Numerical and Test Evaluation on Adhesion Properties in Cr/Al Interface Film Structure
Source abstract
Abstract
The aim of this article is to provide a systematic method to perform experimental test and theoretical evaluation on adhesion properties of the Cr/Al interface structure. A specified Cr/Al interface film assembly was deposited on the quartz glass by using RF magnetron sputtering. The elastic modulus and the hardness of the sample are tested by the nanoindentation tester. The test results show that the elastic modulus and the hardness of the sample have a nonlinear characteristic with different depth h of the interface structure. In the meantime, a finite element model is built to simulate the interface characteristics of the sample. The analysis shows that the stress mainly centralizes close to the top of the nanoindentation tester and the maximum stress occurs in the second layer Al film, not the first layer Cr film. The comparison between the test and the simulation shows the validity of the experimental test and the modeling method of each other. It builds a basis for future work such as fabrication of Cr/Al interface structure for micro/nano manufacturing.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Copper Interconnects and Reliability · Electronic Packaging and Soldering Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.