Effect of surface modifications on the bond strength of zirconia ceramic with resin cement resin
Source abstract
Abstract
Objectives Purpose of this in vitro study was to evaluate the effect of surface modifications on the tensile bond strength between zirconia ceramic and resin. Methods Zirconia ceramic surfaces were treated with 150-μm abrasive alumina particles, 150-μm abrasive zirconia particles, argon-ion bombardment, gas plasma, and piranha solution (H2SO4:H2O2=3:1). In addition, slip casting surfaces were examined. Untreated surfaces were used as the control group. Tensile bond strengths (TBS) were measured after water storage for 3 days or 150 days with additional 37,500 thermal cycling for artificial aging. Statistical analyses were performed with 1-way and 3-way ANOVA, followed by comparison of means with the Tukey HSD test. Results After storage in distilled water for three days at 37 °C, the highest mean tensile bond strengths (TBS) were observed for zirconia ceramic surfaces abraded with 150-μm abrasive alumina particles (TBS(AAP)=37.3 MPa, TBS(CAAP)=40.4 MPa), and 150-μm abrasive zirconia particles (TBS(AZP)=34.8 MPa, TBS(CAZP)=35.8 MPa). Also a high TBS was observed for specimens treated with argon-ion bombardment (TBS(BAI)=37.8 MPa). After 150 days of storage, specimens abraded with 150-μm abrasive alumina particles and 150-μm abrasive zirconia particles revealed high TBS (TBS(AAP)=37.6 MPa, TBS(CAAP)=33.0 MPa, TBS(AZP)=22.1 MPa and TBS(CAZP)=22.8 MPa). A high TBS was observed also for specimens prepared with slip casting (TBS(SC)=30.0 MPa). A decrease of TBS was observed for control specimens (TBS(UNT)=12.5 MPa, TBS(CUNT)=9.0 MPa), specimens treated with argon-ion bombardment (TBS(BAI)=10.3 MPa) and gas plasma (TBS(GP)=11.0 MPa). A decrease of TBS was observed also for specimens treated with piranha solution (TBS(PS)=3.9 MPa, TBS(CPS)=4.1 MPa). A significant difference in TBS after three days storage was observed for specimens treated with different methods (p<0.001). Thermal cycling significantly reduced TBS for all groups (p<0.001) excluding groups: AAP(p>0.05), CAAP(p>0.05) and SC(p>0.05). However, the failure patterns of debonded specimens prepared with 150-μm abrasive zirconia particles were 96.7% cohesive. Conclusion Treatment of zirconia ceramic surfaces with abrasive zirconia particles is a promising method to increase the tensile bond strength without significant damage of the ceramic surface itself. An alternative promising method is slip casting.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Bonding to zirconia ceramic: adhesion methods and their durability10.1016/S0109-5641(98)00011-6 ↗
2. Long-term resin bond strength to zirconia ceramic
3. Durability of the resin bond strength to the alumina ceramic Procera10.1016/j.dental.2003.10.014 ↗
4. Ceramic Steel?10.1038/258703a0 ↗
5. Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis10.1016/j.biomaterials.2004.01.002 ↗
6. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
7. Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue10.1111/j.1151-2916.1999.tb02213.x ↗
8. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
9. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
10. Microstructural and crystallographic surface changes after grinding zirconia-based dental ceramics10.1002/jbm.b.30382 ↗
11. Influence of surface conditioning and cleaning methods on resin bonding to zirconia ceramic10.1016/j.dental.2010.10.004 ↗
12. Some recent progress in adhesion technology and science10.1016/j.crci.2004.11.016 ↗
13. Resin bonding to oxide ceramics for dental restorations10.1163/156856109X432721 ↗
14. Bonding to oxide ceramics – laboratory testing versus clinical outcome10.1016/j.dental.2014.06.007 ↗
15. Bond strength of composite luting cement to zirconia ceramic surfaces10.1016/j.dental.2005.02.005 ↗
16. Influence of prolonged thermal cycling and water storage on the tensile bond strength of composite to NiCr alloy10.1016/0109-5641(94)90017-5 ↗
17. 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures10.1016/j.dental.2006.03.008 ↗
18. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗
19. Damage accumulation and fatigue life of particle-abraded ceramics
20. Effect of blasting pressure, abrasive particle size and grade on phase transformation and morphological change of dental zirconia surface10.1016/j.surfcoat.2012.04.043 ↗
21. Surface characterization of dental Y-TZP ceramic after air abrasion treatment10.1016/j.jdent.2012.05.003 ↗
22. Effect of surface treatments on the properties and morphological change of dental zirconia
23. Surface characterization and bonding of Y-TZP following non-thermal plasma treatment10.1016/j.jdent.2012.10.002 ↗
24. The effect of atmospheric plasma treatment of dental zirconia ceramics on the contact angle of water10.1186/2196-4351-2-17 ↗
25. The bright future of dentistry with cold plasma – review
26. Influence of argon-ion bombardment of titanium surface on the cell behavior10.1016/j.surfcoat.2008.12.017 ↗
27. Ion-bombardment modification of surface morphology of solids10.1007/BF00352061 ↗
28. A unique ECR broad beam source for thin film processing
29. Proccesing of nanostructured zirconia composite ceramics with high aging resistance
30. Non-electrostatic diagnostics for ion beams and sputter effects10.1088/0741-3335/54/12/124005 ↗
31. Measurement of the force on microparticles in a beam of energetic ions and neutral atoms10.1063/1.3489795 ↗
32. Lieberman · 1994 · 571
33. Transient calorimetric diagnostics for plasma processing10.1140/epjd/e2013-40148-8 ↗
34. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
35. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by X-ray diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
36. Cleaning of porous aluminium titanate by oxygen plasma10.1007/s11090-006-9025-3 ↗
37. Enhanced hydrophilicity and biocompatibility of dental zirconia ceramics by oxygen plasma treatment10.3390/ma8020684 ↗
38. Chemical modification of titanium surfaces for covalent attachment of biological molecules10.1002/(SICI)1097-4636(199805)40:2<324::AID-JBM18>3.0.CO;2-L ↗