Edge chipping damage in lithium silicate glass-ceramics induced by conventional and ultrasonic vibration-assisted diamond machining
Source abstract
Abstract
Objectives Diamond machining of lithium silicate glass-ceramics (LS) induces extensive edge chipping damage, detrimentally affecting LS restoration functionality and long-term performance. This study approached novel ultrasonic vibration-assisted machining of pre-crystallized and crystallized LS materials to investigate induced edge chipping damage in comparison with conventional machining. Methods The vibration-assisted diamond machining was conducted using a five-axis ultrasonic high-speed grinding/machining machine at different vibration amplitudes while conventional machining was performed using the same machine without vibration assistance. LS microstructural characterization and phase development were performed using scanning electron microscopy (SEM) and x-ray diffraction (XRD) techniques. Machining-induced edge chipping depths, areas and morphology were also characterized using the SEM and Java-based imaging software. Results All machining-induced edge chipping damages resulted from brittle fractures. The damage scales, however, depended on the material microstructures; mechanical properties associated with the fracture toughness, critical strain energy release rates, brittleness indices, and machinability indices; and ultrasonic vibration amplitudes. Pre-crystallized LS with more glass matrix and lithium metasilicate crystals yielded respective 1.8 and 1.6 times greater damage depths and specific damage areas than crystallized LS with less glass matrix and tri-crystal phases in conventional machining. Ultrasonic machining at optimized amplitudes diminished such damages by over 50 % in pre-crystallized LS and up to 13 % in crystallized LS. Significance This research highlights that ultrasonic vibration assistance at optimized conditions may advance current dental CAD/CAM machining techniques by significant suppression of edge chipping damage in pre-crystallized LS.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Concurrent kinetics of crystallization and toughening in multicomponent biomedical SiO2-Li2O-P2O5-ZrO2 glass-ceramics10.1016/j.jnoncrysol.2020.120607 ↗
2. Bioactive and inert dental glass-ceramics10.1002/jbm.a.35923 ↗
3. Zirconia-reinforced lithium silicate (ZLS) mechanical and biological properties: a literature review10.1016/j.jdent.2021.103661 ↗
4. Lithium disilicate: the restorative material of multiple options
5. All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part I: single crowns (SCs)10.1016/j.dental.2015.02.011 ↗
6. Fracture rates and lifetime estimations of CAD/CAM all-ceramic restorations10.1177/0022034515608187 ↗
7. In-vitro fatigue and fracture testing of CAD/CAM-materials in implant-supported molar crowns10.1016/j.dental.2017.01.003 ↗
8. Mechanical and optical properties of monolithic CAD-CAM restorative materials10.1016/j.prosdent.2017.06.012 ↗
9. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
10. Saavedra GDSFA. Impact of crystallization firing process on the microstructure and flexural strength of zirconia-reinforced lithium silicate glass-ceramics10.1016/j.dental.2018.06.010 ↗
11. Optical behaviors, surface treatment, adhesion, and clinical indications of zirconia-reinforced lithium silicate (ZLS): a narrative review10.1016/j.jdent.2021.103722 ↗
12. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
13. Crack-healing during two-stage crystallization of biomedical lithium (di) silicate glass-ceramics10.1016/j.dental.2019.05.013 ↗
14. Machinability: zirconia-reinforced lithium silicate glass ceramic versus lithium disilicate glass ceramic10.1016/j.jmbbm.2019.103435 ↗
15. Effect of sintering parameters on phase evolution and strength of dental lithium silicate glass-ceramics10.1016/j.dental.2019.07.002 ↗
16. Responses of pre-crystallized and crystallized zirconia-containing lithium silicate glass ceramics to diamond machining10.1016/j.ceramint.2019.09.170 ↗
17. Strength-limiting damage and its mitigation in CAD-CAM zirconia-reinforced lithium-silicate ceramics machined in a fully crystallized state10.1016/j.dental.2020.09.012 ↗
18. Strength influencing variables on CAD/CAM zirconia frameworks10.1016/j.dental.2007.06.030 ↗
19. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
20. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
21. Influence of CAD/CAM milling, sintering and surface treatments on the fatigue behavior of lithium disilicate glass ceramic10.1016/j.jmbbm.2020.104133 ↗
22. Wear behavior of dental Y-TZP ceramic against natural enamel after different finishing procedures10.1016/j.dental.2012.04.010 ↗
