Impact of oral fluids on dental ceramics: What is the clinical relevance?
Source abstract
Abstract
Objectives In this brief and selective overview, basic factors contributing to aqueous induced dissolution, phase changes of zirconia and mechanical strength degradation of dental ceramics are considered. Methods Dissolution is important for porcelain and glass-ceramic materials as they predominantly contain a silica glass structure with various other cations incorporated which disrupt the silica network. In glass-ceramic materials and porcelains containing crystalline components the situation is more complex as the difference in the dissolution rate may increase the surface roughness and contribute to abrasion of the opposing definition. Results Factors contributing to the aqueous dissolution of silicate based dental ceramics and induced destabilization of Y-TZP zirconia or low temperature degradation (LTD) are considered. It is also noted that there have been a number of reports of spontaneous fracture of 3Y-TZP specimens because of LTD in the absence of external stress. A simple analysis of this situation is presented which indicates a strong specimen-size effect and also implicates the role of the remnant "pseudo-grain" structure resulting from the pressing of spray-dried powder agglomerates. Significance The final section of this review addresses the consequences of various environments on crack growth and strength degradation. In some situations it is suggested that the aqueous environment may enhance the strength of restorative materials. In all instances discussed above the clinical consequences are pointed out.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Aerogels and thermal insulation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Surface degradation of dental ceramics as a function of environmental pH10.1177/0022034513484332 ↗
2. Gastric volume and pH in outpatients10.1007/BF03006781 ↗
3. The effects of fluoride and mineralising treatments on plaque microcosm Ca, P and F, pH responses and cariogenicity
4. Surface degradation of glass ceramics after exposure to acidulated phosphate fluoride10.1590/S1678-77572010000200010 ↗
5. Temperature extremes produced orally by hot and cold liquids10.1016/0022-3913(92)90239-7 ↗
6. Ion leaching from dental ceramics during static in-vitro corrosion testing10.1002/jbm.10109 ↗
7. On the surface elemental composition of corroded and non-corroded dental ceramic materials in vitro10.1023/A:1023416232222 ↗
8. Lawn · 1993
9. Significance of internal stresses for the martensitic transformation in Y-TZP polycrystals during degradation10.1111/j.1151-2916.1986.tb04789.x ↗
10. Moisture assisted crack growth in ceramics10.1007/BF00188945 ↗
11. Physical chemistry of glass surfaces10.1016/0022-3093(78)90077-7 ↗
12. Theory of corrosion of glass and ceramics
13. A simplified model for glass dissolution in water10.1023/A:1017591100985 ↗
14. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics10.1016/j.dental.2003.05.003 ↗
15. Influence of hot pressing on the microstructure and fracture toughness of two pressable dental glass-ceramics10.1002/jbm.b.30066 ↗
16. Factors affecting enamel and ceramic wear: a literature review10.1067/mpr.2002.123851 ↗
17. Wear of ceramic and antagonist—a systematic evaluation of influencing factors in vitro10.1016/j.dental.2007.06.016 ↗
18. Prospective clinical split-mouth study of pressed and CAD/CAM all ceramic partial coverage restorations: 7 year results10.11607/ijp.3043 ↗
19. Phase evolution upon aging of air-plasma sprayed t′-zirconia coatings: 1. Synchrotron X-ray diffraction10.1111/j.1551-2916.2012.05451.x ↗
20. Ceramic steel?10.1038/258703a0 ↗
21. Green · 1991
22. Phase change and mechanical properties of ZrO2–Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
23. Low temperature degradation and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
