journal article·2020-09-26Open access

Stimulated Raman Scattering in Yttrium, Gadolinium, and Calcium Orthovanadate Crystals with Single and Combined Frequency Shifts under Synchronous Picosecond Pumping for Sub-Picosecond or Multi-Wavelength Generation around 1.2 µm

Milan Frank, Sergei N. Smetanin, Michal Jelínek, David Vyhlídal, Lyudmila I. Ivleva, Elizaveta E. Dunaeva, Irina S. Voronina, Dmitry P. Tereshchenko, Vladislav E. Shukshin, Petr G. Zverev, Václav Kubeček

Crystals· Volume 10· Issue 10

Abstract

Comparative investigation of stimulated Raman scattering (SRS) characteristics in the YVO4, GdVO4, and Ca3(VO4)2 orthovanadate crystals at both low and high frequency anionic group vibrations is presented. It was found that GdVO4 is the most perspective for SRS generation on both the ν1 stretching and ν2 bending modes of internal anionic group vibrations with the strongest SRS pulse shortening under synchronous picosecond pumping. It is as a result of GdVO4‘s widest linewidth (17cm−1) of the homogeneously broadened scheelite-type component of the bending ν2 Raman line that led to the strongest SRS pulse shortening down to the dephasing time of the widest (scheelite-type) Raman mode at the secondary intracavity short-shifted SRS conversion. It allowed us to achieve SRS pulses with sub-picosecond duration under tens-of-picoseconds pumping due to the strongest 42-fold pulse shortening. Using the Ca3(VO4)2 crystal with essentially wider Raman lines (~50cm−1) did not allow us to generate SRS pulses shorter than 1 ps. It can be explained by inhomogeneous broadening of the Raman lines in Ca3(VO4)2 because of its structural disordering. Using the measured SRS pulse duration, the homogeneous broadening of the inhomogeneously broadened bending Raman line of Ca3(VO4)2 was estimated to be ~9cm−1. Among the orthovanadate crystals, the YVO4 crystal with the highest Raman gain and with homogeneously broadened Raman lines allowed us to realize the most efficient SRS lasing and SRS pulse shortening truly down to inverse half-width of the bending Raman line.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Solid State Laser Technologies · Luminescence Properties of Advanced Materials · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Physical Electronics, Faculty of Nuclear Sciences and Physical Engineering, Czech Technical University in Prague, Břehová 7, 11519 Prague 1, Czech Republic

Research Center for Laser Materials and Technologies, Prokhorov General Physics Institute of the Russian Academy of Sciences, Vavilova 38, 119991 Moscow, Russia

References (29)

Show source-provided references
1. Zagumennyi, A.I., Mikhailov, V.A., and Shcherbakov, I.A. (2004). Rare earth ion lasers—Nd3+. Handbook of Laser Technology and Applications, Volume II: Laser Design and Laser Systems, Institute of Physics Publishing.
2. Impact of Tm3+/Ho3+ co-doping on spectroscopic and laser properties of Ca3(VO4)2 single crystal10.1016/j.jcrysgro.2019.02.054 ↗
3. Tetragonal vanadates YVO4 and GdVO4—New efficient χ(3) materials for Raman lasers10.1016/S0030-4018(01)01274-3 ↗
4. Stimulated Raman scattering of picosecond pulses in SrMoO4 and Ca3(VO4)2 crystals10.1070/QE2003v033n04ABEH002408 ↗
5. Diode pumped 500-picosecond Nd: GdVO4 Raman laser10.1002/lapl.200410057 ↗
6. Diode-pumped simultaneously Q-switched and mode-locked YVO4/Nd:YVO4/YVO4 crystal self-Raman first-Stokes laser10.1364/OE.21.019723 ↗
7. Cascaded self-Raman lasers based on 382 cm–1 shift in Nd:GdVO410.1364/OE.20.015180 ↗
8. Continuous-wave Nd: YVO4 self-Raman lasers operating at 1109 nm, 1158 nm and 1231 nm10.1364/OE.21.017745 ↗
9. 1097 nm Nd:YVO4 self-Raman laser
10. High power Stokes generation based on a secondary Raman shift of 259 cm–1 of Nd: YVO4 self-Raman crystal10.1016/j.optlastec.2018.07.067 ↗
11. Raman investigation of lattice vibration modes and thermal conductivity of Nd-doped zircon-type laser crystals10.1016/S0921-5107(03)00044-8 ↗
12. Raman scattering study of calcium orthovanadate crystal10.7567/JJAPS.24S2.508 ↗
13. Raman spectra of CaWO4, SrWO4, CaMoO4, and SrMoO410.1103/PhysRev.157.716 ↗
14. Highly efficient picosecond all-solid-state Raman laser at 1179 and 1227 nm on single and combined Raman lines in a BaWO4 crystal10.1364/OL.43.002527 ↗
15. Synchronously-pumped all-solid-state SrMoO4 Raman laser generating at combined vibrational Raman modes with 26-fold pulse shortening down to 1.4 ps at 1220 nm10.1016/j.optlastec.2018.09.045 ↗
16. Efficient synchronously-pumped all-solid-state Raman laser at 1178 and 1227 nm on stretching and bending anionic group vibrations in a SrWO4 crystal with pulse shortening down to 1.4 ps10.1016/j.optlastec.2019.105660 ↗
17. Frank, M., Smetanin, S.N., Jelínek, M., Vyhlídal, D., Shukshin, V.E., Ivleva, L.I., Dunaeva, E.E., Voronina, I.S., Zverev, P.G., and Kubeček, V. (2019). Stimulated Raman scattering in alkali-earth tungstate and molybdate crystals at both stretching and bending Raman modes under synchronous picosecond pumping with multiple pulse shortening down to 1 ps. Crystals, 9.10.3390/cryst9030167 ↗
18. 860 fs GdVO4 Raman laser at 1228 nm pumped by 36 ps, 1063 nm laser10.1088/1612-202X/ab2b92 ↗
19. Raman spectroscopic study of structural disordering in YVO4, GdVO4, and CaWO4 crystals10.1134/S1063783409090200 ↗
20. The structure of Ca3(VO4)2
21. High-temperature transformations in calcium orthovanadate studied with Raman scattering10.1021/cm9705810 ↗
22. Four-wave-mixing and nonlinear cavity dumping at 1.3 μm from Nd: SrMoO4 self-Raman laser10.1088/1612-2011/13/1/015801 ↗
23. Synchronously pumped picosecond Raman laser utilizing an LiIO3 crystal10.1070/QE1989v019n11ABEH009263 ↗
24. Synchronously pumped continuous-wave mode-locked yellow Raman laser at 559 nm10.1364/OE.17.000569 ↗
25. Pulse compression in synchronously pumped mode locked Raman lasers10.1364/OE.18.020422 ↗
26. Highly efficient picosecond diamond Raman laser at 1240 and 1485 nm10.1364/OE.22.003325 ↗
27. Efficient diamond Raman laser generating 65 fs pulses10.1364/OE.23.015504 ↗
28. 25.5 fs dissipative soliton diamond Raman laser10.1364/OL.41.001861 ↗
29. Formation of ultrashort light pulses in a laser with a bleachable filter by intracavity generation of Raman emission10.1070/QE1981v011n03ABEH006336 ↗