Objective The functional monomer 10-MDP has been considered as one of the best performing functional monomers for dental adhesives. Different adhesives containing 10-MDP are commercially available, among which many so-called 'universal' adhesives. We hypothesize that the quality of the functional monomer 10-MDP in terms of purity may affect bonding performance. Methods We therefore characterized three different 10-MDP versions (10-MDP_KN provided by Kuraray Noritake; 10-MDP_PCM provided by PCM; 10-MDP_DMI provided by DMI) using NMR, and analyzed their ability to form 10-MDP_Ca salts on dentin using XRD. The 'immediate' and 'aged' micro-tensile bond strength (μTBS) to dentin of three experimental 10-MDP primers was measured. The resultant interfacial adhesive-dentin ultra-structure was characterized using TEM. Results NMR disclosed impurities and the presence of 10-MDP dimer in 10-MDP_PCM and 10-MDP_DMI. 10-MDP_PCM and 10-MDP_DMI appeared also sensitive to hydrolysis. 10-MDP_KN, on the contrary, contained less impurities and dimer, and did not undergo hydrolysis. XRD revealed more intense 10-MDP_Ca salt deposition on dentin induced by 10-MDP_KN. The adhesive based on the experimental 10-MDP_KN primer resulted in a significantly higher 'immediate' bond strength that remained stable upon aging; the μTBS of the experimental 10-MDP_PCM and 10-MDP_DMI adhesives significantly dropped upon aging. TEM revealed thicker hybridization and more intense nano-layering for 10-MDP_KN. Significance It was concluded that primer impurities and the presence of 10-MDP dimer affected not only hybridization, but also reduced the formation of 10-MDP_Ca salts and nano-layering. 10-MDP in a high purity grade is essential to achieve durable bonding.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Surgical Sutures and Adhesives

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Hydrolytic stability of self-etch adhesives bonded to dentin10.1177/154405910508401213 ↗
2. Eight-year clinical evaluation of a 2-step self-etch adhesive with and without selective enamel etching10.1016/j.dental.2010.08.190 ↗
3. Meta-analytical review of parameters involved in dentin bonding10.1177/0022034511431251 ↗
4. A randomized, controlled clinical trial of one-step self-etching adhesive systems in non-carious cervical lesions
5. The effect of 6-month water storage on the bond strength of self-etch adhesives bonded to dentin
6. Two-year bond strengths of “all-in-one” adhesives to dentine10.1016/j.jdent.2012.03.003 ↗
7. Comparative study on adhesive performance of functional monomers10.1177/154405910408300604 ↗
8. Chemical interaction of phosphoric acid ester with hydroxyapatite10.1177/154405910608501014 ↗
9. Effect of reacted acidic monomer with calcium on bonding performance10.1177/0022034510397837 ↗
10. Self-assembled nano-layering at the adhesive interface10.1177/0022034512437375 ↗
11. Nano-controlled molecular interaction at adhesive interfaces for hard tissue reconstruction10.1016/j.actbio.2010.03.024 ↗
12. Nanolayering of phosphoric acid ester monomer on enamel and dentin10.1016/j.actbio.2011.04.026 ↗
13. Bonding performance of universal adhesives in different etching modes10.1016/j.jdent.2014.04.012 ↗
14. Influence of a hydrophobic resin coating on the bonding efficacy of three universal adhesives10.1016/j.jdent.2014.01.013 ↗
15. HEMA inhibits interfacial nano-layering of the functional monomer MDP10.1177/0022034512460396 ↗
16. 13C NMR analysis of the etching efficacy of acidic monomers in self-etching primers10.1016/j.jdent.2005.04.005 ↗
17. Omura I, Yamauchi J, Nagase Y, Uemura F. Adhesive compositions. US Patent 4537940.
18. Synthesis of phosphate monomers and bonding to dentin: esterification methods and use of phosphorus pentoxide10.1016/j.jdent.2007.11.003 ↗
19. Influence of three specimen fixation modes on the micro-tensile bond strength of adhesives to dentin10.4012/dmj.26.694 ↗
20. A TEM study of two waterbased adhesive systems bonded to dry and wet dentin10.1177/00220345980770010501 ↗
21. Chemical aspects of self-etching enamel-dentin adhesives: a systematic review10.1016/j.dental.2005.05.001 ↗
22. Degradation-stage effect of self-etching primer on dentin bond durability10.1177/0022034509337146 ↗
23. Degradation of 10-methacryloyloxydecyl dihydrogen phosphate10.1177/0022034510379018 ↗