journal article·2011-04

Slow crack growth and reliability of dental ceramics

Carla Castiglia Gonzaga, Paulo Francisco Cesar, Walter Gomes Miranda, Humberto Naoyuki Yoshimura

Dental Materials· Volume 27· Issue 4
Publisher page

Abstract

Objective To determine the slow crack growth (SCG) and Weibull parameters of five dental ceramics: a vitreous porcelain (V), a leucite-based porcelain (D), a leucite-based glass-ceramic (E1), a lithium disilicate glass-ceramic (E2) and a glass-infiltrated alumina composite (IC). Methods Eighty disks (Ø 12 mm × 1.1mm thick) of each material were constructed according to manufacturers' recommendations and polished. The stress corrosion susceptibility coefficient (n) was obtained by dynamic fatigue test, and specimens were tested in biaxial flexure at five stress rates immersed in artificial saliva at 37 °C. Weibull parameters were calculated for the 30 specimens tested at 1 MPa/s in artificial saliva at 37 °C. The 80 specimens were distributed as follows: 10 for each stress rate (10(-2), 10(-1), 10(1), 10(2)MPa/s), 10 for inert strength (10(2)MPa/s, silicon oil) and 30 for 10(0)MPa/s. Fractographic analysis was also performed to investigate the fracture origin. Results E2 showed the lowest slow crack growth susceptibility coefficient (17.2), followed by D (20.4) and V (26.3). E1 and IC presented the highest n values (30.1 and 31.1, respectively). Porcelain V presented the lowest Weibull modulus (5.2). All other materials showed similar Weibull modulus values, ranging from 9.4 to 11.7. Fractographic analysis indicated that for porcelain D, glass-ceramics E1 and E2, and composite IC crack deflection was the main toughening mechanism. Significance This study provides a detailed microstructural and slow crack growth characterization of widely used dental ceramics. This is important from a clinical standpoint to assist the clinician in choosing the best ceramic material for each situation as well as predicting its clinical longevity. It also can be helpful in developing new materials for dental prostheses.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Ten-year outcome of crowns placed within the General Dental Services in England and Wales10.1016/j.jdent.2008.03.017 ↗
2. Green · 1998
3. Wachtman · 1996
4. Predicting lifetimes of materials and material structures10.1016/0109-5641(95)80050-6 ↗
5. Design data for engineering ceramics: a review of the flexure test10.1111/j.1151-2916.1991.tb08259.x ↗
6. A practical and systematic review of Weibull statistics for reporting strengths of dental materials
7. Critique of test methods for lifetime predictions10.1016/0109-5641(95)80051-4 ↗
8. Fatigue of dental ceramics in a simulated oral environment10.1177/00220345860650071901 ↗
9. Influence of pH on slow crack growth of dental porcelains10.1016/j.dental.2007.10.001 ↗
10. Lifetime prediction of all-ceramic bridges by computational methods10.1177/154405910308200317 ↗
11. Correlation of in vitro fatigue data and in vivo clinical performance of a glass ceramic material10.1016/j.dental.2007.01.011 ↗
12. Lifetime prediction of CAD/CAM dental ceramics10.1002/jbm.10468 ↗
13. Investigations of subcritical crack propagation of the Empress 2 all-ceramic system10.1016/j.dental.2007.05.010 ↗
14. Dynamic fatigue and strength characterization of three ceramic materials10.1007/s10856-007-0131-4 ↗
15. Lifetime of alumina- and zirconia ceramics used for crown and bridge restorations10.1002/jbm.b.30599 ↗
16. Dynamic fatigue of feldspathic porcelain10.1016/0109-5641(93)90073-Y ↗
17. Analysis of subcritical crack growth in dental ceramics using fracture mechanics and fractography10.1016/j.dental.2007.08.001 ↗
18. Influence of leucite content on slow crack growth of dental porcelains10.1016/j.dental.2008.01.003 ↗
19. Fatigue failure parameters of IPS-Empress porcelain
20. Fatigue characteristics of a high-strength porcelain
21. Biaxial flexural strength, elastic moduli, and X-ray diffraction characterization of three pressable all-ceramic materials10.1067/mpr.2003.42 ↗
22. Influence of test method on failure stress of brittle dental materials10.1177/00220345900690120201 ↗
23. Flexural strength optimisation of a leucite reinforced glass ceramic10.1016/S0109-5641(00)00046-4 ↗
24. The biaxial flexural strength and reliability of four dental ceramics. Part II10.1016/S0300-5712(96)00059-0 ↗
25. The transverse strength, reliability and microstructural features of four dental ceramics. Part I10.1016/S0300-5712(96)00058-9 ↗
26. Relationship between fracture toughness and flexural strength in dental porcelains10.1002/jbm.b.30482 ↗
27. Strength, reliability, and mode of fracture of bilayered porcelain/core ceramics
28. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
29. Biaxial flexural strength and indentation fracture toughness of three new dental core ceramics10.1016/S0022-3913(96)90297-8 ↗
30. Comparative mechanical property characterization of 3 all-ceramic core materials
31. Fracture toughness of dental porcelains evaluated by IF SCF, and SEPB methods10.1111/j.1551-2916.2005.00334.x ↗
32. ASTM-C1161 · 2002
33. ASTM-C1368 · 2001
34. Strength–probability–time (SPT) relationships in ceramics10.1007/BF02403519 ↗
35. Alternating demineralization and remineralization of artificial enamel lesions10.1159/000260599 ↗
36. ASTM-F394-78 · 1996
37. Biaxial flexure test of ceramic substrates
38. Porosity dependence of elastic constants in aluminum nitride ceramics10.1590/S1516-14392007000200006 ↗
39. ASTM-C1499 · 2009
40. Ball-on-ring test revisited10.1111/j.1151-2916.1989.tb07702.x ↗
41. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
42. ASTM-C1239 · 2000
43. High temperature flexural strength and fracture toughness of AlN with Y2O3 ceramic10.1007/s10853-009-3809-9 ↗
44. Effect of processing induced particle alignment on the fracture toughness and fracture behavior of multiphase dental ceramics10.1016/j.dental.2009.03.013 ↗
45. Fractography: determining the sites of fracture initiation10.1016/0109-5641(95)80045-X ↗
46. Quinn · 2007
47. Fractographic failure analysis of a Procera AllCeram crown using stereo and scanning electron microscopy10.1016/j.dental.2008.01.002 ↗
48. Fréchete · 1990
49. Toughening mechanisms for ceramics
50. Stress intensity factor threshold in dental porcelains10.1007/s10856-007-3290-4 ↗
51. Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials10.1016/S0300-5712(03)00025-3 ↗
52. Influence of hot pressing on the microstructure and fracture toughness of two pressable dental glass-ceramics10.1002/jbm.b.30066 ↗
53. Subcritical crack growth in porcelains, glass-ceramics, and glass-infiltrated alumina composite for dental restorations10.1007/s10856-008-3667-z ↗
54. Influence of environment on delayed failure of alumina ceramics10.1016/S0955-2219(98)00116-2 ↗
55. Slow crack-growth behavior of alumina ceramics10.1557/JMR.2000.0024 ↗
56. Comparison of slow crack growth behavior in alumina and SiC-whisker-reinforced alumina10.1111/j.1151-2916.1993.tb06634.x ↗
57. Subcritical crack growth behavior of Al2O3-glass dental composites10.1002/jbm.b.10007 ↗