A physico-chemical explanation of the post-polymerization shrinkage in dental resins
Source abstract
Abstract
Unlabelled The main problem of a methacrylated dental resin's photopolymerization is the shrinkage phenomenon. This occurs, as expected, during light irradiation but also, unexpectedly, during about 24h after photopolymerization (i.e. during the so-called 'post-polymerization' stage). During this period, the conversion degree does not change significantly (no more initiation, very limited, if any, propagation reaction) but free radicals concentration decreases. Objectives To better understand what happens during the 24h after the photopolymerization, a thermal study of these resins is investigated at first and an explanation is then discussed. Methods In this paper, the glass transition temperatures (T(g)) are measured at 0 and 24h by DMA. The post-shrinkage phenomenon is observed by TMA. Conversion degree (DC) is followed by Raman and free radical decay by ESR spectroscopy. Results T(g) increases significantly during post-polymerization (55-80 degrees C). The same samples were studied by TMA at room temperature and shrinkage is observed. The fact that the degree of conversion (DC) does not increase significantly and that the 'post-shrinkage' occurs at TSignificanceThe proposed explanation is that, as photopolymerization of dental resins is very fast, a large excess of free volume is trapped in non-equilibrated samples. As they have no time to return to an equilibrium state, free volume should decrease below T(g) and samples do physically shrink during the first 24h. As a consequence, free radicals can come into 'contact' and undergo limited propagation but significant termination justifying the decrease in overall radical concentration.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Photopolymerization techniques and applications · Dental materials and restorations · Radiation Effects and Dosimetry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Temperature rise during polymerization of visible light-activated composite resins10.1016/S0109-5641(88)80059-9 ↗
2. Resisting the curing contraction with adhesive composites10.1016/0022-3913(86)90173-3 ↗
3. The micro-Raman spectroscopy, a useful tool to determine the degree of conversion of light-activated composite resins10.1002/(SICI)1097-4636(1999)48:5<675::AID-JBM11>3.0.CO;2-P ↗
4. Does an incremental filling technique reduce polymerization shrinkage stresses?10.1177/00220345960750030301 ↗
5. Polymerization shrinkage: effects of constraint and filling technique in composite restorations10.1016/S0109-5641(03)00098-8 ↗
6. Shrinkage stresses associated with incremental composite filling techniques
7. The polymerization contraction of visible-light activated composite resins10.1016/0300-5712(88)90032-2 ↗
8. The polymerization shrinkage of composite resins10.1016/0109-5641(89)90092-4 ↗
9. Direct filling resins: dimensional changes resulting from polymerization shrinkage and water sorption10.14219/jada.archive.1953.0089 ↗
10. A study of the volumetric setting shrinkage of some dental materials10.1002/jbm.820160206 ↗
11. A simple method for the measurement of polymerization shrinkage in dental composites10.1016/S0109-5641(99)00073-1 ↗
12. Curing shrinkage and volumetric changes of resin-modified glass ionomer restorative materials10.1016/0109-5641(95)80035-2 ↗
13. Wilson HJ. Proceedings of the international symposium on fotofil dental restorative Ed; 1978, p. 11–6
14. Determination of polymerization shrinkage kinetics in visible-light-cured materials: methods development10.1016/S0109-5641(05)80030-2 ↗
15. Strain gauge method for measuring polymerization contraction of composite restoratives10.1016/0300-5712(91)90081-9 ↗
16. Laser interferometric method for measuring linear polymerization shrinkage in light cured dental restoratives10.1016/S0109-5641(01)00057-4 ↗
17. Resin cure determination by polymerization shrinkage10.1016/0109-5641(95)80060-3 ↗
18. Post-irradiation polymerization of visible light-activated composite resin10.1177/00220345830620031201 ↗
19. Post-curing of dental restorative resin10.1002/pen.760231303 ↗
20. Polymerization of methyl methacrylates10.1002/macp.1948.020010301 ↗
21. Identification of free radicals trapped in solid methacrylated resins10.1002/pola.10692 ↗
22. Remaining methacrylate groups in composite restorative materials10.3109/00016357809027569 ↗
23. Formation and properties of network polymeric materials10.1002/pen.760191005 ↗
24. Effect of chemical structure on degree of conversion in light-cured dimethacrylate-based dental resins10.1016/j.biomaterials.2003.09.078 ↗
25. Diffusion model for volume recovery in glasses10.1021/ma00234a032 ↗
26. A free-volume interpretation of the influence of the glass transition on diffusion in amorphous polymers10.1002/app.1978.070220823 ↗
27. Temperatures of the oral cavity in 50 healthy students
28. Reduction of polymerization contraction stress for dental composites by two-step light-activation10.1016/S0109-5641(01)00066-5 ↗
29. Application of dynamic mechanical testing to thermoset and coatings research and development