journal article·2014-04

Mechanical fatigue degradation of ceramics versus resin composites for dental restorations

Renan Belli, Eva Geinzer, Anna Muschweck, Anselm Petschelt, Ulrich Lohbauer

Dental Materials· Volume 30· Issue 4
Publisher page

Abstract

Objectives For posterior partial restorations an overlap of indication exists where either ceramic or resin-based composite materials can be successfully applied. The aim of this study was to compare the fatigue resistance of modern dental ceramic materials versus dental resin composites in order to address such conflicts. Methods Bar specimens of five ceramic materials and resin composites were produced according to ISO 4049 and stored for 14 days in distilled water at 37°C. The following ceramic materials were selected for testing: a high-strength zirconium dioxide (e.max ZirCAD, Ivoclar), a machinable lithium disilicate (e.max CAD, Ivoclar), a pressable lithium disilicate ceramic (e-max Press, Ivoclar), a fluorapatite-based glass-ceramic (e.max Ceram, Ivoclar), and a machinable color-graded feldspathic porcelain (Trilux Forte, Vita). The composite materials selected were: an indirect machinable composite (Lava Ultimate, 3M ESPE) and four direct composites with varying filler nature (Clearfil Majesty Posterior, Kuraray; GrandioSO, Voco; Tetric EvoCeram, Ivoclar-Vivadent; and CeramX Duo, Dentsply). Fifteen specimens were tested in water for initial strength (σin) in 4-point bending. Using the same test set-up, the residual flexural fatigue strength (σff) was determined using the staircase approach after 10(4) cycles at 0.5 Hz (n=25). Weibull parameters σ0 and m were calculated for the σin specimens, whereas the σff and strength loss in percentage were obtained from the fatigue experiment. Results The zirconium oxide ceramic showed the highest σin and σff (768 and 440 MPa, respectively). Although both lithium disilicate ceramics were similar in the static test, the pressable version showed a significantly higher fatigue resistance after cyclic loading. Both the fluorapatite-based and the feldspathic porcelain showed equivalent initial and cyclic fatigue properties. From the composites, the highest filled direct material Clearfil Majesty Posterior showed superior fatigue performance. From all materials, e.max Press and Clearfil Majesty Posterior showed the lowest strength loss (29.6% and 32%, respectively), whereas the other materials lost between 41% and 62% of their flexural strength after cyclic loading. Conclusions Dental ceramics and resin composite materials show equivalent fatigue strength degradation at loads around 0.5σin values. Apart from the zirconium oxide and the lithium disilicate ceramics, resin composites generally showed better σff after 10,000 cycles than the fluorapatite glass-ceramic and the feldspathic porcelain. Resin composite restorations may be used as an equivalent alternative to glass-rich-ceramic inlays regarding mechanical performance.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Health and Care Utilization · Dental Research and COVID-19

