Abstract
Objectives To evaluate the effect of the ceramic processing and aging method on the microstructure, optical, and mechanical properties of a third generation ultra-translucent zirconia, yttria partially stabilized zirconia (5Y-PSZ). Methods In-house discs were obtained through uniaxial and isostatic pressing an ultra-translucent Y-PSZ powder and sintering at 1450 °C for 2 h. As control, a commercial disc was milled from pre-sintered blocks fabricated with the same 5Y-PSZ powder through isostatic pressing and sintered under the same protocol. Discs were allocated into three groups according to aging condition as immediate (non-aged) and aged using autoclave or hydrothermal reactor at 134ºC for 20 h at 2.2 bar. Crystalline content and microstructure were evaluated using X-ray diffraction (XRD) and scanning electron microscopy (SEM), respectively. Optical properties were determined using reflectance data to calculate the contrast ratio (CR) and translucency parameter (TP). Mechanical properties were assessed by Vickers hardness, fracture toughness and biaxial flexural strength tests. Results XRD spectra revealed a prevalence of cubic (70%) and tetragonal (30%) phases, and the SEM images showed a dense fully crystalline ceramic matrix for both materials. Crystalline content and microstructure of the in-house and commercial 5Y-PSZs were not affected by aging. As-sintered 5Y-PSZs demonstrated similar CR (~0.6) and TP (~18) values, as well as Vickers hardness (~14 GPa) and fracture toughness (~3.8 Mpa.m1/2), with no significant alteration after both aging methods. In-house and commercial Y-PSZs Weibull moduli ranged from 3.0 to 5.3. 5Y-PSZ processing methods resulted in similar characteristic strength after sintering (592-618 Mpa). While commercial 5Y-PSZ showed no significant influence of aging on strength, hydrothermal reactor aging significantly decreased the in-house Y-PSZ characteristic strength (474 Mpa). Both 5Y-PSZs demonstrated high reliability up to 300-Mpa strength missions, with no detrimental effect of aging (88-100%). Significance Irrespective of the processing method, ultra-translucent 5Y-PSZ showed high aging resistance and translucency stability, as well as strength corresponding to the indication up to short-span anterior prostheses.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Dental materials and restorations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. New Y-TZP powders for medical grade zirconia10.1023/A:1018562917779 ↗
2. An overview of zirconia ceramics: basic properties and clinical applications10.1016/j.jdent.2007.07.008 ↗
3. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
4. Ceramic steel?10.1038/258703a0 ↗
5. Low‐temperature aging of Y‐TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
6. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
7. Stabilized zirconia as a structural ceramic: an overview10.1016/j.dental.2007.05.005 ↗
8. Effect of heat treatment on grain size, phase assemblage, and mechanical properties of 3 mol% Y‐TZP10.1111/j.1151-2916.1996.tb08980.x ↗
9. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
10. Ceramics for medical applications: a picture for the next 20 years10.1016/j.jeurceramsoc.2008.08.025 ↗
11. All-ceramic systems: laboratory and clinical performance10.1016/j.cden.2011.01.005 ↗
12. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
13. Restoring severely compromised anterior teeth with zirconia crowns and feather-edged margin preparations: a 3-year follow-up of a prospective clinical trial
14. Survival and complications of zirconia-based fixed dental prostheses: a systematic review10.1016/S0022-3913(12)60051-1 ↗
15. Clinical outcomes of partial and full-arch all-ceramic implant-supported fixed dental prostheses. A systematic review and meta-analysis10.1111/clr.13345 ↗
16. Corrigendum to “All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part II: Multiple-unit FDPs” [Dental Materials 31 (6) (2015) 624-639]10.1016/j.dental.2016.09.033 ↗
17. A systematic review of the survival and complication rates of zirconia-ceramic and metal-ceramic single crowns10.1111/clr.13306 ↗
18. A systematic review of the survival and complication rates of zirconia-ceramic and metal-ceramic multiple-unit fixed dental prostheses10.1111/clr.13277 ↗
19. Influence of hydrothermal and mechanical conditions on the strength of zirconia10.1016/j.actbio.2010.07.025 ↗
