Fracture-resistant monolithic dental crowns
Source abstract
Abstract
Objective To quantify the splitting resistance of monolithic zirconia, lithium disilicate and nanoparticle-composite dental crowns. Methods Fracture experiments were conducted on anatomically-correct monolithic crown structures cemented to standard dental composite dies, by axial loading of a hard sphere placed between the cusps. The structures were observed in situ during fracture testing, and critical loads to split the structures were measured. Extended finite element modeling (XFEM), with provision for step-by-step extension of embedded cracks, was employed to simulate full failure evolution. Results Experimental measurements and XFEM predictions were self-consistent within data scatter. In conjunction with a fracture mechanics equation for critical splitting load, the data were used to predict load-sustaining capacity for crowns on actual dentin substrates and for loading with a sphere of different size. Stages of crack propagation within the crown and support substrate were quantified. Zirconia crowns showed the highest fracture loads, lithium disilicate intermediate, and dental nanocomposite lowest. Dental nanocomposite crowns have comparable fracture resistance to natural enamel. Significance The results confirm that monolithic crowns are able to sustain high bite forces. The analysis indicates what material and geometrical properties are important in optimizing crown performance and longevity.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Health and Care Utilization · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Porcelain-fused-to-metal vs nonmetal crowns10.14219/jada.archive.1999.0211 ↗
2. Fatigue of dental ceramics10.1016/j.jdent.2013.10.007 ↗
3. Edge chipping and flexural resistance of monolithic ceramics10.1016/j.dental.2013.09.004 ↗
4. Is the rush to all-ceramic crowns justified10.14219/jada.2013.19 ↗
5. Clinical outcome of three-unit lithium-disilicate glass-ceramic fixed dental prostheses: up to 8 years results10.1016/j.dental.2009.05.003 ↗
6. Clinical results of lithium-disilicate crowns after up to 9 years of service10.1007/s00784-012-0700-x ↗
7. Clinical outcomes of three different crown systems with cad/cam technology10.1016/j.prosdent.2014.05.002 ↗
8. Enamel wear caused by monolithic zirconia crowns after 6 months of clinical use10.1111/joor.12139 ↗
9. Clinical outcomes of lithium disilicate single crowns and partial fixed dental prostheses: a systematic review10.1016/j.prosdent.2014.01.005 ↗
10. Fatigue resistance of cad/cam complete crowns with a simplified cementation process10.1016/j.prosdent.2013.09.020 ↗
11. Load-bearing capacity and the recommended thickness of dental monolithic zirconia single crowns10.1016/j.jmbbm.2014.03.014 ↗
12. Fracture resistance of a selection of full-contour all-ceramic crowns: an in vitro study10.11607/ijp.3815 ↗
13. Fracture strength of monolithic all-ceramic crowns made of high-translucent yyttrium-oxide-stabilized zirconium dioxide compared to porcelain-veneered crowns and lithium disilicate crowns10.3109/00016357.2013.822098 ↗
14. Fracture resistance of monolithic zirconia molar crowns with reduced thickness10.3109/00016357.2015.1007479 ↗
15. Fatigue resistance of ultrathin CAD/CAM complete crowns with a simplified cementation process10.1016/j.prosdent.2015.04.014 ↗
16. A clinical evaluation of chairside lithium disilicate cad/cam crowns: a two-year report10.14219/jada.archive.2010.0355 ↗
17. Ten-year outcome of three-unit fixed dental prostheses made from monolithic lithium disilicate ceramic10.14219/jada.archive.2012.0147 ↗
18. Chair-side generated posterior lithium disilicate crowns after 4 years10.1007/s00784-012-0868-0 ↗
19. Materials for chairside cad/cam-produced restorations10.14219/jada.archive.2006.0397 ↗
20. Clinical success and survival of indirect resin composite crowns: results of a 3-year prospective study10.1016/j.dental.2012.04.007 ↗
21. Fatigue resistance and microleakage of cad/cam ceramic and composite molar crowns10.1111/j.1532-849X.2011.00773.x ↗
22. On the chipping and splitting of teeth10.1016/j.jmbbm.2010.10.011 ↗
23. Contact damage in brittle coating layers: influence of surface curvature10.1002/jbm.b.30188 ↗
24. Fracture modes in human teeth10.1177/0022034508330055 ↗
25. Fracture in teeth—a diagnostic for inferring bite force and tooth function10.1111/j.1469-185X.2011.00181.x ↗
26. Mechanics of longitudinal cracks in tooth enamel10.1016/j.actbio.2011.01.038 ↗
27. Role of tooth elongation in promoting fracture resistance10.1016/j.jmbbm.2011.11.014 ↗
28. Effect of property gradients on enamel fracture in human enamel10.1016/j.jmbbm.2012.06.014 ↗
29. Role of multiple cusps in tooth fracture10.1016/j.jmbbm.2014.03.018 ↗
30. Remarkable resilience of teeth10.1073/pnas.0902466106 ↗
31. Morphology and fracture of enamel10.1016/j.jbiomech.2009.05.013 ↗
32. Occlusal geometrical considerations in all-ceramic pre-molar crown failure testing10.1016/j.dental.2011.08.005 ↗
33. Mechanics analysis of molar tooth splitting10.1016/j.actbio.2015.01.004 ↗
34. Materials design in the performance of all-ceramic crowns10.1016/j.biomaterials.2003.09.050 ↗
35. Effect of sandblasting on the long-term strength of dental ceramics10.1002/jbm.b.30097 ↗
36. Damage accumulation and fatigue life of particle-abraded dental ceramics
37. Fracture of tooth enamel from incipient microstructural defects10.1016/j.jmbbm.2009.08.002 ↗
38. Micromechanics of wear traces in tooth enamel10.1016/j.actbio.2014.11.047 ↗
39. Fracture surface analysis of dental ceramics: clinically failed restorations
40. Ceramics in restorative and prosthetic dentistry10.1146/annurev.matsci.27.1.443 ↗
41. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
42. Dental ceramics: current thinking and trends10.1016/j.cden.2004.01.003 ↗
43. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
44. Role of indenter material and size in veneer failure of brittle layer structures10.1002/jbm.b.30728 ↗
45. Gross dental wear and dental microwear in historical perspective
46. Mechanisms and causes of wear in tooth enamel: implications for hominin diets10.1098/rsif.2012.0923 ↗
47. A comparison of observed molar wear rates in extant herbivorous mammals10.5735/086.051.0219 ↗
48. A model for predicting wear rates in tooth enamel10.1016/j.jmbbm.2014.05.023 ↗
49. A fractographic study of clinically retrieved zirconia–ceramic and metal–ceramic fixed dental prostheses10.1016/j.dental.2015.07.003 ↗