Improved Microstructure and Enhanced Tensile Properties of Hypoeutectic AlMg5Si2Mn Alloy Modified by Yttrium
Source abstract
Abstract
AlMg5Si2Mn alloys are widely used in the field of automotive castings. Since the morphology, size, and distribution of the primary Al dendrite and eutectic Mg2Si have a decisive influence on the mechanical properties of the alloy, a comprehensive analysis of AlMg5Si2Mn alloys with varying Y contents was conducted using optical microscopy (OM), X-ray diffraction (XRD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The influence of Y on the microstructural evolution and mechanical behavior of the cast hypoeutectic AlMg5Si2Mn alloy was studied. Experimental findings indicate that the addition of Y significantly refines and alters the morphology of both primary Al and eutectic Mg2Si in AlMg5Si2Mn alloys. Specifically, in the alloy containing 0.45 wt.% Y, the primary Al undergoes a structural transformation from a coarse dendritic morphology to finer ellipsoidal grains, with a minimum secondary dendritic arm spacing (SDAS) of 18.6 ± 1.6 μm. Simultaneously, the eutectic Mg2Si morphology transitions from a coarse lamellar structure to finer worm-like, coral-like, and fibrous forms, exhibiting a reduced average length and aspect ratio (AR) of 3.1 ± 0.4. Furthermore, the AlMg5Si2Mn alloy leads to significant improvements in mechanical performance, particularly in tensile strength. The measured average ultimate tensile strength, yield strength, and elongation are 243.3 MPa, 199.0 MPa, and 8.5%, respectively, representing increases of 19.16%, 24.6%, and 203.6% compared to the Y-free alloy. The fracture mode of the alloy fracture transitioned from brittle fracture in its unmodified condition to ductile fracture characteristics.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870, China
College of Mechanical and Electrical Engineering, Jilin Institute of Chemical Technology, Jilin 132022, China
Key Laboratory of Light Metal Materials and Engineering at Universities of Liaoning Province, Shenyang University of Technology, Shenyang 110870, China
Funding
Liaoning Joint Fund of NSFC · Liaoning Natural Science Foundation
References (44)
Show source-provided references
1. Simultaneous grain refinement and eutectic Mg2Si modification in hypoeutectic Al-11Mg2Si alloys by Sc addition10.1016/j.jallcom.2019.03.326 ↗
2. Improving microstructure and mechanical properties of hypoeutecticAl-Mg2Si alloy by Gd addition10.1016/j.jallcom.2019.152178 ↗
3. Enhanced mechanical properties of hypoeutectic Al-10Mg2Si cast alloys by Bi addition10.1016/j.jallcom.2018.07.070 ↗
4. Microstructure refinement and enhanced tensile properties of Al-11Mg2Si alloy modified by erbium10.1016/j.jallcom.2020.158421 ↗
5. Effects of Bi modification and ultrasonic treatment on microstructure evolution and mechanical properties of AlMg5Si2Mn alloy10.1016/j.jallcom.2021.163486 ↗
6. Precipitation hardening and intergranular corrosion behavior of novel Al-Mg-Zn(-Cu) alloys10.1016/j.jallcom.2020.157199 ↗
7. Review of new process technologies in the aluminum die-casting industry10.1081/AMP-100108624 ↗
8. Effect of pre-homogenization deformation treatment on the workability and mechanical properties of AlMg5Si2Mn alloy10.1016/j.msea.2016.12.107 ↗
9. Effect of heat treatment on microstructure and mechanical property of Al-10%Mg2Si alloy10.1016/j.jallcom.2015.12.128 ↗
10. Microstructure and corrosion behavior of Al-10%Mg2Si cast alloy after heat treatment10.1016/j.matchar.2016.10.027 ↗
11. Effect of cooling rates during solidification of Al-5.5%Mg-2.3%Si-0.6%Mn and Al-13%Mg2Si pseudo-binary alloys on their secondary-particle morphology and tear toughness10.2320/matertrans.L-MZ201125 ↗
12. Development of an efficient grain refiner for Al-7Si alloy and its modification with strontium10.1016/S0921-5093(99)00794-7 ↗
13. Effects of modifying the hypoeutectic AlMg5Si2Mn alloy via addition of Al10Sr and/or Al5TiB
