Stimulated Raman Scattering in Pb(MoO4)1−x(WO4)x with x = 0, 0.5, 0.8 and 1.0 with Combined Frequency Shifts on High- and Low-Frequency Raman Modes under Synchronous Picosecond Laser Pumping
Source abstract
Abstract
Comparative characteristics of spontaneous and stimulated Raman scattering in Pb(MoO4)1−x(WO4)x single crystals (x = 0, 0.5, 0.8, and 1.0) including both the high (ν1) and low (ν2) frequency internal anionic group vibrations have been investigated. It was found that among these crystals, Pb(MoO4)0.2(WO4)0.8 is the most suitable for multi-wavelength Raman laser in several Raman modes simultaneously. This is caused by the optimal relative Mo/W content corresponding to the most efficient coherent combination of the (MoO4)2− and (WO4)2− vibrations enhancing the output radiation characteristics of the synchronously pumped Pb(MoO4)0.2(WO4)0.8 Raman laser. Oscillation of up to twelve, closely spaced SRS components in a range of 1128–1360 nm and the strongest pulse shortening down to 1.16 ps in comparison with not only PbMoO4 and PbWO4 but also with all the earlier investigated nominally pure scheelite-like tungstate and molybdate crystals has been achieved.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Solid State Laser Technologies · Luminescence Properties of Advanced Materials · Laser Design and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Faculty of Nuclear Sciences and Physical Engineering, Czech Technical University, Břehová 7, 11519 Prague, Czech Republic
Prokhorov General Physics Institute of the Russian Academy of Sciences, Vavilova 38, 119991 Moscow, Russia
State Scientific Institution, Institute for Single Crystals of National Academy of Sciences of Ukraine, Nauky Ave. 60, 61000 Kharkiv, Ukraine
Funding
European Regional Development Fund · Russian Science Foundation
References (30)
Show source-provided references
1. Lead molybdate: A melt-grown crystal with a high figure of merit for acousto-optic device applications10.1063/1.1652917 ↗
2. Physical properties of lead molybdate relevant to acousto-optic device applications10.1063/1.1660520 ↗
3. Lead tungstate (PbWO4) scintillators for LHC EM calorimetry10.1016/0168-9002(95)00589-7 ↗
4. Feasibility study of PbWO4 and PbMoO4 crystal scintillators for cryogenic rare events experiments10.1016/j.nima.2010.07.060 ↗
5. Properties of Nd3+-doped and undoped tetragonal PbWO4,NaY(WO4)2, CaWO4, and undoped monoclinic ZnWO4and CdWO4 as laser-active and stimulatedRaman scattering-active crystals10.1364/AO.38.004533 ↗
6. Multiple Stokes and anti-Stokes picosecond generation, cw laser action at wavelengths of two stimulated-emission channels 4F3/2→4I11/2 and4F3/2→4I13/2, and nanosecond self-SRS lasing in undoped and Nd3+-doped tetragonal PbMoO4 crystals
7. Highly efficient 1.3-µm second-Stokes PbWO4 Raman laser10.1364/OL.28.000426 ↗
8. Picosecond stimulated Raman scattering in crystals10.1134/1.1842874 ↗
9. Laser properties of selectively pumped Raman-active Nd3+-doped molybdate and tungstate crystals10.1070/QE2006v036n08ABEH013200 ↗
10. Laser diode pumped, actively Q-switched, and mode-locked Nd:YAG/PbWO4 Raman laser10.1364/AO.54.005375 ↗
11. Spontaneous Raman spectroscopy of tungstate and molybdate crystals for Raman lasers10.1016/S0925-3467(00)00037-9 ↗
12. BaWO4 crystal for quasi-cw yellow Raman laser
13. Cascaded self-Raman lasers based on 382 cm–1 shift in Nd:GdVO410.1364/OE.20.015180 ↗
14. Multi-wavelength passively Q-switched c-cut Nd:YVO4 self-Raman laser with Cr4+:YAG saturable absorber10.1016/j.optcom.2016.01.083 ↗
15. Xie, Z., Lou, S., Duan, Y., Li, Z., Chen, L., Wang, H., Zhang, Y., and Zhu, H. (2021). Passively Q-switched KTA cascaded Raman laser with 234 and 671 cm–1 shifts. Appl. Sci., 11.10.3390/app11156895 ↗
16. Raman spectra of CaWO4, SrWO4, CaMoO4, and SrMoO410.1103/PhysRev.157.716 ↗
17. Highly efficient picosecond all-solid-state Raman laser at 1179 and 1227 nm on single and combined Raman lines in a BaWO4 crystal10.1364/OL.43.002527 ↗
18. Frank, M., Smetanin, S.N., Jelínek, M., Vyhlídal, D., Shukshin, V.E., Ivleva, L.I., Dunaeva, E.E., Voronina, I.S., Zverev, P.G., and Kubeček, V. (2019). Stimulated Raman scattering in alkali-earth tungstate and molybdate crystals at both stretching and bending Raman modes under synchronous picosecond pumping with multiple pulse shortening down to 1 ps. Crystals, 9.10.3390/cryst9030167 ↗
19. Highly efficient, high-energy, picosecond, synchronously pumped Raman laser at 1171 and 1217 nm based on PbMoO4 crystals with single and combined Raman shifts10.1364/OE.414842 ↗
20. Growth and properties of PbWO4 and Pb(WO4)1–x(MoO4)x mixed crystals10.1016/0022-0248(78)90356-1 ↗
21. Raman scattering in Pb(MoO4)1–x(WO4)x mixed crystals10.1002/pssb.2221100148 ↗
22. Synthesis of scheelite group minerals in the CaWO4-CaMoO4-PbMoO4-PbWO4 system from aqueous solutions at 100 °C10.2473/shigentosozai.118.217 ↗
23. Structural investigation of Pb(MoxW1–x)O4 solid solutions via X-ray and neutron diffraction10.1016/j.materresbull.2016.02.036 ↗
24. Multi-wave SRS oscillation in PbMoO4 and PbMo0.5W0.5O4 crystals under 18 picosecond laser pumping10.7452/lapl.201210091 ↗
25. Application of a compact all solid-state laser system to the in situ detection of atmospheric OH, HO2, NO and IO by laser-induced fluorescence10.1039/b208714f ↗
26. Space-based, multi-wavelength solid-state lasers for NASA’s Cloud Aerosol Transport System for International Space Station (CATS-ISS)10.1117/12.2005545 ↗
27. All-solid-state, narrow linewidth, wavelength-agile terahertz-wave generator10.1063/1.2181196 ↗
28. Frank, M., Smetanin, S.N., Jelínek, M., Vyhlídal, D., Shukshin, V.E., Zverev, P.G., and Kubeček, V. (October, January 29). Laser output radiation characteristics controlled by the GdVO4 crystal length in the extracavity synchronously pumped Raman laser with combined Raman shift resulting in generation of 860 fs pulses at 1228 nm. Proceedings of the OSA Laser Congress 2019- Paper JTh3A.32, Vienna, Austria.10.1364/ASSL.2019.JTh3A.32 ↗
29. Efficient synchronously-pumped all-solid-state Raman laser at 1178 and 1227 nm on stretching and bending anionic group vibrations in a SrWO4 crystal with pulse shortening down to 1.4 ps10.1016/j.optlastec.2019.105660 ↗
30. Ordinary and extraordinary complex refractive index of the lead tungstate (PbWO4) crystal10.1016/S0168-9002(96)01016-9 ↗