Origins of a Low-Sulfur Superalloy Al2O3 Scale Adhesion Map
Source abstract
Abstract
Low-sulfur single-crystal Ni-base superalloys have demonstrated excellent cyclic oxidation resistance due to improved Al2O3 scale adhesion. This derives from preventing deleterious interfacial sulfur segregation that occurs at common ppm levels of S impurity. Multiple hydrogen-annealing desulfurization treatments were employed to produce a continuum of levels demonstrating this oxidative transition, using 1 h cyclic oxidation at 1100 °C for 500 h to 1000 h. The sulfur content was determined by glow discharge mass spectrometry. The complete gravimetric database of 25 samples is revealed and correlated with sulfur content. Maximum adhesion (i.e., no weight loss) was achieved at ≤ 0.3 ppmw S, significant spallation (20–30 mg/cm2) above 2 ppmw, with transitional behavior between 0.3 and 2 ppmw S. A map suggested that adhesion was enabled when the total sulfur reservoir was less than one S atom per Ni interface atom. Equilibrium models further suggest that segregation may be minimized (~1% at 0.2 ppmw bulk), regardless of section thickness. 1st order adhesion effects have thus been demonstrated for PWA 1480 having no Y, Zr, or Hf reactive element dopants and no possibility of confounding reactive element effects. The results are compared with 2nd generation PWA 1484, Rene’N5, N6, and CMSX-4® SLS, all having Hf dopants.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Catalysis and Hydrodesulfurization Studies · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
NASA Glenn Research Center, Cleveland, OH 44135, USA
References (17)
Show source-provided references
1. Srinivasan, V., and Vedula, K. (1989). Effect of Sulfur Removal on Scale Adhesion to PWA 1480. Corrosion and Particle Erosion at High Temperatures, TMS-AIME.
2. Effect of sulfur removal on scale adhesion to PWA 148010.1007/BF02664679 ↗
3. Oxidation Resistance and Critical Sulfur Content of Single Crystal Superalloys10.1115/1.2818132 ↗
4. Effect of Hydrogen Annealing and Sulfur Content on the Oxidation Resistance of PWA 1480
5. Maintaining Adhesion of Protective Al2O3 Scales10.1007/s11837-000-0110-4 ↗
6. Toward Optimum Scale and TBC Adhesion on Single Crystal Superalloys
7. COSP for Windows: Strategies for Rapid Analyses of Cyclic Oxidation Behavior10.1023/A:1015308606869 ↗
8. Newcomb, S.B., and Bennett, M.J. (1993). A Sulfur Segregation study of PWA 1480, NiCrAl, and NiAl Alloys. Microscopy of Oxidation II, Institute of Metals.
9. Segregation Phenomena at Thermally Grown Al2O3/Alloy Interfaces10.1146/annurev.matsci.38.060407.130323 ↗
10. Sulfur Segregation on Nickel10.1016/0036-9748(85)90276-5 ↗
11. Optimizing Scale Adhesion for Single Crystal Superalloys10.4028/www.scientific.net/MSF.369-372.459 ↗
12. Smialek, J.L. (2002, January 1). Scale Adhesion, Sulfur Content, and TBC Failure on Single Crystal Superalloys. Proceedings of the 26th Annual Conference on Composites, Advanced Ceramics, Materials, and Structures: B: Ceramic En-gineering and Science Proceedings, Cocoa Beach, FL, USA.
13. Improved Oxidation Life of Segmented Plasma Sprayed 8YSZ Thermal Barrier Coatings10.1007/s11666-004-0051-5 ↗
14. Effect of sulfur on the cyclic oxidation behavior of a single crystalline, nickel-base superalloy10.1016/0921-5093(95)09819-4 ↗
15. Irvine, J.D., Vogt, R.G., Bierstine, D.L., Stabile, C.M., Mihalisin, J.R., Smith, J.S., Kunkle, J.P., Cole, G.R., and Nielsen, T.W. (1999). Ultra Low Sulfur Superalloy. (5,922,148), US Patent.
16. Gray, S., and Harris, K. (2017). Cranfield and Cannon-Muskegon, Unpublished work.
17. Harris, K. Personal communication.