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Can hygroscopic expansion compensate for the polymerization shrinkage? Part I. Deformation of restored teeth10.1016/j.dental.2010.09.007 ↗
2. Longevity of posterior composite restorations: not only a matter of materials10.1016/j.dental.2011.09.003 ↗
3. Patient risk factors’ influence on survival of posterior composites10.1177/0022034513484337 ↗
4. Influence of microstructure and chemistry on the fracture toughness of dental ceramics10.1016/S0109-5641(03)00002-2 ↗
5. Resin composite – state of the art10.1016/j.dental.2010.10.020 ↗
6. Effect of microstructure on the lifetime of dental ceramics10.1016/j.dental.2011.04.003 ↗
7. Slow crack growth and reliability of dental ceramics10.1016/j.dental.2010.10.025 ↗
8. Resin-based composite performance: Are there some things we can’t predict10.1016/j.dental.2012.06.013 ↗
9. Fracture behavior of lithia disilicate- and leucite-based ceramics10.1016/j.dental.2004.02.004 ↗
10. Influence of surface roughness on mechanical strength of resin composite versus glass ceramic materials10.1016/j.dental.2007.05.006 ↗
11. Investigations of subcritical crack propagation of the Empress 2 all-ceramic system10.1016/j.dental.2007.05.010 ↗
12. Standardizing failure, success, and survival decisions in clinical studies of ceramic and metal–ceramic fixed dental prostheses10.1016/j.dental.2011.09.012 ↗
13. Correlation of clinical performance with ‘in vitro tests’ of restorative dental materials that use polymer-based matrices10.1016/j.dental.2011.08.594 ↗
14. Factors involved in the fatigue degradation of dental resin composites10.1177/0022034513490734 ↗
15. Are linear elastic material properties relevant predictors of the fatigue resistance of dental resin composites?10.1016/j.dental.2014.01.009 ↗
16. Correlation of in vitro fatigue data and in vivo clinical performance of a glass ceramic material10.1016/j.dental.2007.01.011 ↗
17. Fatigue of tooth-colored restoratives in aqueous environment10.4012/dmj.26.1 ↗
18. Mechanical fatigue of a feldspathic dental porcelain10.1016/0109-5641(93)90071-W ↗
19. R-curve behavior and micromechanisms of fracture in resin based dental restorative composites10.1016/j.jmbbm.2008.12.005 ↗
20. A comparison of fatigue crack growth in resin composite, dentin and the interface10.1016/j.dental.2006.05.003 ↗
21. Fatigue behavior of resin composites in aqueous environments10.1016/j.dental.2006.06.031 ↗
22. European Standard EN-843/5 · 1997
23. Fatigue mechanisms in high-strength silica-glass fibers10.1111/j.1151-2916.1991.tb07820.x ↗
24. Engineering design and fatigue failure of brittle materials
25. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
26. Lifetime prediction of CAD/CAM dental ceramics10.1002/jbm.10468 ↗
27. Analysis of subcritical crack growth in dental ceramics using fracture mechanics and fractography10.1016/j.dental.2007.08.001 ↗
28. Phenomena and mechanics of crack propagation in glass-ceramics10.1016/j.jmbbm.2007.11.005 ↗
29. In vitro lifetime of dental ceramics under cyclic loading in water10.1016/j.biomaterials.2006.12.033 ↗
30. Fatigue of zirconia under cyclic loading in water and its implications for the design of dental bridges10.1016/j.dental.2005.12.008 ↗
31. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses10.1016/S0142-9612(01)00206-X ↗
32. The tetragonal-monoclinic in zirconia; lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
33. Subcritical crack growth and thresholds in a 3Y-TZP ceramic under static and cyclic loading conditions10.1016/S0272-8842(96)00037-5 ↗
34. Static and cyclic crack propagation in Ce-TZP ceramics with different amounts of transformation toughening10.1016/j.jeurceramsoc.2006.04.108 ↗
35. Hygroscopic and hydrolytic effects in dental polymer networks10.1016/j.dental.2005.05.005 ↗
36. Fatigue behaviour of dental composite materials10.1016/j.jdent.2008.12.008 ↗
37. Cyclic loading of notched dental composite specimens10.1016/j.dental.2009.10.002 ↗
38. Effect of cyclic loading and environmental aging on the fracture toughness of dental resin composite10.1002/jbm.b.30588 ↗
39. R-curve behavior and toughening mechanisms of resin-based dental composites: effects of hydration and post-cure heat treatment10.1016/j.dental.2008.12.004 ↗
40. Fracture resistance curves and toughening mechanisms in polymer based dental composites10.1016/j.jmbbm.2011.01.003 ↗
41. Subcritical crack growth and in vivo lifetime prediction of resin composites with different filler distribution10.1016/j.dental.2012.05.001 ↗
42. Survival of inlays and partial crowns made of IPS Empress after a 10-year observation period and in relation to various treatment parameters10.2341/07-13 ↗
43. Computer-aided direct ceramic restorations: a 10-years prospective clinical study of Cerec CAD/CAM inlays and onlays
44. Leucita-reinforced glass ceramic inlays and onlays after 12 years
45. Clinical evaluation of ceramic inlays compared to composite restorations10.2341/08-95 ↗
46. 22-Year clinical evaluation of the performance of two posterior composites with different filler characteristics10.1016/j.dental.2011.06.001 ↗
47. Clinical evaluation of posterior composite restorations: the 10-year report
48. A retrospective clinical study on longevity of posterior composite and amalgam restorations10.1016/j.dental.2005.11.036 ↗
49. Durability of resin composite restorations in high C-factor cavities: a 12-year follow-up10.1016/j.jdent.2010.02.007 ↗
50. The clinical success of all-ceramic restorations10.14219/jada.archive.2008.0361 ↗
51. Longevity of resin composite restorations10.1016/j.jdsr.2010.05.002 ↗
52. Operator vs. material influence on clinical outcome of bonded ceramic inlays10.1016/j.dental.2009.02.002 ↗
53. Clinical study of indirect composite resin inlays in posterior stress-bearing cavities placed by dental students: Results after 4 years10.1016/j.jdent.2011.04.005 ↗
54. Composite resin fillings and inlays. An 11-year evaluation10.1007/s00784-003-0201-z ↗