedia of Materials: Metals and Alloys Volume 3, Elsevier.
33. (2022). Practice for Using Significant Digits in Test Data to Determine Conformance with Specifications (Standard No. ASTM E29-22 Standard).
34. (2024). Test Methods for Tension Testing of Metallic Materials (Standard No. ASTM E8-24 Standard).
35. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing10.1080/09506608.2021.1951580 ↗
36. New Nomenclatures for Heat Treatments of Additively Manufactured Titanium Alloys10.1007/s11837-017-2358-y ↗
37. Effects of Sc(Zr) on the microstructure and mechanical properties of as-cast Al–Mg alloys10.1080/02670836.2016.1270573 ↗
38. Martucci, A., Aversa, A., Manfredi, D., Bondioli, F., Biamino, S., Ugues, D., Lombardi, M., and Fino, P. (2022). Low-Power Laser Powder Bed Fusion Processing of Scalmalloy®. Materials, 15.10.3390/ma15093123 ↗
39. Influence of coherent intermetallic nano-precipitates on the nano-level mechanical and tribological properties of the Laser-Powder bed fused Scalmalloy10.1016/j.matchar.2022.112269 ↗
40. Manipulating the microstructure and tensile properties of selective laser melted Al–Mg-Sc-Zr alloy through heat treatment10.1016/j.jallcom.2020.154773 ↗
41. An improved process scan strategy to obtain high-performance fatigue properties for Scalmalloy®10.1016/j.matdes.2022.111410 ↗
42. Insights into laser powder bed fused Scalmalloy®: Investigating the correlation between micromechanical and macroscale properties10.1016/j.jmrt.2023.06.228 ↗
43. Strength-ductility synergy of selective laser melted Al-Mg-Sc-Zr alloy with a heterogeneous grain structure
44. Microstructural evolution and strengthening mechanisms of additively-manufactured Al-Mg-Sc-Zr alloys: Laser directed energy deposition versus laser powder bed fusion10.1016/j.jallcom.2024.173946 ↗
45. Nanoscale structural evolution of Al3Sc precipitates in Al(Sc) alloys10.1016/S1359-6454(01)00116-1 ↗