The effect of five silane coupling agents on the bond strength of a luting cement to a silica-coated titanium
Source abstract
Abstract
Objectives The adhesive performance of five silane coupling agents in adhering resin composite cement (3M ESPE) to silica-coated titanium was evaluated. Titanium was tribochemically silica-coated by using the Rocatec system. Methods Two volume percent solutions of 3-acryloyloxypropyltrimethoxysilane (Toray Dow Corning Silicone), N-[3-(trimethoxysilyl)propylethylenediamine] (Dow Corning), 3-mercaptopropyltrimethoxysilane (Toray Dow Corning Silicone) and bis-[3-(triethoxysilyl)propyl]polysulfide (Dow Corning) were prepared in 95 vol.% acidified ethanol and allowed to activate (hydrolyze). A pre-activated ca. 2 vol.% 3-methacryloyloxypropyltrimethoxysilane (ESPE Sil) was used as a control. The silanes were applied onto silica-coated titanium slides. Chemical activation reactions of the silanes were monitored by Fourier transform infrared spectrometry (Perkin-Elmer Spectrum One). RelyX ARC (3M ESPE) resin composite cement stubs were applied and photo-polymerized onto silica-coated titanium. The specimens were thermo-cycled (6000 cycles, 5-55 degrees C). Results Statistical analysis (ANOVA) showed that the highest shear bond strength (n=8 per group) value after thermocycling, 14.8 MPa (S.D. 3.8 MPa), was obtained with 2.0 vol.% 3-acryloyloxypropyltrimethoxysilane. Silanization and results with 3-methacryloyloxypropyltrimethoxysilane (control, ESPE Sil) did not statistically differ from 3-acryloyloxypropyltrimethoxysilane, 14.2 MPa (S.D. 5.8). The lowest shear bond strength was 7.5 (S.D. 1.9) MPa for N-[3-(trimethoxysilyl)propylethylenediamine] and 7.5 (S.D. 2.5) MPa for bis-[3-(triethoxysilyl)propyl]polysulfide. Both the type of silane (p<0.001) and storage conditions affected significantly the shear bond strength values (p<0.001). All silanes became activated according to the infrared spectroscopic analysis. Significance Silanization with 3-acryloyloxypropyltrimethoxysilane or 3-mercaptopropyltrimethoxysilane might offer an alternative for bonding a luting cement to silica-coated titanium.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Marine Biology and Environmental Chemistry · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. An introduction to silanes and their clinical applications in dentistry
2. From treating solution to filler surface and beyond: the life history of a silane coupling agent
3. To silanate or not to silanate: making a clinical decision
4. Silane based concepts on bonding resin composite to metals10.5005/jcdp-8-2-1 ↗
5. Storage effect of a pre-activated silane on the resin to ceramic bond10.1016/j.dental.2003.08.005 ↗
6. Properties of a silica-reinforced polymer for dental restorations10.14219/jada.archive.1963.0010 ↗
7. Use of epoxy resins in restorative materials10.1177/00220345560350030501 ↗
8. Roulet · 1987
9. Composites having ionomer bonds with silanes at the interfaces10.1163/156856189X00119 ↗
10. Protecting metals with silane coupling agents
11. Das rocatec system—haftung durch tribochemische beschichtung
12. Metal surface treatment: characterization and effect on composite-to-metal bond strength
13. Bonding porcelain to acrylic resin denture bases10.14219/jada.archive.1967.0178 ↗
14. Isocyanato- and Methacryloxysilanes Promote Bis-GMA adhesion to titanium10.1177/154405910508400413 ↗
15. The effect of a 3-methacryloxypropyltrimethoxysilane and vinyltriisopropoxysilane blend and tris(3-trimethoxysilylpropyl)isocyanurate on the shear bond strength of composite resin to titanium metal10.1016/j.dental.2003.10.009 ↗
16. The effect of a novel silane blend system on resin bond strength to silica-coated Ti substrate10.1016/j.jdent.2005.09.007 ↗
17. Vollhardt · 2002
18. Shear bond strength of bis-GMA and methacrylated dendrimer resins on silanized titanium substrate10.1016/j.dental.2004.03.011 ↗
19. Dental casting alloys
20. Durability of resin bonds to pure titanium10.1111/j.1532-849X.1995.tb00309.x ↗
21. Effects of sandblasting and silica-coating procedures on pure titanium10.1016/0300-5712(94)90067-1 ↗
22. Clinical factors affecting adhesive fixed partial dentures: a 6-year study10.1016/0022-3913(93)90212-7 ↗
23. Arkles · 2003
24. Evidence for chemical bond formation at silane coupling agent interfaces10.1177/002199836700100304 ↗
25. Effect of silanation of fillers on their dispersability by monomer systems10.1111/j.1365-2842.1995.tb01562.x ↗
26. Factors contributing to the stability of alkoxysilanes in aqueous solution
27. Shear versus tensile bond strength of resin composite bonded to ceramic10.1177/00220345950740091401 ↗
28. International Standardization Organization (ISO), Dentistry-polymer-based crown and bridge materials, Amendment 1996; ISO 10477.