23. Review of vibration-assisted machining10.1016/j.precisioneng.2007.08.003 ↗
24. Review of ultrasonic vibration-assisted machining in advanced materials10.1016/j.ijmachtools.2020.103594 ↗
25. Formation mechanism and modelling of exit edge-chipping during ultrasonic vibration grinding of deep-small holes of microcrystalline-mica ceramics10.1016/j.ceramint.2020.02.008 ↗
26. Green ceramic machining benefits through ultrasonic-assisted turning: an experimental investigation10.1007/s00170-021-08174-0 ↗
27. Zirconia responses to edge chipping damage induced in conventional and ultrasonic vibration-assisted diamond machining10.1016/j.jmrt.2021.05.005 ↗
28. Ultrasonic vibration assisted grinding of bio-ceramic materials: an experimental study on edge chippings with Hertzian indentation tests10.1007/s00170-015-8326-1 ↗
29. Mechanisms of edge chipping in laser-assisted milling of silicon nitride ceramics10.1016/j.ijmachtools.2008.09.006 ↗
30. Microstructural influence on damage-induced zirconia surface asperities produced by conventional and ultrasonic vibration-assisted diamond machining10.1016/j.ceramint.2021.05.301 ↗
31. Ultrasonic assisted high rotational speed diamond machining of dental glass ceramics
32. Phase characterization of lithium silicate biomedical glass-ceramics produced by two-stage crystallization10.1016/j.jnoncrysol.2019.01.027 ↗
33. Nucleation mechanisms in a SiO2-Li2O-P2O5-ZrO2 biomedical glass-ceramic: Insights on crystallisation, residual glasses and Zr4+ structural environment10.1016/j.jeurceramsoc.2021.12.009 ↗
34. VITA SUPRINITY Technical and Scientific Documentation, VITA Zahnfabrik H. Rauter GmbH & Co. KG, Germany, 2013. Vita-Suprinity-Technical-and-Scientific-Document.pdf (panadent.co.uk).
35. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
36. Fracture toughness testing of biomedical ceramic-based materials using beams, plates and discs10.1016/j.jeurceramsoc.2018.08.012 ↗
37. A universal relation for edge chipping from sharp contacts in brittle materials: a simple means of toughness evaluation10.1016/j.actamat.2006.10.061 ↗
38. “Edge toughness” and material properties related to the machining of dental ceramics10.1080/10940340008945711 ↗
39. Indentation brittleness of ceramics: a fresh approach10.1023/A:1018671823059 ↗
40. Ceramic grinding temperatures
41. Anisotropic residual stresses in partially crystallized Li2O–2SiO2 glass-ceramics10.1016/S0022-3093(99)00038-1 ↗
42. Microstructure and mechanical properties of nucleant-free Li2O-CaO-SiO2 glass-ceramics10.1016/j.actamat.2017.03.010 ↗
43. Experimental investigation of surface/subsurface damage formation and material removal mechanisms in SiC grinding10.1016/j.ijmachtools.2007.10.013 ↗
44. Machinability: zirconia-reinforced lithium silicate glass ceramic versus lithium disilicate glass ceramic10.1016/j.jmbbm.2019.103435 ↗
45. Evaluation of grinding-induced subsurface damage in optical glass BK710.1016/j.jmatprotec.2015.11.003 ↗
46. Ultrasonic assisted high rotational speed diamond machining of dental glass ceramics
47. Malkin · 2008
48. Additive manufacturing technologies: current status and future perspectives10.1111/jopr.13477 ↗
49. Stereolithography-based additive manufacturing of lithium disilicate glass ceramic for dental applications10.1016/j.msec.2020.111180 ↗
50. Additive manufacturing of lithium disilicate with the LCM process for classic and non-prep veneers: preliminary technical and clinical case experience10.3390/ma15176034 ↗
51. Additive manufacturing in dentistry: current technologies, clinical applications, and limitations10.1007/s40496-020-00288-w ↗
52. Additive manufacturing of zirconia ceramic and its application in clinical dentistry: a review10.3390/dj9090104 ↗
53. Materials in digital dentistry—a review10.1111/jerd.12566 ↗
54. Additive manufacturing of lithium disilicate glass-ceramic by vat polymerization for dental appliances10.1016/j.dental.2022.11.005 ↗
55. Additive manufacturing of ceramics for dental applications: a review10.1016/j.dental.2019.02.026 ↗
56. 3D printing restorative materials using a stereolithographic technique: a systematic review10.1016/j.dental.2020.11.030 ↗
57. Load-bearing capacity of CAD/CAM 3D-printed zirconia, CAD/CAM milled zirconia, and heat-pressed lithium disilicate ultra-thin occlusal veneers on molars10.1016/j.dental.2020.01.016 ↗
58. Comparison of marginal and internal fit of pressed lithium disilicate veneers fabricated via a manual waxing technique versus a 3D printed technique10.1111/jerd.12675 ↗
59. Marginal and internal gap of handmade, milled and 3D printed additive manufactured patterns for pressed lithium disilicate onlay restorations