Nanohybrid vs. fine hybrid composite in Class II cavities: Clinical results and margin analysis after four years
Source abstract
Abstract
Objectives This controlled prospective split-mouth study evaluated the clinical behavior of two different resin composites in extended Class II cavities over a period of four years. Methods Thirty patients received 68 direct resin composite restorations (Grandio bonded with Solobond M: n=36, Tetric Ceram bonded with Syntac: n=32) by one dentist in a private practice. All restorations were replacement fillings, 24 cavities (35%) revealed no enamel at the bottom of the proximal box, in 33 cavities (48%) the proximal enamel width was less than 0.5mm. The restorations were examined according to modified USPHS criteria at baseline, and after six months, one, two, and four years. At each recall, impressions were taken for replica preparation. Replicas of 44 select subjects were assessed for marginal quality under a stereo light microscope (SLM) at 130x and 22 replicas were assessed under a scanning electron microscope (SEM) at 200x. Results Both recall rate and survival rate were 100% after four years of clinical service. No significant difference was found between the restorative materials (p>0.05; Mann-Whitney U-test). Hypersensitivities were significantly reduced over time (p<0.05; Friedman test). A significant deterioration over time was found for the criteria marginal integrity (66% bravo after four years), tooth integrity (15% bravo), filling integrity (73% bravo) and proximal contact (p<0.05; Friedman test). SLM and SEM analysis of restoration margins revealed differences in the amount of perfect margins, in favor of Tetric Ceram (p<0.05). Significances Both materials performed satisfactorily over the four-year observation period. Due to the extension of the restorations, wear was clearly visible after four years of clinical service with 50% bravo ratings.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Orthodontics and Dentofacial Orthopedics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Direct posterior restorations: clinical results and new developments10.1016/S0011-8532(01)00010-6 ↗
2. Longevity of restorations in posterior teeth and reasons for failure
3. The reasons for replacement and the age of failed restorations in general dental practice10.3109/00016359709091943 ↗
4. Clinical status of ten dentin adhesive systems10.1177/00220345940730110401 ↗
5. Evidence for bacterial causation of adverse pulpal responses in resin-based dental restorations10.1177/10454411000110040501 ↗
6. Buonocore Memorial Lecture. Review of the clinical survival of direct and indirect restorations in posterior teeth of the permanent dentition
7. Manhart J, Chen HY, Hickel R. Three-year results of a randomized controlled clinical trial of the posterior composite QuiXfil in class I and II cavities. Clin Oral Investig; in press.
8. Clinical effectiveness of contemporary adhesives: a systematic review of current clinical trials10.1016/j.dental.2005.02.003 ↗
9. Single-bottle adhesives behave as permeable membranes after polymerization. I. In vivo evidence10.1016/j.jdent.2004.04.006 ↗
10. Four-year clinical evaluation of posterior resin-based composite restorations placed using the total-etch technique10.1111/j.1708-8240.2001.tb00251.x ↗
11. Two-year clinical evaluation of ormocer and nanofill composite with and without a flowable liner
12. Two-year clinical performance of a nanofiller vs a fine-particle hybrid resin composite10.1007/s00784-006-0041-8 ↗
13. Setting stress in composite resin in relation to configuration of the restoration10.1177/00220345870660110601 ↗
14. A critical review of the durability of adhesion to tooth tissue: methods and results10.1177/154405910508400204 ↗
15. Evaluation of resin composite materials. Part II. In vivo investigations
16. Totally bonded ceramic inlays and onlays after eight years
17. No-bottle vs “multi-bottle” dentin adhesives—a microtensile bond strength and morphological study10.1016/S0109-5641(00)00084-1 ↗
18. Influence of c-factor and layering technique on microtensile bond strength to dentin10.1016/j.dental.2003.08.001 ↗
19. The clinical performance of adhesives10.1016/S0300-5712(96)00070-X ↗
20. Buonocore memorial lecture. Adhesion to enamel and dentin: current status and future challenges
21. Long-term evaluation of extensive restorations in permanent teeth10.1016/S0300-5712(03)00084-8 ↗
22. A randomized controlled study evaluating the effectiveness of a two-step self-etch adhesive with and without selective phosphoric-acid etching of enamel10.1016/j.dental.2004.05.008 ↗
23. Four-year water degradation of total-etch adhesives bonded to dentin10.1177/154405910308200212 ↗
24. Self-etch vs etch-and-rinse adhesives: effect of thermo-mechanical fatigue loading on marginal quality of bonded resin composite restorations10.1016/j.dental.2004.07.005 ↗
25. Marginal integrity: is the clinical performance of bonded restorations predictable in vitro?
26. Influence of the restorative technique and new adhesives on the dentin marginal seal and adaptation of resin composite Class II restorations: an in vitro evaluation
27. Evaluation of the fatigue behavior of the resin-dentin bond with the use of different methods10.1002/jbm.b.10052 ↗
28. The effect of six years of water storage on resin composite bonding to human dentin10.1002/jbm.b.20024 ↗
29. Technique sensitivity of dentin bonding: effect of application mistakes on bond strength and marginal adaptation
30. Clinical evaluation of a nanofilled composite in posterior teeth: 12-month results10.2341/05-103 ↗
31. Hickel · J Adhes Dent · 2007 · 9 · 121
32. Buonocore memorial lecture. Evaluation of clinical performance for posterior composite resins and dentin adhesives
33. Strength and fatigue performance versus filler fraction of different types of direct dental restoratives10.1002/jbm.b.30338 ↗
34. Relative wear of flowable and highly filled composite10.1016/j.prosdent.2004.11.006 ↗
35. Effects of filler size, water, and alcohol on hardness and laboratory wear of dental composites10.1080/00016350410005555 ↗
36. Wear of dental resin composites: insights into underlying processes and assessment methods—a review10.1002/jbm.b.10563 ↗
37. In vitro evaluation of the marginal degradation of dental composites under simulated occlusal loading10.1016/S0109-5641(99)00045-7 ↗
38. Improving the completeness and transparency of reports of randomized trials in oral health: the CONSORT statement
39. Comparison of the marginal integrity of in vivo and in vitro Class II composite restorations10.1016/0300-5712(93)90026-M ↗
40. Clinical performance of posterior compomer restorations over 4 years
41. Evaluation of resin composite materials. Part I. In vitro investigations
42. The effect of finishing and polishing procedures on the surface roughness of composite resin materials10.5005/jcdp-8-1-27 ↗
43. Surface texture of four nanofilled and one hybrid composite after finishing10.2341/06-9 ↗