Unlabelled The aim of this study was to examine the morphology of the hybrid layer (HL) of bonded water-stored specimens after different chemical pre-treatments of dentin. Materials and methods Twenty-seven recently extracted human molars were selected. Fifty-four dentin disks in middle/deep dentin were obtained with a slow speed saw with a diamond-impregnated disk under water lubrication. Smear layers were created with 180 grit silicon carbide under running water for 1 min. Different pre-treatments of dentin were: Group (1) no treatment; Group (2) 35% H3PO4 etch for 15 s followed by 10% glutaraldehyde for 120 s; Group (3) 37% H3PO4 etch for 15 s followed by 5% NaOCl for 120 s. Three dentin bonding agents (DBAs), Prime and Bond NT (P and B), AdmiraBond (AB), and Clearfil SE Bond (SEB) were applied in association with a resin composite following the manufacturers' directions. Each specimen was then longitudinally sectioned and polished with wet SiC papers (up to #4000 grit). Impressions of the polished dentin were immediately taken with a silicone impression material. Bonded specimens were then stored for 3 or 12 h in deionized water. Further impressions of stored specimens were taken after air-drying of specimens for 10 s. Positive replicas were obtained using a polyether impression material. All the replicas and the original specimens were inspected by SEM. Results A line of droplets (0.5-4 microm in diameter) was observed along the region of the adhesive-HL junction in all replicas of specimens stored in water, except in group 3, when P and B and AB were used. When SEB was used in each group the droplet were found in all groups except the zone of droplets was thinner. No differences in droplets dimensions were seen between 3 or 12 h water storage, or between the different dentin treatments. Conclusions The replica procedure used in this study was able to detect water trapped in the adhesive-HL region that was released during the setting of the impression material. The droplets observed in this region support the hypothesis that there can be bidirectional water movement within the adhesive-HL complex.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Goracci · Marginal seal and biocompatibility of a fourth-generation bonding agent Dent Mater · 1995 · 11 · 343
2. In vitro interfacial relationship between human dentin and one-bottle dental adhesives10.1016/S0109-5641(97)80032-2 ↗
3. Analysis of dental adhesives system using scanning electron microscopy
4. Comparative SEM and TEM examination of the ultrastructure of the resin-dentin interdiffusion zone10.1177/00220345930720020501 ↗
5. The promotion of adhesion by the infiltration of monomers into tooth substrates10.1002/jbm.820160307 ↗
6. Morphological aspects of the resin–dentin interdiffusion zone with different dentin adhesive systems10.1177/00220345920710081301 ↗
7. Water sorption of several bonding resins
8. Early elution of uncured components from light-activated dental composites
9. Effect of delayed activation of light-cured resin composites on bonding of all-in-one adhesives
10. Single-step adhesives are permeable membranes10.1016/S0300-5712(02)00064-7 ↗
11. Nanoleakage: leakage within the hybrid layer
12. Comparative SEM and TEM observations of nanoleakage within the hybrid layer
13. Nanoleakage patterns of four dentin bonding system10.1016/S0109-5641(99)00085-8 ↗
14. Fluoride penetration into the hybrid layer from a dentin adhesive
15. Influence of polymer morphology of water treeing10.1109/94.368653 ↗
16. Silver tree10.1109/94.485525 ↗
17. Water treeing—a potential mechanism for degradation of dentin adhesives
18. Two modes of nanoleakage expression in single-step adhesives10.1177/154405910208100708 ↗
19. How can nanoleakage occur in self-etching adhesive systems that demineralize and infiltrate simultaneously?
20. Comparative SEM and TEM observation of nanoleakage within the hybrid layer
21. Nanoleakage at the composite–dentin interface: a review
22. Self-contamination of deep dentin by dentin fluid
23. Effect of smear layers on the bonding of a self-etching primer to dentin
24. Effect of smear layer thickness on bond strength mediated by three all-in-one self-etching priming adhesives
25. Field emission SEM comparison of four postfixation drying techniques for human dentin10.1002/jbm.820290911 ↗
26. Microscopy investigations. Techniques, results, limitations
27. Long-term durability of resin dentin interface: nanoleakage vs. microtensile bond strength
28. In vivo degradation of resin-dentin bonds in humans over 1 to 3 years10.1177/00220345000790060601 ↗
29. Effect of removal of surface collagen fibrils on resin-dentin bonding10.1016/S0109-5641(99)00052-4 ↗
30. Correlation of dentin bond durability with water absorption of bonding layer10.4012/dmj.18.11 ↗
31. Osmotically induced tissue expansion with hydrogels: a new dimension in tissue expansion? A preliminary report10.1016/S1010-5182(05)80353-1 ↗
32. Mechanical and thermal properties of gelatin films at different degrees of glutaraldehyde crosslinking10.1016/S0142-9612(00)00236-2 ↗
33. Swelling of poly(vinyl amine)gels: applicability of the Donnan theory
34. Dentin proteoglycans: an immunocytochemical FEISEM study10.1002/jbm.10102 ↗
35. Interfacial chemistry of the dentin/adhesive bond10.1177/00220345000790070501 ↗
36. Quantifying adhesive penetration in adhesive/dentin interface using confocal Raman microspectroscopy10.1002/jbm.1215 ↗
37. Effect of collagen crosslinking on collagen–water interaction (A DSC investigation)10.1016/S0934-8832(11)80013-2 ↗