Mechanical and physical properties of splint materials for oral appliances produced by additive, subtractive and conventional manufacturing
Source abstract
Abstract
To investigate the flexural strength (FS), elastic modulus (E), Martens hardness (HM), water sorption (wsp), water solubility (wsl) and degree of conversion (DC) of 3D-printed, milled and injection molded splint materials. Specimens (N = 1140) were fabricated from five 3D-printed (GR-22 flex, GR-10 guide, ProArt Print Splint clear, V-Print Splint, V-Print Splint comfort), five milled (BioniCut, EldyPlus, ProArt CAD Splint clear, Temp Premium Flexible, Thermeo) and two injection molded (PalaXPress clear, Pro Base Cold) materials. FS, E, HM, wsp, wsl and DC were tested initially (24 h, 37 °C, H2O), after water storage (90 d, 37 °C, H2O) as well as after thermal cycling (5000 thermal cycles, 5/55 °C). Data were analyzed with Kolmogorov-Smirnov, Kruskal- Wallis, Mann-Whitney U test and Spearman’s correlation (p < 0.05). Initially, the mean flexural strength values ranged from 1.9 to 90.7 MPa for printed, 3.8 to 107 MPa for milled and 99.7 to 102 MPa for injection molded materials. The initial mean elastic modulus values were 0.0 to 2.4 GPa for printed, 0.1 to 2.7 GPa for milled and 2.8 GPa for injection molded materials. The initial mean Martens hardness values were 14.5 to 126 N/mm2 for printed, 50.2 to 171 N/mm2 for milled and 143 to 151 N/mm2 for injection molded materials. Initially, the mean water sorption values ranged from 23.1 to 41.2 μg/mm3 for printed, 4.5 to 23.5 μg/mm3 for milled and from 22.5 to 23.3 μg/ mm3 for injection molded materials. The initial mean water solubility values ranged from 2.2 to 7.1 μg/mm3 for printed, 0.0 to 0.5 μg/mm3 for milled and 0.1 to 0.3 μg/mm3 for injection molded materials. After water storage and thermal cycling most of the values decreased and some increased. The mean DC values ranged initially from 72.3 to 94.5 %, after water storage from 74.2 to 96.8 % and after thermal cycling from 75.6 to 95.4 % for the printed materials. The mechanical and physical properties of printed, milled and injection molded materials for occlusal devices vary and are influenced by aging processes. For clinical applications, materials need to be chosen according to the specific indications.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Temporomandibular Joint Disorders · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Evaluation of various treatment modalities in sleep bruxism10.1016/j.prosdent.2015.02.025 ↗
2. Topical review: sleep bruxism, headaches, and sleep-disordered breathing in children and adolescents
3. A study of the flexural strength and surface hardness of different materials and technologies for occlusal device fabrication10.1016/j.prosdent.2018.09.022 ↗
4. Polishability and wear resistance of splint material for oral appliances produced with conventional, subtractive, and additive manufacturing10.1016/j.jmbbm.2017.07.019 ↗
5. Comparing the mechanical properties of pressed, milled, and 3D-printed resins for occlusal devices10.1016/j.prosdent.2019.10.024 ↗
6. Pilot in-vitro study on insertion/removal performance of hand-cast, milled and 3D printed splints10.1016/j.jmbbm.2021.104612 ↗
7. Fracture resistance and 2-body wear of 3-dimensional-printed occlusal devices10.1016/j.prosdent.2018.04.007 ↗
8. Computer-aided design and fabrication of dental restorations: current systems and future possibilities10.14219/jada.archive.2006.0389 ↗
9. 3D printing in dentistry-state of the art10.2341/18-229-L ↗
10. Characterization of occlusal splint materials: CAD-CAM versus conventional resins10.1016/j.jmbbm.2021.104813 ↗
11. Comparison of hardness and polishability of various occlusal splint materials10.1016/j.jmbbm.2020.104270 ↗
12. Evaluation of wear behaviour of various occlusal splint materials and manufacturing processes10.1016/j.jmbbm.2021.105053 ↗
13. Polymers for conventional, subtractive, and additive manufacturing of occlusal devices differ in hardness and flexural properties but not in wear resistance10.1016/j.dental.2020.11.020 ↗
14. Evaluation of the mechanical properties and degree of conversion of 3D printed splint material10.1016/j.jmbbm.2020.104254 ↗
15. In vitro study on the influence of postpolymerization and aging on the Martens parameters of 3D-printed occlusal devices10.1016/j.prosdent.2019.12.026 ↗
16. The effect of artificial aging on Martens hardness and indentation modulus of different dental CAD/CAM restorative materials10.1016/j.jmbbm.2018.06.028 ↗
17. Influence of different postpolymerization strategies and artificial aging on hardness of 3D-printed resin materials: an in vitro study10.11607/ijp.6634 ↗
18. Water sorption, water solubility, degree of conversion, elastic indentation modulus, edge chipping resistance and flexural strength of 3D-printed denture base resins10.1016/j.jmbbm.2022.105565 ↗
19. Comparison of flexural strength of different CAD/CAM PMMA-based polymers10.1111/jopr.12755 ↗
20. The anisotropicity of the flexural properties of an occlusal device material processed by stereolithography10.1016/j.prosdent.2016.03.018 ↗
21. Objects build orientation, positioning, and curing influence dimensional accuracy and flexural properties of stereolithographically printed resin10.1016/j.dental.2018.09.011 ↗
22. Mechanical properties of injection-molded thermoplastic denture base resins10.3109/00016357.2010.517557 ↗
23. Comparative analysis of mechanical properties of orthodontic aligners produced by different contemporary 3D printers10.1111/ocr.12537 ↗
24. Evaluation of flexible three-dimensionally printed occlusal splint materials: an in vitro study10.1016/j.dental.2023.08.178 ↗
25. Comparison of mechanical properties of PMMA disks for digitally designed dentures10.3390/polym13111745 ↗
26. Effect of post-curing light exposure time on the physico-mechanical properties and cytotoxicity of 3D-printed denture base material10.1016/j.dental.2021.10.011 ↗
27. Effect of monomer type on the CC degree of conversion, water sorption and solubility, and color stability of model dental composites10.1016/j.dental.2017.01.010 ↗
28. Strength and surface properties of a 3d-printed denture base polymer10.1111/jopr.13413 ↗
29. Water sorption, solubility, and translucency of 3d-printed denture base resins