journal article·2015-06

Damage tolerance of indirect restorative materials (including PICN) after simulated bur adjustments

Andrea Coldea, Jens Fischer, Michael V. Swain, Norbert Thiel

Dental Materials· Volume 31· Issue 6
Publisher page

Abstract

Objective To analyze the damage tolerance of indirect restorative materials after grinding with diamond burs to simulate adjustments by clinicians and technicians. Methods Seven commercially available restorative materials (Mark II, ENAMIC, In-Ceram Alumina, VM 9, In-Ceram YZ, IPS e.max CAD) and an experimental one (PICN) were analyzed. Forty bending bars per material were fabricated according to manufacturer's instructions and lapped with 15 μm diamond suspension. The initial flexural strength was determined in three-point-bending on 10 specimens. Additionally the elastic modulus and Poisson's ratio were determined by the resonant frequency method. The remaining bending bars were divided into six groups (n=5) and subjected to standardized grinding with three different diamond grit burs (coarse, 151 μm; medium, 107 μm and extra fine 25 μm) and two grinding directions (transversal and longitudinal). The ground specimens were subsequently loaded to fracture and analyzed by SEM. Results Except for the YTZP bending bars, the initial materials strength of all tested materials decreased significantly with all diamond burs upon adjustments in both transversal and longitudinal grinding directions. The resistance of the ground materials to strength reduction follow the order from highest to least damage tolerant material: PICN>ENAMIC>Mark II>VM 9>In-Ceram Alumina>IPS e.max CAD. The loss in strength of all examined materials after longitudinal grinding is generally less compared to transversal grinding. The lowest loss in strength occurred for VM 9 (7.79%) and ENAMIC (9.18%) upon longitudinal grinding direction with extra fine and medium diamond grit bur, respectively. Significance The damage tolerance of restorative materials upon adjustments depends on specific mechanical properties and the adjustment procedure. The outcomes of the simulated grinding protocols of this study can be adopted clinically in terms of the selection of appropriate materials, burs and adjustment parameters.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. A novel polymer infiltrated ceramic dental material10.1016/j.dental.2011.02.002 ↗
2. The influence of surface roughness on porcelain strength10.1016/S0109-5641(00)00030-0 ↗
3. Abrasive machining of glass-ceramics with a dental handpiece10.1080/10940340008945707 ↗
4. Evaluation of subsurface damage in CAD/CAM machined dental ceramics10.1023/A:1008812929476 ↗
5. An overview of in vitro abrasive finishing & CAD/CAM of bioceramics in restorative dentistry10.1016/j.ijmachtools.2005.07.045 ↗
6. Effect of surface treatment on flexural strength of zirconia bars10.1016/S0022-3913(10)60100-X ↗
7. CAD/CAM-machining effects on Y-TZP zirconia10.1016/j.dental.2003.08.007 ↗
8. Cutting characteristics of dental glass ceramics during in vitro dental abrasive adjusting using a high-speed electric handpiece10.1016/j.ceramint.2013.01.045 ↗
9. Cracking of porcelain surfaces arising from abrasive grinding with a dental air turbine10.1111/j.1532-849X.2011.00760.x ↗
10. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
11. A novel polymer infiltrated ceramic for dental simulation10.1007/s10856-011-4350-3 ↗
12. In-vitro strength degradation of dental ceramics and novel PICN material by sharp indentation10.1016/j.jmbbm.2013.05.004 ↗
13. Hertzian contact response and damage tolerance of dental ceramics10.1016/j.jmbbm.2014.02.002 ↗
14. Swain · 2001 · 825
15. ISO standard 6872:2008. Dentistry—ceramic materials, January 2009.
16. ASTM E 1876:2009. Standard Test Method for Dynamic Young's Modulus, Shear Modulus, and Poisson's Ratio by Impulse Excitation of Vibration, 2009.
17. ISO standard 7711-3:2004. Dentistry—diamond rotary instruments—Part 3: Grit sizes, designation and colour code, February 2005.
18. An evaluation of the effects of handpiece speed, abrasive characteristics, and polishing load on the flexural strength of polished ceramics10.1016/j.prosdent.2005.08.014 ↗
19. Effects of acid hydrolysis and mechanical polishing on surface residual stresses of low-fusing dental ceramics10.1016/S0022-3913(03)00277-4 ↗
20. In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics10.1016/j.prosdent.2006.08.004 ↗
21. Property-process relations in simulated clinical abrasive adjusting of dental ceramics10.1016/j.jmbbm.2012.07.011 ↗
22. In vitro rapid intraoral adjustment of porcelain prostheses using a high-speed dental handpiece10.1016/j.actbio.2007.08.006 ↗
23. Kingery · 1976 · 816
24. Effect of surface finish on strength degradation of glass ceramics10.1016/S1350-6307(99)00007-2 ↗
25. Influence of grinding, sandblasting, polishing and heat treatment on the flexural strength of a glass-infiltrated alumina-reinforced dental ceramic10.1016/j.biomaterials.2003.08.056 ↗
26. Lifetime prediction of CAD/CAM dental ceramics10.1002/jbm.10468 ↗
27. Correlation of in vitro fatigue data and in vivo clinical performance of a glass ceramic material10.1016/j.dental.2007.01.011 ↗
28. Ashby · 2011 · 57
29. Fast XRD2 microdiffraction with focusing X-ray microlenses10.1002/ppsc.200800038 ↗
30. XRD2 micro-diffraction analysis of the interface between Y-TZP and veneering porcelain: role of application methods10.1016/j.dental.2010.02.002 ↗
31. Long-term aging in 3mol.% yttria-stabilized tetragonal zirconia polycrystals at human body temperature10.1016/j.actbio.2013.09.033 ↗
32. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics10.1016/j.jeurceramsoc.2007.09.013 ↗
33. Evaluation of subsurface defects created during the finishing of composites10.1177/00220345920710091601 ↗
34. Quinn · 2007 · 6
35. Role of microstructure on contact damage and strength degradation of micaceous glass-ceramics10.1016/S0109-5641(98)00013-X ↗
36. Flexural strength of feldspathic porcelain treated with ion exchange, overglaze, and polishing10.1016/0022-3913(94)90184-8 ↗