24. Low temperature degradation-ageing of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
25. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
26. Formation of monoclinic zirconia at the anodic face of tetragonal zirconia polycrystalline solid electrolytes10.1007/BF00615460 ↗
27. Impurity and yttrium segregation in yttria-tetragonal zirconia10.1016/0167-2738(91)90225-Z ↗
28. Degradation during aging of transformation-toughened ZrO2–Y2O3 materials at 250°C10.1111/j.1151-2916.1986.tb07415.x ↗
29. Direct evidence for continuous linear kinetics in the low-temperature degradation of Y-TZP10.1016/j.actbio.2012.08.032 ↗
30. Keuper · Long-time aging in 3Y-TZP at Human Body Temperature Acta Biomaterialia · 2013
31. Prevention of low temperature surface transformation by surface recrystallization in yttria doped tetragonal zirconia10.1111/j.1151-2916.1989.tb06124.x ↗
32. Concerns of hydrothermal degradation of CAD/CAM zirconia10.1177/0022034509354193 ↗
33. Ageing and fatigue behaviour of surface treated Y-TZP dental ceramics
34. Martensitic transformation in zirconia. Part I. Nanometer scale prediction and measurement of transformation induced relief
35. Mixed oxides prosthetic ceramic ball heads. Part 1. Effect of the ZrO2 fraction on the wear of ceramic on polyethylene joints10.1016/S0142-9612(98)00253-1 ↗
36. Mixed oxides prosthetic ceramic ball heads. Part 2. Effect of the ZrO2 fraction on the wear of ceramic on ceramic joints10.1016/S0142-9612(99)00093-9 ↗
37. Mixed oxides prosthetic ceramic ball heads. Part 1. effect of the ZrO2 fraction on the wear of ceramic on ceramic joints prostheses. A long term in-vitro wear study10.1016/S0142-9612(00)00235-0 ↗
38. Low temperature degradation of Y-TZP materials10.1007/BF02402664 ↗
39. Effect of grain size on mechanical properties of submicrometer 3Y-TZP: fracture strength and hydro-thermal degradation10.1111/j.1551-2916.2007.01643.x ↗
40. Compositional effects in nano-structured yttria partially stabilised zirconia10.1111/j.1744-7402.2010.02503.x ↗
41. Relation of transformation temperature to the fracture toughness of transformation-toughened ceramics10.1007/BF01160553 ↗
42. Processing-related fracture origins: 11. Agglomerate motion and crack-like internal surfaces caused by differential sintering10.1111/j.1151-2916.1983.tb10069.x ↗
43. Powder processing science and technology for increased reliability10.1111/j.1151-2916.1989.tb05945.x ↗
44. Fatigue behaviour in water of Y-TZP ceramics after abrasion with 30 um silica coated alumina particles10.1016/j.dental.2010.10.003 ↗
45. Degration of partially stabilized zirconia ceramics under an applied stress10.1007/BF02835078 ↗
46. Research on mechanical strength of glasses
47. Fatigue of glass under static loads10.1063/1.1707702 ↗
48. The fatigue of glass under stress10.1038/154341a0 ↗
49. Stress corrosion and static fatigue of glass10.1111/j.1151-2916.1970.tb15962.x ↗
50. Effect of corrosive media on crack growth of model glasses and commercial silicate glasses
51. Strength–probability–time (SPT) relationships in ceramics10.1007/BF02403519 ↗
52. Stress corrosion of silicate glass: a review10.1016/S0022-3093(02)01931-2 ↗
53. Charles · 1962 · 511
54. Fracture of glasses10.1146/annurev.ms.26.080196.000355 ↗
55. Crack growth threshold in soda lime silica glass: role of hold time10.1016/S0022-3093(02)01932-4 ↗
56. Glass breaks like metals but at the nanometre scale10.1103/PhysRevLett.90.075504 ↗
57. Influence of pH on slow crack growth of dental porcelains10.1016/j.dental.2007.10.001 ↗
58. Mechanical fatigue and hydrothermal stability of Y-TZP dental ceramics10.4028/www.scientific.net/KEM.409.161 ↗
59. Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue10.1111/j.1151-2916.1999.tb02213.x ↗
60. Influence of connector design on fracture probability of ceramic fixed-partial dentures10.1177/154405910208100909 ↗
61. Thermal induced fracture for core-veneered dental ceramic structures10.1016/j.actbio.2013.05.009 ↗