journal article·2003-11

Stress-relieving and porcelain firing cycle influence on marginal fit of commercially pure titanium and titanium–aluminum–vanadium copings

Johnson Campideli Fonseca, Guilherme Elias Pessanha Henriques, Lourenço Correr Sobrinho, Mário Fernando de Góes

Dental Materials· Volume 19· Issue 7
Publisher page

Abstract

Objectives This study evaluated: (1) the marginal fit of copings fabricated from commercially pure titanium (cp Ti) and titanium-aluminum-vanadium alloy (Ti-6Al-4V) after each firing cycle for a recommended porcelain; and (2) the effectiveness of a stress-relieving treatment on the fit. The results were compared with copings made with Pd-Ag alloy submitted to the recommended porcelain firing protocol. Methods Bovine teeth were machined for metal-ceramic crowns and die casts were obtained for waxing patterns. The firing cycle of titanium porcelain was performed on cp Ti and Ti-6Al-4V copings obtained using the Rematitan System. A stress-relieving treatment (cp Ti treated and Ti-6Al-4V treated groups) was performed on original invested castings at the first porcelain firing temperature (800 degrees C). Fit (microm) was measured in the 'as cast' condition and after each porcelain firing cycle with a traveling microscope. The values were compared using the analysis of variance and Tukey's test (P<0.05), the Pd-Ag group was compared to titanium groups using Dunnett's test (P<0.05). Results The marginal fit values in the as-cast condition (initial) were 84.43 microm for Ti-6Al-4V not treated, 76.35 microm for Ti-6Al-4V treated, 86.09 microm for cp Ti not treated, 97.66 microm for cp Ti treated and 58.11 microm for Pd-Ag group. The Ti-6Al-4V, cp Ti, and Pd-Ag groups exhibit significant differences in marginal fit values when the as-cast condition (initial) was compared with those after the recommended porcelain firing protocol (by Tukey's test at 5% probability level). No significant differences were observed between stress-relieving treated and not treated groups.Significance. The firing cycles used for porcelain build-up may worsen the fit of titanium copings to values that suggest no inferences to the detriment of clinical applications.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Titanium and titanium alloys as dental materials
2. Titanium for prosthodontics applications: a review of the literature
3. Corrosion-fatigue life of commercially pure titanium and Ti–6Al–4V alloys in the different storage environments10.1067/mpr.2000.108758 ↗
4. Effect of pressure difference on the quality of titanium casting10.1177/00220345970760031001 ↗
5. Titanium dental castings, cold worked titanium restorations—yes or not?
6. Donachie · 1988
7. Effect of magnesia investments in the dental casting of pure titanium or titanium alloys10.4012/dmj.1.8 ↗
8. Marginal accuracy and geometry of cast titanium copings10.1016/0022-3913(92)90068-L ↗
9. Casting of Ti–6Al–4V alloy compared with pure Ti an Ar-arc casting machine10.1111/j.1600-0722.1995.tb00034.x ↗
10. Marginal fit changes during porcelain firing cycles10.1016/S0022-3913(05)80272-0 ↗
11. The effect of repeated firings on the margins of nonprecious ceramometals10.1016/0022-3913(84)90406-2 ↗
12. Thermal cycling distortion of metal ceramics: part I—metal collar width10.1016/0022-3913(92)90155-4 ↗
13. Evaluation of high-temperature distortion of high-palladium metal–ceramic crowns10.1067/mpr.2001.113707 ↗
14. Thermal cycling distortion of metal ceramics: part II—etiology10.1016/0022-3913(92)90331-4 ↗
15. Effects of firing cycle and surface finishing on distortion of metal ceramic castings10.1016/S0022-3913(05)80348-8 ↗
16. A review of methods and techniques to improve the fit of cast restorations10.1016/0022-3913(86)90003-X ↗
17. Effect of in vivo crown margin discrepancies on periodontal health10.1016/0022-3913(91)90225-L ↗
18. Titanium for prosthodontic applications: a review of the literature
19. Thermal distortion of different materials in crown construction10.1016/0022-3913(94)90554-1 ↗
20. Marginal fit of machined-milled titanium and cast titanium single crowns
21. Fit of titanium and a base metal alloy metal–ceramic crown10.1016/S0022-3913(00)70134-X ↗
22. Distortion of metal–ceramic fixed partial dentures resulting from metal conditioning firing
23. Creep rate of porcelain-bonding alloys as a function of temperature10.1177/00220345800590120601 ↗
24. Distortion of ceramometal fixed partial dentures during the firing cycle10.1016/0022-3913(81)90036-6 ↗
25. Creep and sag properties of porcelain–gold alloy10.1177/00220345670460032101 ↗
26. Bagby · 1985 · 31
27. Preparation design and margin distortion in porcelain-fused-to-metal restorations10.1016/0022-3913(73)90007-3 ↗
28. Bovine teeth as possible substitutes in the adhesion test10.1177/00220345830620101501 ↗