Trends in Longer-Term Corrosion Loss of Magnesium Alloys
Source abstract
Abstract
The corrosion of magnesium alloys is often considered to differ in behaviour and development with time from most other metals and alloys because they show evolution of hydrogen right from first exposure. However, data extracted from the open literature indicate that magnesium alloys develop corrosion mass-loss trends with time that are consistent with the so-called bimodal pattern, which is topologically similar to those of other alloys. Examples are given of such trending for magnesium alloys under immersion, half-tide and various atmospheric exposure conditions. The critical roles of corrosion pitting and its development into localised corrosion are discussed. For high-purity magnesium alloys, the transition to longer-term corrosion, which is rate-controlled by the hydrogen evolution cathodic reaction, occurs quickly, within days. Comments are made about the application of measurements of hydrogen evolution and of electrochemical methods to make rapid estimates of shorter-term corrosion rates.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Centre for Infrastructure Performance and Reliability, The University of Newcastle, Newcastle, NSW 2308, Australia
References (33)
Show source-provided references
1. Evans, U.R. (1960). The Corrosion and Oxidation of Metals: Scientific Principles and Practical Applications, Edward Arnold.
2. Advances in Mg corrosion and research suggestions10.1016/j.jma.2013.09.003 ↗
3. Fundamentals and advances in magnesium alloy corrosion10.1016/j.pmatsci.2017.04.011 ↗
4. The electrochemical corrosion of pure magnesium in 1 N NaCl10.1016/S0010-938X(96)00172-2 ↗
5. On the development of hydrogen from the anode10.1080/14786446608644179 ↗
6. Corrosion behavior of magnesium in aqueous sulfate-containing electrolytes10.1016/j.jma.2023.06.001 ↗
7. Corrosion and protection of magnesium alloys: Recent advances and future prospects10.3390/coatings13091533 ↗
8. Recently deepened insights regarding Mg corrosion and advanced engineering applications of Mg alloys10.1016/j.jma.2023.08.012 ↗
9. Melchers, R.E. (2018). A review of trends for corrosion loss and pit depth in longer-term exposures. Corros. Mater. Degrad., 1.10.3390/cmd1010004 ↗
10. The transition from short- to long-term marine corrosion of carbon steels: 1. Experimental observations10.5006/4061 ↗
11. The transition from short- to long-term marine corrosion of carbon steels: 2. Parameterization and modeling10.5006/4062 ↗
12. Review of Mg alloy corrosion rates10.1016/j.jma.2020.08.002 ↗
13. An innovative specimen configuration for the study of Mg corrosion10.1016/j.corsci.2010.09.016 ↗
14. Southwell, C.R., Hummer, C.W., and Alexander, A.L. (1964). Corrosion of Metals in Tropical Environments, Part 6—Aluminum and Magnesium, NRL Report 6105, US Naval Research laboratory.10.21236/AD0609618 ↗
15. Schumacher, M. (1979). Seawater Corrosion Handbook, Noyes Data Corporation.
16. Atmospheric corrosion of field exposed AZ31 magnesium in a tropical marine environment10.1016/j.corsci.2013.06.047 ↗
17. Atmospheric corrosion of field-exposed magnesium alloy AZ91D10.1016/j.corsci.2007.12.005 ↗
18. Atmospheric corrosion of two field-exposed AZ31B magnesium alloys with different grain size10.1016/j.corsci.2013.02.003 ↗
19. Atmospheric corrosion of AM60 Mg alloys in an industrial environment10.1016/j.corsci.2012.11.022 ↗
20. Atmospheric corrosion of field-exposed AZ91D Mg alloys in a polluted environment10.1016/j.corsci.2010.03.011 ↗
21. Results of some marine-atmosphere corrosion tests on magnesium-Lithium alloys10.1149/1.2430032 ↗
22. Corrosion of ultra-high-purity Mg in 3.5% NaCl solution saturated with Mg(OH)210.1016/j.corsci.2013.05.018 ↗
23. Corrosion behavior of magnesium in naturally aerated stagnant seawater and 3.6% sodium chloride solutions10.1016/S1452-3981(23)19534-4 ↗
24. A Consistently Well-Behaved Method of Interpolation
25. Corrosion of mild steel in water10.1179/bcj.1995.30.1.43 ↗
26. Corrosion of AA2024-T3 Part III: Propagation10.1016/j.corsci.2010.09.035 ↗
27. Two years pitting corrosion of AA5005-H34 aluminium alloy immersed in natural seawater10.1080/1478422X.2020.1777363 ↗
28. Important early developments and current understanding of the IR mechanism of localized corrosion10.1149/1.1565142 ↗
29. Jones, D.A. (1996). Principles and Prevention of Corrosion, Prentice-Hall. [2nd ed.].
30. Pitting and sulphide inclusions in steel10.1016/S0010-938X(74)80047-8 ↗
31. An electrochemical study of phase-transitions in rust layers10.1016/0010-938X(83)90024-0 ↗
32. Leygraf, C., Wallinder, I.O., Tidblad, J., and Graedel, T. (2016). Atmospheric Corrosion, Wiley. [2nd ed.].10.1002/9781118762134 ↗
33. Influence of water velocity on marine corrosion of mild steel10.5006/1.3299235 ↗