journal article·2013-03

Temperature dependent electrophysical characteristics of GaAs-polymer composite varistors

H. Bidadi, S. Mohammadi Aref, M. Ghafouri, M. Parhizkar, A. Olad

Current Applied Physics· Volume 13· Issue 2
Publisher page

Abstract

Abstract A composition of GaAs-polymer tiny particles was pressed at a temperature of 130 °C and a pressure of 60 MPa and its current–voltage characteristic was studied. The result shows that the prepared disk has varistor behavior and can therefore be used to protect circuits from low overvoltage transients higher than 62 V. Temperature dependence of current-voltage characteristic and the electrical conductivity of the sample were investigated in the temperature range of 25–100 °C. It has been found that increase in temperature results in lower breakdown voltage and nonlinearity coefficient. At high temperatures, nonlinearity in the I–V characteristic of sample disappears and the conductivity becomes Ohmic in nature. The sample has hysteresis which decreases through increase in temperature. Annealing effect on leakage current and breakdown voltage was both investigated and analyzed using SEM micrographs. Finally, the electrical bandgap of the sample was measured.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and interfaces · Semiconductor materials and devices · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Nahm · Ceram. Int. · 2012 · 38 · 259310.1016/j.ceramint.2011.10.050 ↗
2. Bueno · J. Appl. Phys. · 1998 · 84 · 370010.1063/1.368587 ↗
3. Mergen · J. Eur. Ceram. Soc. · 1996 · 16 · 104110.1016/0955-2219(96)00037-4 ↗
4. Levinson · Am. Ceram. Soc. Bull. · 1986 · 65 · 639
5. Gupta · J. Am. Ceram. Soc. · 1990 · 73 · 181710.1111/j.1151-2916.1990.tb05232.x ↗
6. Nahm · J. Phys. Chem. Solids · 2012 · 73 · 83410.1016/j.jpcs.2012.02.007 ↗
7. Zhu · Ceram. Int. · 2012 · 38S · S46310.1016/j.ceramint.2011.05.040 ↗
8. Cheng · Ceram. Int. · 2012 · 38S · S45710.1016/j.ceramint.2011.05.039 ↗
9. Sönmezoglu · Curr. Appl. Phys. · 2012 · 12 · 137210.1016/j.cap.2012.03.030 ↗
10. Liu · Solid State Electron. · 2005 · 49 · 107710.1016/j.sse.2005.05.006 ↗
11. Ghosh · J. Appl. Phys. · 1980 · 51 · 215310.1063/1.327888 ↗
12. Farag · Curr. Appl. Phys. · 2012 · 12 · 143610.1016/j.cap.2012.03.032 ↗
13. Cristovan · Synth. Met. · 2011 · 161 · 204110.1016/j.synthmet.2011.06.030 ↗
14. Cao · Polymer · 1989 · 30 · 230510.1016/0032-3861(89)90266-8 ↗
15. Lin · Ceram. Int. · 2008 · 34 · 13110.1016/j.ceramint.2006.09.018 ↗
16. Bidadi · Vacuum · 2010 · 84 · 123210.1016/j.vacuum.2009.10.031 ↗
17. Matsuoka · J. Appl. Phys. · 1971 · 10 · 73610.1143/JJAP.10.736 ↗
18. Levinson · Ceram. Trans. · 1989 · 3 · 145
19. Tu · Colloids Surf. A · 2012 · 407 · 12610.1016/j.colsurfa.2012.05.019 ↗
20. Solymar · 2010