journal article·2016-07Open access

Microstructure characterization and SCG of newly engineered dental ceramics

Nathália de Carvalho Ramos, Tiago Moreira Bastos Campos, Igor Siqueira de La Paz, João Paulo Barros Machado, Marco Antonio Bottino, Paulo Francisco Cesar, Renata Marques de Melo

Dental Materials· Volume 32· Issue 7

Abstract

Objectives The aim of this study was to characterize the microstructure of four dental CAD-CAM ceramics and evaluate their susceptibility to stress corrosion. Methods SEM and EDS were performed for microstructural characterization. For evaluation of the pattern of crystallization of the ceramics and the molecular composition, XRD and FTIR, respectively, were used. Elastic modulus, Poisson's ratio, density and fracture toughness were also measured. The specimens were subjected to biaxial flexure under five stress rates (0.006, 0.06, 0.6, 6 and 60MPa/s) to determine the subcritical crack growth parameters (n and D). Twenty-five specimens were further tested in mineral oil for determination of Weibull parameters. Two hundred forty ceramic discs (12mm diameter and 1.2mm thick) were made from four ceramics: feldspathic ceramic - FEL (Vita Mark II, Vita Zahnfabrik), ceramic-infiltrated polymer - PIC (Vita Enamic, Vita Zahnfabrik), lithium disilicate - LD (IPS e.max CAD, Ivoclar Vivadent) and zirconia-reinforced lithium silicate - LS (Vita Suprinity, Vita Zahnfabrik). Results PIC discs presented organic and inorganic phases (n=29.1±7.7) and Weibull modulus (m) of 8.96. The FEL discs showed n=36.6±6.8 and m=8.02. The LD discs showed a structure with needle-like disilicate grains in a glassy matrix and had the lowest value of n (8.4±0.8) and m=6.19. The ZLS discs showed similar rod-like grains, n=11.2±1.4 and m=9.98. Significance The FEL and PIC discs showed the lowest susceptibility to slow crack growth (SCG), whereas the LD and ZLS discs presented the highest. PIC presented the lowest elastic modulus and no crystals in its composition, while ZLS presented tetragonal zirconia. The overall strength and SCG of the new materials did not benefit from the additional phase or microconstituents present in them.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
2. In-vitro strength degradation of dental ceramics and novel PICN material by sharp indentation10.1016/j.jmbbm.2013.05.004 ↗
3. Monolithic CAD/CAM lithium disilicate versus veneered Y-TZP crowns: comparison of failure modes and reliability after fatigue
4. ISO 6872. · 1999
5. Fracture toughness testing of small ceramic discs and plates10.1016/j.jeurceramsoc.2013.12.021 ↗
6. ASTM C1368-10. · 2011
7. FT-IR monomer conversion analysis of UDMA-based dental resins10.1111/j.1365-2842.1996.tb00903.x ↗
8. Materials for chairside CAD/CAM-produced restorations10.14219/jada.archive.2006.0397 ↗
9. Characterization of a polymer-infiltrated ceramic-network material10.1016/j.dental.2014.02.019 ↗
10. Zahnfabrik · 2013
11. A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics10.1002/1097-4636(2000)53:4<297::AID-JBM3>3.0.CO;2-G ↗
12. Phenomena and mechanisms of crack propagation in glass-ceramics10.1016/j.jmbbm.2007.11.005 ↗
13. Slow crack growth and reliability of dental ceramics10.1016/j.dental.2010.10.025 ↗
14. Investigations of subcritical crack propagation of the Empress 2 all-ceramic system10.1016/j.dental.2007.05.010 ↗
15. Gilbertson · 1981