Abstract

Objectives Evaluation of a new surface treatment method to obtain a good bond strength between a luting composite and several ceramics. Methods Specimen preparation and test procedure were done according to ISO 10477 Amendment 1. The surfaces of Empress II, InCeram-Alumina, InCeram-Zirconia and Frialit (ZrO2) were ground under water-cooling with 400 grit grinding paper, afterwards polished with 800 grit and air-dried. Each ceramic material investigated was divided into three groups of 10 specimens each. Group 1 was flame-treated with the PyrosilPen for 2.5 s, group 2 for 5 s and group 3 for 10 s/cm(2). After the flame treatment, a methacryl silane was applied followed by a luting composite. Prior to measuring shear bond strength, the specimens were thermocycled 5,000 times in a water-bath between +5 and +55 degrees C. Furthermore, SEM- and Fourier-transform infrared spectrophotometer (FT-IR)-investigations were done. As a control, Empress II etched and silaned was used. Results Shear bond strength measurements indicated that the optimal treatment time was 5 s/cm(2). Regarding this time the following bond strength values between the luting composite and the various ceramics were obtained: Empress II 23 (5)MPa, InCeram-Alumina 23 (5)MPa, InCeram-Zirconia 13 (8)MPa, and Frialit 16 (6)MPa. The control achieved 27 (6)MPa. On all surfaces of the flamed specimens Si could be detected by FT-IR.Significance. The PyrosilPen-Technology is an easy and effective method for surface-treating silicate, aluminum oxide and zirconium oxide ceramics to obtain good bonding to luting composites.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Effect of prebonding procedures on shear bond strength of resin composite to pressable ceramic
2. Shear vs. tensile bond strength of resin composite bonded to ceramic10.1177/00220345950740091401 ↗
3. Dentin bond strength and marginal adaptation: direct composite resins vs. ceramic inlays
4. Microtensile strength of composite bonded to hot-pressed ceramics
5. Molar fracture resistance after adhesive restoration with ceramic inlays or resin-based composites
6. In vitro evaluation of a glass ceramic restorative material10.1046/j.1365-2842.1997.00560.x ↗
7. Comparison of composite resin-to-porcelain bond strength with three adhesives
8. The influence of a simplified application technique for ceramic inlays on the margin quality
9. Matos · Am J Dent · 1999 · 12 · 113
10. A study of the bond strength and color of ultra-low fusing porcelain
11. Surface energy of etched ceramic
12. Crack formation of all-ceramic crowns dependent on different core build-up and luting materials10.1016/S0300-5712(98)00049-9 ↗
13. Pilot study on the early shear strength of porcelain–dentin bonding using dual-cure cements10.1016/S0022-3913(99)70270-2 ↗
14. Evaluation of the marginal and internal adaptation of different ceramic and composite inlay systems after an in vitro fatigue test
15. Tensile bond strengths of dual-cured cements between a glass–ceramic and enamel10.1016/S0022-3913(98)70169-6 ↗
16. IPS Empress inlays and onlays after four years—a clinical study10.1016/S0300-5712(98)00059-1 ↗
17. Adhesion of composite to porcelain with various surface conditions10.1016/S0022-3913(05)80076-9 ↗
18. Leucite-reinforced glass ceramic inlays and onlays after six years
19. Ceramic restorations for posterior teeth: guidelines for the clinician10.1111/j.1708-8240.1999.tb00381.x ↗
20. Microleakage of dentin-bonded crowns placed with different luting materials
21. All-ceramic restorations by new direct ceramic machining process (DCM)
22. Untersuchungen zum Ermüdungsverhalten der Dentalkeramiken Zirkonoxid-TZP und In-Ceram
23. Vergleichende Untersuchungen zur Bruchfestigkeit von vollkeramischen Frontzahnbrücken
24. Festigkeit und Randzonenschädigung von Zirconia-TZP-Keramik nach simulierter Innenbearbeitung von Kronen
25. Kronen aus Hochleistungkeramik. Zirkonoxid, ein neuer Werkstoff in der Kronenprothetik
26. CAD/CAM-gefertigte Kronengerüste aus Zirkonoxid-Keramik
27. Restaurations indirectes en céramique
28. Future ceramic systems
29. Belastbarkeit vollkeramischer Seitenzahnbrücken aus neuen Hartkeramiken
30. Belastbarkeit von zirkonoxidverstärkter In-ceram Alumina-Keramik
31. Prothetische Versorgung avitaler Frontzähne mit vollkeramischen Stiftkernaufbauten und Kronen
32. Clinical evaluation of all-ceramic zirconia posts. A pilot study
33. Erste klinische Erfahrungen mit Wurzelstiften aus Zirkonoxidkeramik
34. All-ceramic posts and cores: the state of the art
35. Adhäsion von Kompositen an hochfesten Strukturkeramiken nach unterschiedlicher Oberflächenbehandlung
36. Experimentelle untersuchungen zur befestigung von restaurationen aus zirkonoxid und titan
37. Factors influencing adhesion to Al2O3- and ZrO2-ceramics
38. Long-term resin bond strength to zirconia ceramic
39. Bonding to zirconia ceramic: adhesion methods and their durability10.1016/S0109-5641(98)00011-6 ↗
40. Evaluation of three silicoating methods for resin-bonded protheses
41. Strength of bond with with Comspan opaque to three silicoated alloys and titanium
42. Adhesion of resins to Ag–Pd alloy by means of the silicoating technique10.1177/00220345870660081901 ↗
43. A comparison of two silicoating techniques10.1111/j.1532-849X.1994.tb00137.x ↗
44. Effectiveness of a method used in bonding resins to metal10.1016/0022-3913(90)90150-B ↗
45. Resin–metal bonding systems: a review of the silicoating and Kevloc systems
46. Das silicoater verfahren nach fünfjähriger klinischer Bewährung
47. Musil · 1989
48. Kulzer's silicoater: a new technique for bonding methacrylates to metal
49. US Patent 4,600,390. Apparatus and method for applying a silicon oxide-containing adhesion-promoting layer on metallic dental prostheses, Kulzer, Wehrheim, Germany.
50. Etablierte und neuentwickelte Metall-Kunststoff-Verbundverfahren im experimentellen Vergleich
51. Kleben und Klebetechniken
52. Kappert H-F, Schüren M, Fritsch F. Dauerfestigkeitsprüfung des Metall-Kunststoff-Verbundes unter dem Einfluss von Temperaturlastwechseln Quintessenz Zahntech 1996;22:293–307.
53. Neue Kunststoff-Metall-Verbundsysteme und ihre legierungsabhängige Haftqualität
54. SurA Instruments. Jena, Germany, Company brochure and instructions for use.