The repair potential of resin composite materials
Source abstract
Abstract
Objectives To measure the 'repair' strength of various combinations of composite using four manufacturers' adhesive systems, to compare the bond strengths with the cohesive strength of the original, unrepaired products and to assess whether the chemical nature of the resin matrix influenced the repair strength. Methods Specimens were prepared of three composite materials Durafill, Heraeus Kulzer; P90 (Silorane) 3M ESPE; Z250 (3M ESPE) and aged in water at 60°C for 1 month. One surface of each specimen was faced with 80-grit silicone carbide paper, one of four adhesives placed (Ecusit, DMG; Clearfil Repair, Kuraray; P90 System Adhesive; Single Bond 2, 3M ESPE) and 'repair' composite added of the same type as above, such that all combinations of original and repair composite and adhesive were used. 'Stick' samples, approximately 6 mm × 0.8 mm × 4 mm were prepared from each repair specimen, a neck created at the junction of original and repair composites and the hour-glass sample tested in tension at 1 mm/min. The microtensile bond strength of the repair was calculated and the mode of failure (adhesive; cohesive in the original composite; cohesive in the repair composite) recorded. Results There was no significant difference between the cohesive strengths of Filtek P90 and Filtek Z250 (both ≈106 MPa); both were significantly stronger than Durafill (67.0 MPa). For bonding to Durafill the bond strengths ranged from 17.6 MPa to 50.9 MPa; for bonding to P90, the bond strengths ranged from 5.0 MPa to 54.2 MPa; for bonding to Z250, the bond strengths ranged from 17.2 MPa to 75.4 MPa. Clearfil Repair appeared to provide the most consistently high bond strengths, followed by the P90 System Adhesive, Single Bond 2 and Ecusit. Overall, the majority of failures (74%) was adhesive. Significance It appears that bonding of new dimethacrylate-based composite to old dimethacrylate-based composite can be a viable clinical procedure. However, if the original composite is silorane-based (e.g., P90), then using the silane-based adhesive may be the best repair option, and similarly if it is planned to effect a repair with a silorane-based composite, using a silane-based adhesive may give the best outcome. The null hypotheses are thus rejected.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Trauma and Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Buonocore memorial lecture. Review of the clinical survival of direct and indirect restorations in posterior teeth of the permanent dentition
2. A retrospective clinical study on longevity of posterior composite and amalgam restorations10.1016/j.dental.2005.11.036 ↗
3. A long-term evaluation of alternative treatments to replacement of resin-based composite restorations: results of a seven-year study10.14219/jada.archive.2009.0098 ↗
4. Minimal intervention dentistry – a review10.1111/j.1875-595X.2000.tb00540.x ↗
5. The opinions of manufacturers of resin-based composite materials towards the repair of failing composite restorations10.1308/135576109789389487 ↗
6. Increasing the longevity of restorations by minimal intervention: a two-year clinical trial10.2341/07-113 ↗
7. Failure, repair, refurbishing and longevity of restorations
8. Repair versus replacement of defective direct composite restorations in teaching programmes in United Kingdom and Irish dental schools
9. Teaching students the repair of resin-based composite restorations: a survey of North American dental schools10.14219/jada.archive.2003.0160 ↗
10. The repair of direct composite restorations: an international survey of the teaching of operative techniques and materials10.1034/j.1600-0579.2003.00275.x ↗
11. Introduction to and outcomes of the conference on adhesion in dentistry10.1016/j.dental.2009.12.003 ↗
12. The effect of air abrasion with two new bonding agents on composite repair
13. Fatigue behavior of the resin-resin bond of partially replaced resin-based composite restorations
14. Composite-to-composite microtensile bond strength in the repair of a microfilled hybrid resin: effect of surface treatment and oxygen inhibition
15. Effect of intermediate agents and pre-heating of repairing resin on composite-repair bonds10.2341/06-105 ↗
16. Hydrolytic stability of composite repair bond10.1111/j.1600-0722.2007.00475.x ↗
17. Effect of different surface treatments on the composite–composite repair bond strength10.1007/s00784-008-0228-2 ↗
18. Initial repair bond strength of a nano-filled hybrid resin: effect of surface treatments and bonding agents10.1111/j.1708-8240.2009.00271.x ↗
19. Composite–composite repair bond strength: effect of different adhesion primers10.1016/S0300-5712(03)00093-9 ↗
20. Bonding of composite to water aged composite with surface treatments10.1016/j.dental.2006.03.010 ↗
21. Effect of physicochemical aging conditions on the composite–composite repair bond strength
22. Immediate repair bond strengths of microhybrid, nanohybrid and nanofilled composites after different surface treatments10.1016/j.jdent.2009.08.009 ↗
23. A review of adhesion science10.1016/j.dental.2009.11.157 ↗
24. Variables related to materials and preparing for bond strength testing irrespective of the test protocol10.1016/j.dental.2009.11.154 ↗
25. Relationship between bond strength tests and other in vitro phenomena10.1016/j.dental.2009.11.156 ↗
26. Relationship between bond-strength tests and clinical outcomes10.1016/j.dental.2009.11.148 ↗
27. How ‘clean’ must a cavity be before restoration?10.1159/000077770 ↗
28. Strength of posterior composite repairs using different composite/bonding agent combinations