journal article·2014-12

Thermoelectric generator based on a bismuth-telluride alloy fabricated by addition of ethylene glycol

Kyung Kuk Jung, Jong Soo Ko

Current Applied Physics· Volume 14· Issue 12
Publisher page

Abstract

Abstract This paper introduces a new method to selectively fabricate n-type and p-type bismuth (Bi)-telluride (Te) thermoelectric materials by the rate of addition of ethylene glycol (EG) in the Bi–Te co-electrodeposition solution. As the amount of added EG is increased, the atomic ratio of Bi in the deposited Bi–Te alloy reached a slope of 0.463 (at.% of Bi/vol.% of EG), and increased in a linear manner. When the EG content reached approximately 20%v/v, the n-type material changed into a p-type. This change implies that adjusting the EG content in the electrodeposition solution affords simple control of the Bi–Te composition. To demonstrate the applicability of the developed thermoelectric materials, thermoelectric generators (TEGs) were fabricated using electrodeposited n-type (using solution without EG) and p-type (using solution with 30%v/v EG) Bi–Te alloys. The Seebeck voltage of the pair of n-type and p-type thermoelectric materials was 140 mV and the power generated from the pair was 24.36 nW at a 10 °C temperature difference.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Thermoelectric Materials and Devices · Chalcogenide Semiconductor Thin Films · Transition Metal Oxide Nanomaterials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Thermoelectric converters of human warmth for self-powered wireless sensor nodes10.1109/JSEN.2007.894917 ↗
2. Preparation and characterization of p-type Sb2Te3 and n-type Bi2Te3 thin films grown by coevaporation10.1116/1.1354600 ↗
3. Effect of deposition temperature on the structural and thermoelectric properties of bismuth telluride thin films grown by co-sputtering10.1016/j.tsf.2005.12.306 ↗
4. MOCVD of Bi2Te3, Sb2Te3 and their superlattice structures for thin-film thermoelectric applications10.1016/S0022-0248(96)00656-2 ↗
5. Preparation of Bi2Te3 films by electrodeposition from solution containing Bi-ethylenediaminetetraacetic acid complex and TeO210.1149/1.1542898 ↗
6. Fabrication of nanostructured thermoelectric bismuth telluride thick films by electrochemical deposition10.1021/cm060171o ↗
7. Fabrication and characterization of electrodeposited bismuth telluride films and nanowires10.1021/jp909926z ↗
8. Electrodeposition of bismuth telluride thermoelectric films from a nonaqueous electrolyte using ethylene glycol10.1016/j.electacta.2012.01.091 ↗
9. Surfactant-mediated electrodeposition of bismuth telluride films and its effect on microstructural properties10.1021/la301367m ↗
10. Novel mixed method for the electrochemical deposition of thick layers of Bi2+xTe3−x with controlled stoichiometry10.1016/j.electacta.2008.06.065 ↗
11. Optimization and fabrication of thick flexible polymer based micro thermoelectric generator10.1016/j.sna.2006.04.024 ↗
12. Pulse and pulse reverse plating-conceptual, advantages and applications10.1016/j.electacta.2007.11.054 ↗
13. Table of standard electrode potentials10.1149/1.2131790 ↗
14. Bard · 1985
15. The composition of electrodeposited Zinc-nickel alloy coatings10.1149/1.2100681 ↗
16. The study of hydrophilic characteristics of ethylene glycol