Surface fluorination of zirconia: Adhesive bond strength comparison to commercial primers

Jeffrey R. Piascik, Edward J. Swift, Krista Braswell, Brian R. Stoner

Dental Materials· Volume 28· Issue 6
Publisher page

Abstract

Objective This study evaluated contact angle and shear bond strength of three commercial zirconia primers and compared them to a recently developed fluorination pre-treatment. Earlier investigations reported that plasma fluorinated zirconia modifies the chemical bonding structure creating a more reactive surface. Materials and methods Yttria-stabilized zirconia (LAVA, 3M ESPE) plates were highly polished using 3μm diamond paste (R(a) ∼200nm) prior to pretreatments. After primer and fluorination treatment, contact angles were measured to quantify surface hydrophobicity before and after ethanol clean. Additionally, simple shear bond tests were performed to measure the adhesion strength to a composite resin. Results Plasma fluorination produced the lowest contact angle (7.8°) and the highest shear bond strength (37.3MPa) suggesting this pretreatment facilitates a more "chemically" active surface for adhesive bonding. Conclusions It is hypothesized that plasma fluorination increase hydroxylation at the surface, making it more reactive, thus allowing for covalent bonding between zirconia surface and resin cement. A strong correlation was observed between contact angle and adhesion strength for all specimens; a relationship which may help understand the frequency and modes of failures, clinically. It is also believed that this surface treatment can increase long-term viability of zirconia restorations over other adhesive techniques.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Polymer Surface Interaction Studies · Surface Modification and Superhydrophobicity

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Clinical trials in zirconia: a systematic review
2. The clinical success of all-ceramic restorations
3. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
4. Stabilized zirconia as a structural ceramic: an overview10.1016/j.dental.2007.05.005 ↗
5. Resin composite – state of the art10.1016/j.dental.2010.10.020 ↗
6. Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now?10.1016/j.dental.2010.10.022 ↗
7. Resin bond to dental ceramics, Part II: high-strength ceramics10.1111/j.1708-8240.2004.tb00061.x ↗
8. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
9. Are adhesive technologies needed to support ceramics? An assessment of the current evidence
10. Materials design of ceramic-based layer structures for crowns10.1177/154405910208100615 ↗
11. Damage and reliability of Y-TZP after cementation surface treatment10.1177/0022034510363253 ↗
12. Recent advances in ceramic for dentistry10.1177/10454411960070020201 ↗
13. Bond strength of composite luting cement to zirconia ceramic surfaces10.1016/j.dental.2005.02.005 ↗
14. Surface modification for enhanced silanation of high strength ceramics10.1016/j.dental.2009.03.008 ↗
15. Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials10.1016/S0022-3913(07)60123-1 ↗
16. Innovations in bonding to zirconia-based materials: Part I10.1016/j.dental.2008.02.010 ↗
17. Innovations in bonding to zirconia-based materials. Part II: focusing on chemical interactions10.1016/j.dental.2009.02.011 ↗
18. Bonding zirconia using a new surface treatment10.1111/j.1532-849X.2010.00575.x ↗
19. The shear bond strength between luting cements and zirconia ceramics after two pre-treatments
20. New zirconia primer improves bond strength of resin-based cements10.1016/j.dental.2009.12.005 ↗
21. Surface conditioning influences zirconia ceramic bonding10.1177/0022034509340881 ↗
22. Hydroxylation of dental surfaces: characterization and bonding potential10.1002/jbm.b.31126 ↗
23. Development of a novel surface modification for improved bonding to zirconia10.1016/j.dental.2011.01.005 ↗
24. Enhanced bonding between YSZ surfaces using a gas-phase fluorination pretreatment10.1002/jbm.b.31840 ↗
25. Characterization of plasma fluorinated zirconia for dental applications by X-ray photoelectron spectroscopy10.1016/j.apsusc.2011.07.013 ↗
26. Hydrolysis reactions at the surface of fluorizirconate glass10.1111/j.1151-2916.1988.tb05922.x ↗
27. A review of adhesion science10.1016/j.dental.2009.11.157 ↗