journal article·2000-03

Flexural properties and impact strength of denture base polymer reinforced with woven glass fibers

T Kanie, K Fujii, H Arikawa, K Inoue

Dental Materials· Volume 16· Issue 2
Publisher page

Abstract

Objectives The present investigation was undertaken to determine the reinforcing effect of woven glass fibers on deflection, flexural strength, flexural modulus and impact strength of acrylic denture base polymer. Methods Three silanized or unsilanized woven glass fibers were used. Specimens were made by heating the denture cure resin dough containing glass fibers, which were sheathed in the dough. Specimens with four different thicknesses and of five different types were made, incorporating the glass fiber. Three-point flexural test and flywheel type impact test were employed to determine the flexural properties and impact strength. Results When specimens contained unsilanized glass fiber, the flexural strength in specimens of 1 and 2 mm thickness and the impact strength in specimens of 2 mm thickness were higher than those of specimens without glass fiber (p < 0.01). On the contrary, the flexural strength and deflection in specimens reinforced with silanized glass fiber of 1 mm thickness were significantly higher (p < 0.01, p < 0.05) than those of unreinforced specimens. Further, the impact strength in specimens reinforced with silanized glass fiber of 2 mm thickness was significantly higher (p < 0.01) than that of unreinforced specimens. Statistically significant differences were found in the flexural strength (p < 0.05) and in the impact strength (p < 0.01) when specimens of 4 mm thickness were reinforced with two or three unsilanized glass fibers. Significance The reinforcement with glass fiber was effective in thin specimens, and the reinforcing effect increased with the increase of the number of glass fibers in the case of thick specimens.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Mechanical Behavior of Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Wire reinforcement of acrylic resin prostheses10.1016/0022-3913(84)90132-X ↗
2. Effect of steel strengtheners on fracture resistance of the acrylic resin complete denture base10.1016/S0022-3913(85)80074-3 ↗
3. Comparison of the in vitro fatigue resistance of an acrylic resin removable partial denture reinforced with continuous glass fibers or metal wires10.1111/j.1532-849X.1996.tb00285.x ↗
4. Carbon fiber acrylic resin composite: an investigation of transverse strength10.1016/0022-3913(85)90431-7 ↗
5. Carbon/graphite fiber reinforced poly(methyl methacrylate): properties under dry and wet conditions10.1002/jbm.820210902 ↗
6. Denture base poly(methyl methacrylate) reinforced with ultra-high modulus polyethylene fibres10.1038/sj.bdj.4806373 ↗
7. The effect of including ultra-high-modulus polyethylene fiber on the impact strength of acrylic resin10.1038/sj.bdj.4806395 ↗
8. Fracture resistance of Kevlar-reinforced poly(methyl methacrylate) resin: a preliminary study
9. Reinforcement of poly(methyl methacrylate) with ultra-high-modulus polyethylene fibre10.1016/0300-5712(92)90012-2 ↗
10. Polyethylene fiber reinforced poly (methyl methacrylate)—water sorption and dimensional changes during immersion10.1016/0300-5712(93)90014-H ↗
11. Effect of five woven fiber reinforcements on the impact and transverse strength of a denture base resin10.1016/S0022-3913(99)70218-0 ↗
12. The effect of plasma-treated polyethylene fiber on the fracture strength of polymethyl methacrylate10.1016/S0022-3913(96)90348-0 ↗
13. Fracture strengths of provisional restorations reinforced with plasma-treated woven polyethylene fiber10.1016/S0022-3913(97)70058-1 ↗
14. The effect of methyl methacrylate reinforcement with silane-treated and untreated glass fibers10.1016/0022-3913(91)90255-U ↗
15. Reinforcement of acrylic resin denture base material with metal or fiber strengtheners10.1111/j.1365-2842.1992.tb01096.x ↗
16. Comparison of two different silane compounds used for improving adhesion between fibers and acrylic denture base material10.1111/j.1365-2842.1993.tb01640.x ↗
17. Acrylic resin–fiber composite—Part I. The effect of fiber concentration on fracture resistance10.1016/0022-3913(94)90446-4 ↗
18. Acrylic resin–fiber composite—Part II. The effect of polymerization shrinkage of polymethyl methacrylate applied to fiber roving on transverse strength10.1016/0022-3913(94)90447-2 ↗
19. Transverse strength and fatigue of denture acrylic–glass fiber composite10.1016/0109-5641(94)90051-5 ↗
20. Impact strength of denture polymethyl methacrylate reinforced with continuous glass fibers or metal wire10.3109/00016359509006007 ↗
21. The effect of void space and polymerization time on transverse strength of acrylic–glass fiber composite10.1111/j.1365-2842.1995.tb00083.x ↗
22. Dimensional accuracy and stability of polymethyl methacrylate reinforced with metal wire or continuous glass fiber10.1016/S0022-3913(96)90246-2 ↗
23. Curing of a silane coupling agent and its effect on the transverse strength of autopolymerizing polymethylmethacrylate–glass fibre composite10.1046/j.1365-2842.1997.00464.x ↗
24. Impact strength of a modified continuous glass fiber–poly(methyl methacrylate)
25. Effect of glass fiber reinforcement on some mechanical properties of autopolymerizing polymethyl methacrylate10.1016/S0022-3913(98)70180-5 ↗
26. Effect of water storage on the flexural properties of E-glass and silica fiber acrylic resin composite
27. Some aspects of the tensile strength of unidirectional glass fibre–polymethyl methacrylate composite used in dentures10.1046/j.1365-2842.1998.00235.x ↗
28. Flexural properties of acrylic resin polymers reinforced with unidirectional and woven glass fibers10.1016/S0022-3913(99)70276-3 ↗
29. The effect of carbon fiber orientation on the fatigue resistance and bending properties of two denture resins10.1016/S0022-3913(84)80117-1 ↗
30. Denture base PMMA resins reinforced with carbon fibers. Part 1. Surface treatments of the carbon fibers and its effects on flexural and tensile strength of the reinforced resins
31. Denture base PMMA resins reinforced with carbon fibers. Part 2. Effects of thickness and number of carbon fiber sheets on physical properties of reinforced specimen
32. Studies on denture base resins reinforced with carbon or aramid fiber. Part 1. The effectiveness of including fiber and surface treatments10.2186/jjps.37.1083 ↗
33. Impact properties of dental materials10.1038/sj.bdj.4802614 ↗
34. Impact properties of acrylic denture base resin. Part 1. A new method for determination of impact properties10.4012/dmj.7.166 ↗