journal article·2014-12

Effects of aging procedures on the topographic surface, structural stability, and mechanical strength of a ZrO2-based dental ceramic

Caroline Cotes, Anelyse Arata, Renata M. Melo, Marco A. Bottino, João P.B. Machado, Rodrigo O.A. Souza

Dental Materials· Volume 30· Issue 12
Publisher page

Abstract

Objective To determine the effects of different aging methods on the degradation and flexural strength of yttria-stabilized tetragonal zirconia (Y-TZP) METHODS: Sixty disc-shaped specimens (∅, 12mm; thickness, 1.6mm) of zirconia (Vita InCeram 2000 YZ Cubes, VITA Zahnfabrik) were prepared (ISO 6872) and randomly divided into five groups, according to the aging procedures (n=10): (C) control; (M) mechanical cycling (15,000,000 cycles/3.8Hz/200N); (T) thermal cycling (6,000 cycles/5-55°C/30s); (TM) thermomechanical cycling (1,200,000 cycles/3.8Hz/200N with temperature range from 5°C to 55°C for 60s each); (AUT) 12h in autoclave at 134°C/2bars; and (STO) storage in distilled water (37°C/400 days). After the aging procedures, the monoclinic phase percentages were evaluated by X-ray diffraction (XRD), and topographic surface analysis was performed by 3D profilometry. The specimens were then subjected to biaxial flexure testing (1mm/min, load 100kgf, in water). The biaxial flexural strength data (MPa) were analyzed by 1-way ANOVA and Tukey's test (α=0.05). The data for monoclinic phase percentage and profilometry (Ra) were analyzed by Kruskal-Wallis and Dunn's tests. Results ANOVA revealed that flexural strength was affected by the aging procedures (p=0.002). The M (781.6MPa) and TM (771.3MPa) groups presented lower values of flexural strength than did C (955MPa), AUT (955.8MPa), T (960.8MPa) and STO (910.4MPa). The monoclinic phase percentage was significantly higher only for STO (12.22%) and AUT (29.97%) when compared with that of the control group (Kruskal-Wallis test, p=0.004). In addition, the surface roughnesses were similar among the groups (p=0.165). Significance Water storage for 400 days and autoclave aging procedures induced higher phase transformation from tetragonal to monoclinic; however, they did not affect the flexural strength of Y-TZP ceramic, which decreased only after mechanical and thermomechanical cycling.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Aerogels and thermal insulation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Zirconia implant abutments: a review10.4317/medoral.16.e50 ↗
2. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
3. Mechanical properties, phase stability, and biocompatibility of (Y, Nb)-TZP/Al(2)O(3) composite abutments for dental implant10.1002/1097-4636(2000)53:4<438::AID-JBM19>3.0.CO;2-3 ↗
4. Fracture strength of four-unit Y-TZP FPD cores designed with varying connector diameter. An in-vitro study10.1111/j.1365-2842.2007.01770.x ↗
5. An overview of zirconia ceramics: basic properties and clinical applications10.1016/j.jdent.2007.07.008 ↗
6. Fracture resistance of yttria-stabilized zirconia dental implant abutments10.1111/j.1532-849X.2008.00378.x ↗
7. Low temperature degradation -aging- of zirconia: A critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
8. Low temperature aging of Y–TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
9. Crystalline phase change in yttria-partially-stabilized zirconia by low-temperature annealing10.1111/j.1151-2916.1984.tb19668.x ↗
10. Transformation of yttria-doped tetragonal ZrO2 polycrystals by annealing in water
11. Role of H2O on the degradation process of Y-TZP10.1007/BF01756800 ↗
12. A critical comparison of methods for the determination of the aging sensitivity in biomedical grade yttria-stabilized zirconia10.1002/jbm.b.30123 ↗
13. Tressler · 1990
14. Effect of HIPping, stress and surface finish on the environmental degradation of Y-TZP ceramics10.1023/A:1011284016483 ↗
15. The effect of low temperature aging on the mechanical property & phase stability of Y-TZP ceramics10.4047/jap.2009.1.3.113 ↗
16. Influence of hydrothermal and mechanical conditions on the strength of zirconia10.1016/j.actbio.2010.07.025 ↗
17. Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems10.1016/j.dental.2006.06.036 ↗
18. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system10.1111/j.1151-2916.1984.tb19614.x ↗
19. Stress fatigue: basic principles and prosthodontic implications
20. In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics10.1016/j.prosdent.2006.08.004 ↗
21. Effect of fatigue on fracture toughness and phase transformation of Y-TZP ceramics by X-ray diffraction and Raman spectroscopy10.1002/jbm.b.31964 ↗
22. Flexural strength, fatigue life, and stress-induced phase transformation study of Y-TZP dental ceramic10.1002/jbm.b.31064 ↗
23. Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading10.1016/j.jmbbm.2013.01.005 ↗
24. Air-particle abrasion on zirconia ceramic using different protocols: Effects on biaxial flexural strength after cyclic loading, phase transformation and surface topography10.1016/j.jmbbm.2013.04.018 ↗
25. Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia10.1016/j.biomaterials.2005.11.021 ↗
26. Influence of low-temperature environmental exposure on the mechanical properties and structural stability of dental zirconia10.1111/j.1532-849X.2011.00838.x ↗
27. Low-temperature degradation of different zirconia ceramics for dental applications10.1016/j.actbio.2011.11.016 ↗
28. Effect of mechanical cycling on the flexural strength of densely sintered ceramics10.1016/j.dental.2005.11.025 ↗
29. Long-term strength of ceramics for biomedical applications
30. Predicting lifetimes of materials and material structures10.1016/0109-5641(95)80050-6 ↗
31. Accelerated aging characteristics of three yttria-stabilized tetragonal zirconia polycrystalline dental materials10.1016/S0022-3913(12)60166-8 ↗