Structural and Spectroscopic Features of the Bixbyite-Type Yttrium Scandate Doped by Rare-Earth Ions
Source abstract
Abstract
Yttrium scandate crystal fiber has been obtained through laser-heated pedestal growth. The crystal belongs to a bixbyite crystal structure and crystallizes in Ia3¯ space group. X-ray diffraction method shows a lattice parameter of a = 10.228(1) Å. Factor-group analysis of YScO3 Raman spectra points to high degree of disorder in crystal structure of the new compound. Spectral-kinetic investigation of the crystal fibers doped by rare-earth ions points to the presence of two independent active optical centers of rare-earth ions. Moreover, the character of rare-earth impurities’ distribution is independent on a rare-earth ionic radius size.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Glass properties and applications · Solid State Laser Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Prokhorov General Physics Institute of the Russian Academy of Sciences, 119991 Moscow, Russia
Funding
Russian Science Foundation
References (31)
Show source-provided references
1. Garlinska, M., Pregowska, A., Masztalerz, K., and Osial, M. (2020). From Mirrors to Free-Space Optical Communication—Historical Aspects in Data Transmission. Future Internet, 12.10.3390/fi12110179 ↗
2. Ligand Engineering for Broadening Infrared Luminescence of Kramers Ytterbium Ions in Disordered Sesquioxides10.1021/acs.cgd.9b00034 ↗
3. Broadening of the Fluorescence Spectra of Sesquioxide Crystals for Ultrafast Lasers10.1021/acs.cgd.0c00473 ↗
4. Spectroscopy and 2.1 μm Laser Operation of Czochralski-Grown Tm3+:YScO3 Crystals10.1364/OE.475711 ↗
5. Czochralski Growth of Mixed Cubic Sesquioxide Crystals in the Ternary System Lu2O3-Sc2O3-Y2O310.1107/S2052520621005321 ↗
6. Thermal Conductivity, Diffusivity, and Expansion of Y2O3, Y3Al5O12, and LaF3 in the Range 77–300° K10.1063/1.1709730 ↗
7. Measurement of the Optical Constants of Yttrium Oxide10.1143/JJAP.7.404 ↗
8. Dy3+:Lu2O3 as a Novel Crystalline Oxide for Mid-Infrared Laser Applications10.1364/OME.8.003447 ↗
9. Ultrashort Pulse Generation from Diode Pumped Mode-Locked Yb3+:Sesquioxide Single Crystal Lasers10.1364/OE.19.002904 ↗
10. Highly Efficient, Compact Tm3+: RE2O3 (RE = Y, Lu, Sc) Sesquioxide Lasers Based on Thermal Guiding10.1109/JSTQE.2018.2789886 ↗
11. Spectroscopy and Mode-Locking Laser Operation of Tm:LuYO3 Mixed Sesquioxide Ceramic10.1364/OE.27.024416 ↗
12. 11 W Continuous-Wave Laser Operation at 209 μm in Tm:Lu1.6Sc0.4O3 Mixed Sesquioxide Ceramics Pumped by a 796 nm Laser Diode10.1364/OME.8.003615 ↗
13. Spectroscopic Investigation and Laser Behaviour of Yb-Doped Laser Ceramics Based on Mixed Crystalline Structure (ScxY1−x)2O310.1016/j.ceramint.2021.07.116 ↗
14. High Efficiency Emission of a Laser Based on Yb-Doped (Lu,Y)2O3 Ceramics10.1016/j.optmat.2018.06.006 ↗
15. Continuously Tuned (Tm0.050Sc0.252Y0.698)2O3 Ceramic Laser with Emission Peak at 2076 nm10.1016/j.jallcom.2021.161585 ↗
16. Pirri, A., Maksimov, R.N., Li, J., Vannini, M., and Toci, G. (2022). Achievements and Future Perspectives of the Trivalent Thulium-Ion-Doped Mixed-Sesquioxide Ceramics for Laser Applications. Materials, 15.10.3390/ma15062084 ↗
17. Photoluminescence Properties of White Light Emitting La2O3:Dy3+ Nanocrystals10.1007/s12648-018-1159-7 ↗
18. Enhanced Photoluminescence and Charge Density Studies of Novel (Sm1−xGdx)2O3 Nanophosphors for WLED Applications10.1007/s10854-018-0066-1 ↗
19. Synthesis of Tm:Lu2O3 Nanocrystals for Phosphor Blue Applications10.1016/j.phpro.2010.10.025 ↗
20. Structural and Optical Properties of Thermal Decomposition Assisted Gd2O3:Ho3+/Yb3+ Upconversion Phosphor Annealed at Different Temperatures10.1016/j.saa.2016.05.010 ↗
21. Spin Localization, Magnetic Ordering, and Electronic Properties of Strongly Correlated Ln2O3 Sesquioxides (Ln=La, Ce, Pr, Nd)10.1103/PhysRevB.97.245118 ↗
22. High-Entropy, Phase-Constrained, Lanthanide Sesquioxide10.1111/jace.16689 ↗
23. Influence of Lanthanum Concentration on Microstructure of (Ho1–xLax)2O3 Magneto-Optical Ceramics10.1002/pssb.201900500 ↗
24. High-Pressure Synthesis of YScO3, HoScO3, ErScO3, and TmScO3, and a Reevaluation of the Lattice Constants of the Rare Earth Scandates10.1016/0022-4596(78)90058-0 ↗
25. Growth and Characterization of Neodymium-Doped Yttrium Scandate Crystal Fiber with a Bixbyite-Type Crystal Structure10.1021/acs.cgd.0c00389 ↗
26. Real Structure of Undoped Y2O3 Single Crystals10.1107/S0108768184001774 ↗
27. Refinement of the Structure of Scandium Sesquioxide10.1524/zkri.1967.124.1-2.136 ↗
28. Raman Spectra of R2O3 (R—Rare Earth) Sesquioxides with C-Type Bixbyite Crystal Structure: A Comparative Study10.1063/1.4894775 ↗
29. Kaminskii, A.A. (2020). Crystalline Lasers: Physical Processes and Operating Schemes, CRC Press.10.1201/9781003067962 ↗
30. Pulling Optical Fibers10.1016/0022-0248(86)90535-X ↗
31. Neodymium-Doped Graded-Index Single-Crystal Fibre Lasers10.1070/QE2006v036n07ABEH013176 ↗