Abstract

Objectives The purpose of the study was to evaluate the influence of preparation design, and ceramic material, masticatory fatigue and fracture resistance of non-retentive all-ceramic full-coverage restorations luted on human mandibular molars. Methods Full-coverage occlusal restorations were laboratory fabricated from leucite reinforced glass-ceramic (IPS Empress Esthetic) or lithium disilicate glass-ceramic (IPS e.max Press). For each ceramic material four groups with eight specimens each were randomly assigned. Groups had either a non-retentive, occlusal preparation with chamfer finishing line or straight-beveled finishing line and the preparation was either completely within enamel or within dentin with a finishing line in enamel. Restorations were adhesively luted to the teeth using composite resin. After storage in water for 1 week specimens were cyclic loaded 600,000 times with a weight of 10kg and additionally, thermocycled 3500 times (5/55 degrees C) in a masticatory simulator. Surviving specimens were loaded until, fracture in a universal testing machine. Statistical analysis was done using three-way ANOVA. Results All specimens survived the masticatory fatigue. Mean fracture resistance ranged from 2895 to 4173N. Influence of ceramic material on fracture resistance was significant (p=0.0001). Lithium disilicate glass-ceramic restorations had higher fracture resistances than leucite reinforced glass-ceramic restorations. Different preparation designs showed no significant influence on fracture resistance (p=0.0969). The design of the finishing line did not influence the fracture resistance (p=0.9461). Significance The fracture resistance of adhesively luted non-retentive full-coverage molar restorations, made of lithium disilicate or leucite reinforced glass-ceramic is promising and seems to permit clinical application.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Dental Health and Care Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
2. A review all-ceramic restorations10.14219/jada.archive.1997.0193 ↗
3. All-ceramic restorations: classification and clinical evaluations
4. Retrospective clinical investigation and survival analysis on ceramic inlays and partial ceramic crowns: results up to 7 years10.1007/s007840050064 ↗
5. Longevity and clinical performance of IPS-Empress ceramic restorations – a literature review
6. Clinical performance of bonded leucite-reinforced glass ceramic inlays and onlays after eight years10.1016/j.dental.2004.03.009 ↗
7. Computer-manufactured, direct ceramic restorations: a prospective, clinical 10-year study of Cerec CAD–CAM inlays and onlays
8. Influence of cyclic loading and luting agents on the fracture load of two all-ceramic crown systems10.1016/j.prosdent.2004.09.002 ↗
9. Fracture frequency of all-ceramic crowns during dynamic loading in a chewing simulator using different loading and luting protocols10.1016/j.dental.2008.02.019 ↗
10. Fracture resistance of different partial-coverage ceramic molar restorations: an in vitro investigation10.14219/jada.archive.2006.0224 ↗
11. Longevity of cast gold inlays and partial crowns. A retrospective study at a dental school clinic10.1007/s007840050086 ↗
12. Survival of Dicor glass-ceramic dental restorations over 16 years. Part III: effect of luting agent and tooth or tooth-substitute core structure10.1067/mpr.2001.119415 ↗
13. Tensile bond strength of four resin luting agents bonded to bovine enamel and dentin10.1016/S0022-3913(03)00177-X ↗
14. Compressive fracture resistance of porcelain laminates bonded to enamel or dentin with four adhesive systems10.1111/j.1532-849X.2007.00227.x ↗
15. Masticatory function – a review of the literature. III. Masticatory performance and efficiency10.1111/j.1365-2842.1976.tb00929.x ↗
16. In vitro evaluation of a mechanical testing chewing simulator10.1016/j.dental.2008.09.010 ↗
17. Influence of water storage and thermal cycling on the fracture strength of all-porcelain, resin-bonded fixed partial dentures10.1016/0022-3913(94)90463-4 ↗
18. Masticatory fatigue, fracture resistance, and marginal discrepancy of ceramic partial crowns with and without coverage of compromised cusps
19. Wear of composite resin veneering materials in a dual-axis chewing simulator10.1046/j.1365-2842.1999.00416.x ↗
20. Maximale Kaukraft als Berechnungsfaktor zahntechnischer Konstruktionen
21. Development of an artificial oral environment for testing of dental restoratives: bi-axial force and movement control10.1177/00220345830620010801 ↗
22. In vitro resistance to fracture of porcelain inlays bonded to tooth