14. Grain refinement response of LM25 alloy towards Al-Ti-C and Al-Ti-B grain refine10.1016/j.jallcom.2008.04.095 ↗
15. The grain refinement of 6063 aluminum using Al-5Ti-1B and Al-3Ti-0.15C grain refiners
16. Grain refinement of A356 alloy by Al-Ti-B-C master alloy and its effect on mechanical properties10.1016/j.matdes.2012.12.033 ↗
17. The study of Li effect on the microstructure and tensile properties of cast Al-Mg2Si metal matrix composite10.1016/j.jallcom.2011.07.012 ↗
18. Effect of complex modification of Ca and Sb on the microstructure and mechanical properties of hypoeutectic Al-11Mg2Si alloy10.1016/j.jallcom.2021.159304 ↗
19. Effect of Sb modification on microstructure and mechanical properties of hypoeutectic Al-11Mg2Si alloy10.1016/j.msea.2020.139247 ↗
20. Effects of yttrium and heat treatment on the microstructure and tensile properties of Al-7.5Si-0.5Mg alloy10.1016/j.matdes.2010.08.040 ↗
21. Effect of yttrium on the microstructure of a semi-solid A356 Al alloy10.1016/S1001-0521(08)60177-1 ↗
22. Effect of trace yttrium addition on the microstructure and tensile properties of recycled Al-7Si-0.3Mg-1.0Fe casting alloys10.1016/j.msea.2016.04.036 ↗
23. The varied mechanisms of yttrium (Y) modifying a hypoeutectic Al-Si alloy under conditions of different cooling rates10.1016/j.jallcom.2019.07.107 ↗
24. Influences of Fe, Mn and Y additions on microstructure and mechanical properties of hypoeutectic Al-7%Si alloy10.1016/j.intermet.2020.106768 ↗
25. (2010). Metallic Materials—Tensile Testing—Part 1: Method of Test at Room Temperature. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China (Standard No. GB/T 228.1-2021).
26. Effect of trace La addition on the microstructures and mechanical properties of A356 (Al-7Si-0.35Mg) aluminum alloys10.1016/j.jallcom.2009.07.183 ↗
27. Solidification and structural characteristics of Al-Mg2Si eutectic10.2320/matertrans1989.38.553 ↗
28. Effect of trace Bi addition on the microstructure and mechanical properties of hypoeutectic Al-Mg-Si-Mn alloy10.1016/j.mtcomm.2024.110954 ↗
29. Modification of eutectic Si and the microstructure in an Al-7Si alloy with barium addition10.1016/j.msea.2018.05.010 ↗
30. Effects of neodymium addition on microstructure and mechanical properties of near-eutectic Al-12Si alloys10.1016/S1003-6326(15)64035-3 ↗
31. The synergic effects of Sc and Zr on the microstructure and mechanical properties of Al-Si-Mg alloy10.1016/j.matdes.2015.09.045 ↗
32. Experimental investigation of the Al-Y particle diagram10.1016/j.jallcom.2005.06.078 ↗
33. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron10.1007/BF02642799 ↗
34. Calculation of planar disregistries between compounds of rare earth-Al and primary α particle in A356-RE alloy and its verification
35. Modification of eutectic Si in Al-Si alloys with Eu addition10.1016/j.actamat.2014.10.064 ↗
36. Experimental and theoretical investigation on refining mechanism of Mg2Si by Y addition in the Mg-Al-Si alloys10.1016/j.jallcom.2024.175432 ↗
37. Effect of yttrium addition on the microstructures and mechanical properties of hypereutectic Al-20Si alloy10.1016/j.msea.2018.03.015 ↗
38. Effect of rare earth cerium addition on the microstructure and tensile properties of hypereutectic Al-20% Si alloy10.1016/j.jallcom.2013.02.016 ↗
39. The role of trace element segregation in the eutectic modification of hypoeutectic Al-Si alloys10.1016/j.jallcom.2009.09.138 ↗
40. Effect of modification treatment on the microstructure and mechanical properties of Al-0.35%Mg-7.0%Si cast alloy10.1016/j.matdes.2010.04.032 ↗
41. Effects of Sc and Zr microalloying additions on the microstructure and mechanical properties of new Al-Zn-Mg alloys10.1016/j.jallcom.2012.03.108 ↗
42. Effect of precipitate shape and orientation on Orowan strengthening of non-basal slip modes in hexagonal crystals, application to magnesium alloys10.1016/j.msea.2016.04.056 ↗
43. Effect of microstructure on cleavage fracture toughness of quenched and tempered steels10.1179/msc.1979.13.6.341 ↗
44. The phenomenon of rupture and flow in solids