20. Aging resistance of an experimental zirconia-toughened alumina composite for large span dental prostheses: optical and mechanical characterization10.1016/j.jmbbm.2020.103659 ↗
21. Effect of intra-oral aging on t→m phase transformation, microstructure, and mechanical properties of Y-TZP dental ceramics10.1016/j.jmbbm.2017.04.014 ↗
22. Low-temperature degradation of Y-TZP ceramics: a systematic review and meta-analysis10.1016/j.jmbbm.2015.10.017 ↗
23. Randomized controlled clinical trial to compare posterior implant-supported modified monolithic zirconia and metal-ceramic single crowns: one-year results10.1111/jopr.12767 ↗
24. Prosthetic outcomes and clinical performance of CAD-CAM monolithic zirconia versus porcelain-fused-to-metal implant crowns in the molar region: 1-year results of a RCT10.1111/clr.13631 ↗
25. Fracture load and phase transformation of monolithic zirconia crowns submitted to different aging protocols10.2341/15-154-L ↗
26. Aging resistant ZTA composite for dental applications: microstructural, optical and mechanical characterization10.1016/j.dental.2020.05.011 ↗
27. Novel zirconia materials in dentistry
28. New multi-layered zirconias: composition, microstructure and translucency10.1016/j.dental.2019.02.017 ↗
29. Stability of Y-TZP during hydrothermal treatment: neutron experiments and stability considerations10.1016/j.jeurceramsoc.2004.03.025 ↗
30. Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications10.1016/j.dental.2018.03.006 ↗
31. Comparison of different low-temperature aging protocols: its effects on the mechanical behavior of Y-TZP ceramics10.1016/j.jmbbm.2016.02.017 ↗
32. Low-temperature degradation of Y-TZP ceramics: a systematic review and meta-analysis10.1016/j.jmbbm.2015.10.017 ↗
33. Degradation kinetics of high-translucency dental zirconias: mechanical properties and in-depth analysis of phase transformation
34. Mechanical and microstructural properties of ultra-translucent dental zirconia ceramic stabilized with 5 mol% yttria10.1016/j.jmbbm.2020.103974 ↗
35. Hydrothermal degradation methods affect the properties and phase transformation depth of translucent zirconia10.1016/j.jmbbm.2020.104021 ↗
36. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
37. Effect of changes in sintering parameters on monolithic translucent zirconia10.1016/j.dental.2014.09.003 ↗
38. The influence of altering sintering protocols on the optical and mechanical properties of zirconia: a review10.1111/jerd.12492 ↗
39. Phase change and mechanical properties of ZrO2-Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
40. Quantitative phase analysis from X-ray diffraction in Y-TZP dental ceramics: a critical evaluation10.1016/j.jdent.2014.08.010 ↗
41. Nanoindentation of yttria-doped zirconia: effect of crystallographic structure on deformation mechanisms10.1557/jmr.2009.0091 ↗
42. ceramics for structural applications
43. Factors affecting the translucency of monolithic zirconia ceramics: a review from materials science perspective
44. Making yttria-stabilized tetragonal zirconia translucent10.1016/j.dental.2014.08.375 ↗
45. Grain‐size‐dependent transformation behavior in polycrystalline tetragonal zirconia10.1111/j.1151-2916.1992.tb07832.x ↗
46. Quantitative phase analysis from X-ray diffraction in Y-TZP dental ceramics: a critical evaluation10.1016/j.jdent.2014.08.010 ↗
47. Fracture toughness analysis of ceramic and resin composite CAD/CAM material10.2341/18-161-L ↗
48. ADM guidance-Ceramics: fracture toughness testing and method selection10.1016/j.dental.2017.03.006 ↗
49. The compelling case for indentation as a functional exploratory and characterization tool10.1111/jace.13729 ↗
50. Graded ultra-translucent zirconia (5Y-PSZ) for strength and functionalities10.1177/0022034518771287 ↗
51. Ten-year outcome of three-unit fixed dental prostheses made from monolithic lithium disilicate ceramic10.14219/jada.archive.2012.0147 ↗
52. Fifteen-year outcome of three-unit fixed dental prostheses made from monolithic lithium disilicate ceramic10.1016/j.jdent.2019.08.001 ↗
53. In vivo aging of zirconia dental ceramics – part I: Biomedical grade 3Y-TZP
54. Intraoral low-temperature degradation of monolithic zirconia dental prostheses: results of a prospective clinical study with ex vivo monitoring10.1016/j.dental.2021.03.008 ↗