journal article·2000-11

The effect of hybrid layer thickness on bond strength: demineralized dentin zone of the hybrid layer

M Hashimoto, H Ohno, K Endo, M Kaga, H Sano, H Oguchi

Dental Materials· Volume 16· Issue 6
Publisher page

Abstract

Objectives The purpose of this study was to evaluate the correlation between hybrid layer thickness and bond strength using specimens acid-conditioned for varying lengths of time. Methods The dentin surfaces of human premolars, sectioned to remove the enamel from the labial surface, were conditioned with 35.0% phosphoric acid of an adhesive resin system (Scotchbond Multi-Purpose; 3M) for 15 (as directed by the manufacturer), 60, 120, or 180 s (experimental acid-conditioning times). The bonded specimens were then sectioned perpendicular to the adhesive interface to measure the hybrid layer thickness by SEM. The specimens for the micro-tensile test were sectioned perpendicular to the adhesive interface and trimmed to an hourglass-shape. Then, the micro-tensile test was performed at a crosshead speed of 1.0 mm/min. The bond strengths and hybrid layer thickness were statistically compared with Student's t-test (p < 0.05). All fractured surfaces were also observed by SEM. Results Significant differences between the groups exposed to acid for 15 and 60 s, and those exposed for 120 and 180 s were observed in hybrid layer thickness and bond strength (p < 0.05). SEM observation of the fractured surfaces revealed that a demineralized dentin zone without resin impregnation remained within the hybrid layer. Significance A demineralized dentin zone was formed in the bond structures after prolonged acid-conditioning, resulting in low bond strength. The shrinkage of the hybrid layer due to desiccation during the SEM examination process provided evidence of the presence of the demineralized dentin zone within the hybrid layer.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Health and Care Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Bonding strength to bovine dentin with 4-META/MMA-TBB resin: long-term stability and influence of water
2. Effect of HEMA on bonding to dentin10.1016/0109-5641(92)90067-M ↗
3. Penetration of a dentin bonding agent into dentin
4. Dentin bond durability after three years using a dentin bonding agent with and without priming10.1016/S0109-5641(96)80038-8 ↗
5. Relation between water content in acetone/alcohol-based primer and interfacial ultrastructure10.1016/S0300-5712(96)00090-5 ↗
6. In vivo degradation of resin–dentin bonds in humans over 1–3 years10.1177/00220345000790060601 ↗
7. Influence of different etching times on hybrid layer formation and tensile bond strength
8. Improving bond strength through acid etching of dentin and bondind to wet dentin surfaces10.14219/jada.archive.1992.0248 ↗
9. Relationship between surface area for adhesion and tensile bond strength-evaluation of a micro-tensile bond test10.1016/0109-5641(94)90067-1 ↗
10. Permeability of dentin adhesive agents
11. Comparative SEM and TEM examination of the ultrastructure of the resin–dentin interdiffusion zone10.1177/00220345930720020501 ↗
12. Interfacial structure between dentin and seven dentin bonding systems revealed using argon ion beam etching
13. Vibrational analysis by Raman spectroscopy of the interface between dental adhesive resin and dentin10.1177/00220345910700071501 ↗
14. A TEM study of two water-based adhesive systems bonded to dry and wet dentin10.1177/00220345980770010501 ↗
15. Microporous dentin zone beneath resin-impregnated layer
16. Dentin bonding: SEM comparison of the resin–dentin interface in primary and permanent teeth10.1177/00220345960750061101 ↗
17. A tensile test to facilitate identification of defects in dentin bonded specimens10.1016/S0300-5712(97)00021-3 ↗
18. Effect of long-term water storage on dentin bonding