Effect of acid etching on tridimensional microstructure of etchable CAD/CAM materials
Source abstract
Abstract
Objective Evaluate if etching protocols affect superficial/internal microstructural integrity of CAD/CAM ceramic materials. Methods Sixty blocks (3×3×3mm) of IPS/Empress-LEU, IPS/e.max-LDC (Ivoclar-Vivadent) and Enamic-PIC (VITA) were used. Lateral surfaces from each block were isolated with Teflon strip and petroleum jelly to keep them untouched. Specimens were distributed into 6 groups (n=10): 1. no treatment (C); 2. hydrofluoric acid (HF) 5%, 20s (HF5%20s); 3. HF5%60s; 4. HF10%20s; 5. HF10%60s; 6. Monobond Etch&Prime (MBEP). Surface roughness (Sa) and 3D profile were obtained using a confocal-laser-optical-microscope (LEXT OLS 4000, Olympus), while element ratios (Si/K for LEU and LDC; Si/C for PIC) were recorded using energy dispersive spectroscopy (EDS). Superior (treated) and lateral (non-treated) surfaces were analyzed using scanning electron microscopy (SEM) (JSM 5600 LV, JEOL). Etching depth was measured on lateral surfaces. Data were submitted to ANOVA-One-Way and Tukey test (α=0.05). Results For LEU, only HF10% treatments produced statistically different roughness values and Si/K ratios compared to C group. Regarding LDC and PIC, groups HF5%60s and HF10% showed higher roughness values than C group. In the case of PIC, all treatments (except MBEP) produced lower Si/C ratios than C group. All treatments (except MBEP) produced higher etching depth values than C group for all materials, being HF10%60s the highest (LEU:403.2±11.4μm; LDC:617.4±75.7; PIC:291.6±6.5μm). HF10% produced more aggressive etching morphology patterns on superior and lateral surfaces (SEM). Treatments MBEP and HF5%20s, produced the least aggressive structural alterations. Acid etching produces superficial and internal alterations on ceramics' structural configuration. Significance Aggressive etching protocols of glass-ceramics may cause internal material loss, consequently, milder etching is recommended to treat those materials before adhesion procedures.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Porcelain veneers: a review of the literature10.1016/S0300-5712(99)00066-4 ↗
2. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
3. A new classification system for all-ceramic and ceramic-like restorative materials10.11607/ijp.4244 ↗
4. Principles of crystal phase formation in ivoclar vivadent glass-ceramics for dental restorations10.1016/j.jnoncrysol.2015.04.034 ↗
5. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
6. In-vitro strength degradation of dental ceramics and novel PICN material by sharp indentation10.1016/j.jmbbm.2013.05.004 ↗
7. VITA ENAMIC Technical and scientific documentation. Consulted on May 25th, 2017 on www.vitanorthamerica.com.
8. Microstructure characterization and SCG of newly engineered dental ceramics10.1016/j.dental.2016.03.018 ↗
9. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
10. Micro-shear bond strength of different resin cements to ceramic/glass-polymer CAD-CAM block materials10.1016/j.jpor.2016.02.003 ↗
11. Bond strength of novel CAD/CAM restorative materials to self-adhesive resin cement: the effect of surface treatments
12. Microtensile bond strength of composite cement to novel CAD/CAM materials as a function of surface treatment and aging10.2341/15-263-L ↗
13. Bonding effectiveness of luting composites to different CAD/CAM materials
14. Aspects of silane coupling agents and surface conditioning in dentistry: an overview10.1016/j.dental.2012.02.009 ↗
15. Resin-ceramic bonding: a review of the literature10.1067/mpr.2003.50 ↗
16. Microtensile bond strength of a resin cement to feldpathic ceramic after different etching and silanization regimens in dry and aged conditions10.1016/j.dental.2006.11.011 ↗
17. The impact of hydrofluoric acid surface treatments on the performance of a porcelain laminate restorative material10.1016/j.dental.2006.03.002 ↗
18. Effect of surface acid etching on the biaxial flexural strength of two hot-pressed glass ceramics10.1111/j.1532-849X.2008.00319.x ↗
19. Aspects of adhesion tests on resin–glass ceramic bonding
20. The effect of hydrofluoric acid concentration on the bond strength and morphology of the surface and interface of glass ceramics to a resin cement10.2341/14-133-L ↗
21. Surface/interface morphology and bond strength to glass ceramic etched for different periods10.2341/09-152-L ↗
22. Volkel T, Braziulis E. Monobond Etch & Prime, Scientific Documentation 2015. Consulted on May 25th, 2017 on www.ivoclarvivadent.com. 10.1093/earlyj/1.1.112-b.
23. Microshear bond strength of resin cements to lithium disilicate substrates as a function of surface preparation10.2341/14-240-L ↗
24. Effects of mechanical and chemical surface treatments on the resin–glass ceramic adhesion properties
25. Effect of etching with distinct hydrofluoric acid concentrations on the flexural strength of a lithium disilicate-based glass ceramic
26. A novel polymer infiltrated ceramic dental material10.1016/j.dental.2011.02.002 ↗
27. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics10.1016/S0022-3913(02)52704-9 ↗
28. The effect of hydrofluoric acid etching duration on the surface micromorphology, roughness, and wettability of dental ceramics
29. Crystallization and flexural strength optimization of fine-grained leucite glass-ceramics for dentistry10.1016/j.dental.2011.08.009 ↗
30. Fischer K, Bühler-Zemp P, Völkel T. IPS Empress CAD® Scientific documentation. Ivoclar Vivadent 2011. Consulted on May 25th, 2017 on www.ivoclarvivadent.com.
31. Monobond Etch & Prime Material Safety Data Sheet, 21/09/2016 version. Ivoclar Vivadent.
32. Rapid prototyping of glass microchannels10.1016/S0003-2670(03)01000-6 ↗
33. Self-etching ceramic primer versus hydrofluoric acid etching: etching efficacy and bonding performance10.1016/j.jpor.2017.06.002 ↗
34. New single-bottle ceramic primer: 6-month case report and laboratory performance10.5005/jp-journals-10024-1977 ↗
35. Bonding to silicate ceramics: conventional technique compared with a simplified technique
36. Aspects of bonding between resin luting cements and glass ceramic materials10.1016/j.dental.2014.01.017 ↗