Effect of grain size on the monoclinic transformation, hardness, roughness, and modulus of aged partially stabilized zirconia

Thomas J. Lucas, Nathaniel C. Lawson, Gregg M. Janowski, John O. Burgess

Dental Materials· Volume 31· Issue 12
Publisher page

Abstract

Objective Low-temperature-degradation (LTD) has been reported to cause property changes in yttria-tetragonal zirconia polycrystals (Y-TZP). The current study measured monoclinic phase transformation of Y-TZP with different grain sizes and corresponding property changes due to artificial aging. Null hypothesis the grain size of aged Y-TZP will not influence its transformation, roughness, hardness or modulus of elasticity. Methods Four groups of Y-TZP were examined with differing grain sizes (n=5). The line intercept technique was used to determine grain sizes on SEM images (100,000×). Artificial aging was accomplished by autoclaving at 2 bar pressure for 5 h. X-ray diffraction (30 mA, 40 kV) was used to measure tetragonal to monoclinic transformation (t→m). Surface roughness analysis was performed using a non-contact surface-profilometer. Nano-hardness and modulus of elasticity were measured using nano-indentation. Results SEM analyses showed different grain sizes for each sample group (0.350 μm, 0.372 μm, 0.428 μm, and 0.574 μm). The fraction of t→m transformation increased as grain size increased; furthermore, aging of zirconia caused increased roughness. Modulus and hardness after aging displayed no significant correlation or interaction with grain size. Significance Smaller grains caused less transformation, and aging caused increased roughness, but grain size did not influence the amount of increased surface roughness. Future studies are needed to determine the effects of grain size on the wear and fracture properties of dental zirconia.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Accelerating aging of zirconia femoral head implants: Change of surface structure and mechanical properties10.1002/jbm.b.30688 ↗
2. Environmental degradation of zirconia ceramics10.1016/0955-2219(95)00035-S ↗
3. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
4. Low-temperature aging of Y-YZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
5. Fracture of porcelain-veneered structures in fatigue10.1177/154405910708600207 ↗
6. Influence of low-temperature environmental exposure on the mechanical properties and structural stability of dental zirconia10.1111/j.1532-849X.2011.00838.x ↗
7. Ageing effects on the nanoindentation response of sub-micrometric 3Y-TZP ceramics10.1007/s10853-006-1177-2 ↗
8. Evaluating mechanical properties and degradation of YTZP dental implants10.1016/j.msec.2009.08.002 ↗
9. SEM observations of porcelain Y-TZP interface10.1016/j.dental.2009.01.006 ↗
10. Effect of heat treatment and in vitro aging on the microstructure and mechanical properties of cold isostatic-pressed zirconia ceramics for dental restorations10.1016/j.dental.2014.05.017 ↗
11. Making yttria-stabilized tetragonal zirconia translucent10.1016/j.dental.2014.08.375 ↗
12. Stabilized zirconia as a structural ceramic: an overview10.1016/j.dental.2007.05.005 ↗
13. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
14. E112-96, A. · 2004
15. Lineal intercept technique for measuring grain size in two-phase polycrystalline ceramics10.1111/j.1151-2916.1972.tb11224.x ↗
16. Phase transformation of dental zirconia following artificial aging10.1002/jbm.b.33334 ↗
17. A critical comparison of methods for the determination of the aging sensitivity in biomedical grade yttria-stabilized zirconia10.1002/jbm.b.30123 ↗
18. Phase transformation: roughness, and microhardness of artificially aged yttria- and magnesia-stabilized zirconia femoral heads10.1002/jbm.a.31438 ↗
19. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by X-ray diffraction10.1111/j.1151-2916.1984.tb19715.x ↗
20. 1996
21. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
22. Zirconia ceramics: their contrast ratio and grain size depending on sintering parameters10.4012/dmj.2014-056 ↗
23. The influence of grain size on low-temperature degradation of dental zirconia10.1002/jbm.b.31969 ↗
24. Enamel wear opposing polished and aged zirconia10.2341/12-345-L ↗
25. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
26. Surface crystalline phases and nanoindentation hardness of explanted zirconia femoral heads10.1023/A:1025678525474 ↗
27. Temperature dependence of the elastic moduli of monoclinic zirconia10.1111/j.1151-2916.1991.tb07177.x ↗