journal article·2011-02

Fatigue behavior in water of Y-TZP zirconia ceramics after abrasion with 30 μm silica-coated alumina particles

Susanne S. Scherrer, Maria Cattani-Lorente, Eric Vittecoq, François de Mestral, Jason A. Griggs, H.W. Anselm Wiskott

Dental Materials· Volume 27· Issue 2
Publisher page

Abstract

Objective The use of a 30 μm alumina-silica coated particle sand (CoJet™ Sand, 3M Espe), has shown to enhance the adhesion of resin cements to Y-TZP. The question is whether or not sandblasting 30 μm particles does negatively affect the fatigue limit (S-N curves) and the cumulative survival of Y-TZP ceramics. Method Four zirconia materials tested were: Zeno (ZW) (Wieland), Everest ZS (KV) (KaVo), Lava white (LV) and Lava colored (LVB) (3M Espe). Fatigue testing (S-N) was performed on 66bar of 3 mm × 5 mm × 40 mm with beveled edges for each zirconia material provided by the manufacturers. One half of the specimens were CoJet sandblasted in the middle of the tensile side on a surface of 5 mm × 6 mm. Cyclic fatigue (N=30/group) (sinusoidal loading/unloading at 10 Hz between 10% and 100% load) was performed in 3-point-bending in a water tank. Stress levels were lowered from the initial static value (average of N=3) until surviving 1 million cycles. Fatigue limits were determined from trend lines. Kaplan-Meier survival analysis was performed to determine the failure stress at the median percentile survival level for 1 million of cycles before and after sandblasting. The statistical analyses used the log-rank test. Characterization of the critical flaw was performed by SEM for the majority of the failed specimens. Results The fatigue limits "as received" (ctr) were: LV=720 MPa, LVB=600 MPa, KV=560 MPa, ZW=470 MPa. The fatigue limits "after CoJet sandblasting" were: LV=840 MPa, LVB=788 MPa, KV=645 MPa, ZW=540 MPa. The increase in fatigue limit after sandblasting was 15% for Zeno (ZW) and Everest (KV), 17% for Lava (LV) and 31% for Lava colored (LVB). The KM median survival stresses in MPa were: ZW(ctr)=549 (543-555), ZW(s)=587 (545-629), KV(ctr)=593 (579-607), KV(s)=676 (655-697), LVB(ctr)=635 (578-692), LVB(s)=809 (787-831), LV(ctr)=743 (729-757), LV(s)=908 (840-976). Log-rank tests were significantly different (p<0.001) for all sandblasted groups vs. the "as received" except for Zeno (Wieland) (p=0.295). Failures started from both intrinsic and machined flaws. Significance 30 μm particle sandblasting did significantly improve the fatigue behavior of three out of four Y-TZP ceramic materials and can therefore be recommended for adhesive cementation procedures. This study was supported in part by grants from the Swiss Society for Reconstructive Dentistry (SSRD) and 3M Espe.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
2. Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study
3. Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics10.1016/j.biomaterials.2004.02.036 ↗
4. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
5. Stabilized zirconia as a structural ceramic: an overview10.1016/j.dental.2007.05.005 ↗
6. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
7. Ceramic steel?10.1038/258703a0 ↗
8. Zirconia—an overview
9. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
10. Crystallography of stress-induced martensitic transformation in partially stabilized zirconia
11. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
12. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic10.1016/j.jdent.2004.07.001 ↗
13. Strength and reliability of surface treated Y-TZP dental ceramics10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
14. Reliability and properties of ground Y-TZP-zirconia ceramics10.1177/154405910208100711 ↗
15. CAD/CAM-machining effects on Y-TZP zirconia10.1016/j.dental.2003.08.007 ↗
16. Bonding to zirconia ceramic: adhesion methods and their durability10.1016/S0109-5641(98)00011-6 ↗
17. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods10.1016/j.dental.2005.11.040 ↗
18. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
19. In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling10.1016/j.prosdent.2004.02.001 ↗
20. The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials10.1016/j.prosdent.2005.08.012 ↗
21. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin10.1016/j.prosdent.2006.03.016 ↗
22. Influence of different surface treatments on the short-term bond strength and durability between a zirconia post and a composite resin core material10.1016/S0022-3913(08)60088-8 ↗
23. Damage accumulation and fatigue life of particle-abraded ceramics
24. Fatigue and damage tolerance of Y-TZP ceramics in layered biomechanical systems
25. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗
26. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic10.1016/j.jdent.2005.06.006 ↗
27. Strength influencing variables on CAD/CAM zirconia frameworks10.1016/j.dental.2007.06.030 ↗
28. Low-temperature aging of Y-TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
29. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
30. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
31. The influence of simulated masticatory loading regimes on the bi-axial flexure strength and reliability of a Y-TZP dental ceramic10.1016/j.jdent.2005.07.009 ↗
32. Fatigue of zirconia under cyclic loading in water and its implications for the design of dental bridges10.1016/j.dental.2005.12.008 ↗
33. In vitro lifetime of dental ceramics under cyclic loading in water10.1016/j.biomaterials.2006.12.033 ↗
34. Dynamic fatigue and strength characterization of three ceramic materials10.1007/s10856-007-0131-4 ↗
35. Lifetime of alumina- and zirconia ceramics used for crown and bridge restorations10.1002/jbm.b.30599 ↗
36. Nonparametric estimation from incomplete observations10.1080/01621459.1958.10501452 ↗
37. Dental ceramics: current thinking and trends10.1016/j.cden.2004.01.003 ↗
38. Quinn · 2007
39. Fracture toughness (KIc) of a dental porcelain determined by fractographic analysis10.1016/S0109-5641(99)00055-X ↗
40. Powder processing science and technology for increased reliability10.1111/j.1151-2916.1989.tb05945.x ↗
41. Processing-related fracture origins: II. Agglomerate motion and cracklike internal surfaces caused by differential sintering10.1111/j.1151-2916.1983.tb10069.x ↗
42. Richerson · 1992
43. On the nature of machining cracks in ground ceramics: Part I. SRBSN strengths and fractographic analysis10.1081/MST-200059038 ↗
44. Effect of grinding on flaw geometry and fracture of glass10.1111/j.1151-2916.1977.tb15484.x ↗
45. Fatigue of yttria-stabilized zirconia: I. Fatigue damage, fracture origins, and lifetime prediction10.1111/j.1151-2916.1991.tb04088.x ↗
46. Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis10.1016/j.biomaterials.2004.01.002 ↗
47. Cubic-formation and grain-growth mechanisms in tetragonal zirconia polycrystal10.1111/j.1151-2916.2003.tb03483.x ↗
48. Isothermal sintering effects on phase separation and grain growth in yttria-stabilized zirconia tetragonal polycrystal10.1111/j.1551-2916.2008.02861.x ↗
49. Ferroelastic domain switching as a toughening mechanism in tetragonal zirconia10.1111/j.1151-2916.1986.tb07341.x ↗
50. The biaxial flexural strength and fatigue property of Lava Y-TZP dental ceramic10.1016/j.dental.2006.09.003 ↗
51. Flexural strength, fatigue life, and stress-induced phase transformation study of Y-TZP dental ceramic10.1002/jbm.b.31064 ↗
52. Surface roughness and EDS characterization of a Y-TZP dental ceramic treated with the CoJet™ Sand10.1016/j.dental.2010.06.005 ↗
53. Surface conditioning influences zirconia ceramic bonding10.1177/0022034509340881 ↗