Effect of immediate and delayed dentin sealing on the fracture strength, failure type and Weilbull characteristics of lithiumdisilicate laminate veneers
Source abstract
Abstract
Objectives Adhesion on dentin is less reliable than on enamel, which could affect the durability of laminate veneers (LV). Immediate dentin sealing (IDS) is suggested instead of delayed dentin sealing (DDS) to overcome hypersensitivity and prevent debonding from dentin. This study evaluated the effect of IDS and DDS on the durability of Li2Si2O5 laminate veneers in vitro. Methods Window preparations were made on the labial surfaces of sound maxillary central incisors (N=50). They were randomly divided into five groups: Group 1: Enamel only+H3PO4+Adhesive (control); Group 2: <1/4 dentin+H3PO4+DDS (2 weeks later); Group 3: Complete dentin+H3PO4+DDS (2 weeks later); Group 4: <1/4 dentin+H3PO4+IDS; Group 5: Complete dentin+H3PO4+IDS. Li2Si2O5 laminate veneers (e.max Press) were bonded to the labial surfaces of the teeth with adhesive resin cement (Variolink Veneer). IDS layers were silicacoated (CoJet System) and silanized (ESPE-Sil). The teeth with their bonded laminates were thermocycled (10.000× cycles) and then subjected to static loading (1mm/min). Failure type and location after debonding were classified. Data were analyzed using ANOVA and Tukey's post hoc test (α=0.05). Two-parameter Weibull distribution values including the Weibull modulus, scale (m) and shape (0), values were calculated. Results Mean fracture strength (N) per group in descending order was as follows: Group 5 (576±254), Group 4 (478±216), Group 1 (473±159), Group 2 (465±186), and Group 3 (314±137). The presence of complete dentin exposure sealed with DDS after 2 weeks on the bonded surface (Group 3) resulted in significantly lower fracture strength results than those in group 5 with IDS (p=0.034). Weibull distribution presented higher shape (0) for Group 1 (3.67), than those of other groups (2.51-2.89). Failure types were predominantly adhesive failure between the cement and the laminate veneer in Groups 1, 2, 4 whereas Group 3 presented more often complete adhesive failures between the cement and dentin. In Group 5, failures showed some IDS and cement with or without ceramic fracture attached on the tooth. Significance When laminate veneers are bonded to a large dentin substrate, application of immediate dentin sealing improves adhesion and thereby, the fracture strength of Li2Si2O5 laminate veneers.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Erosion and Treatment
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Measurement of enamel thickness in relation to reduction for etched laminate veneers
2. An in vitro assessment of tooth preparation for porcelain veneer restorations10.1016/0300-5712(95)93574-L ↗
3. Dentin exposure in tooth preparations for porcelain veneers: a pilot study10.1016/j.prosdent.2005.08.016 ↗
4. Restoring strength of incisors with veneers and full ceramic crowns
5. A 15-year review of porcelain veneer failure-a clinician's observations
6. Porcelain laminate veneers. A retrospective evaluation after 1 to 10 years of service: Part II-clinical results
7. A prospective ten-year clinical trial of porcelain veneers
8. Midterm results of a 5-year prospective clinical investigation of extended ceramic veneers10.1016/j.dental.2007.09.009 ↗
9. Survival rates for porcelain laminate veneers with special reference to the effect of preparation in dentin: a literature review10.1111/j.1708-8240.2012.00517.x ↗
10. Dentin permeability: sealing the dentin in crown preparations
11. Dual application of dentin bonding agents: effect on bond strength
12. The dual bonding technique: a modified method to improve adhesive luting procedures
13. Porcelain veneers: dentin bonding optimization and biomimetic recovery of the crown
14. Immediate dentin sealing supports delayed restoration placement10.1016/S0022-3913(07)60052-3 ↗
15. The effect of three variables on shear bond strength when luting a resin inlay to dentin10.2341/08-82 ↗
16. The effect of immediate dentin sealing on the marginal adaptation and bond strengths of total-etch and self-etch adhesives10.1016/S0022-3913(09)00073-0 ↗
17. The influence of storage time and cutting speed on microtensile bond strength
18. Immediate dentin sealing: a fundamental procedure for indirect bonded restorations10.1111/j.1708-8240.2005.tb00103.x ↗
19. Marginal and internal adaptation of class II restorations after immediate or delayed composite placement10.1016/S0300-5712(02)00041-6 ↗
20. Effect of static and cyclic loading on ceramic laminate veneers adhered to teeth with and without aged composite restorations
21. Clinical longevity of ceramic laminate veneers bonded to teeth with and without existing composite restorations up to 40 months10.1007/s00784-012-0790-5 ↗
22. Porcelain veneers: a review of the literature10.1016/S0300-5712(99)00066-4 ↗
23. Multiple potential of etched porcelain laminate veneers10.14219/jada.archive.1987.0317 ↗
24. A prospective ten-year clinical trial of porcelain veneers
25. Clinical performance of porcelain laminate veneers for up to 20 years
26. Three-year clinical effectiveness of four total-etch dentinal adhesive systems in cervical lesions
27. The clinical performance of adhesives10.1016/S0300-5712(96)00070-X ↗
28. A critical review of the durability of adhesion to tooth tissue: methods and results10.1177/154405910508400204 ↗
29. Dentin contamination protection after mechanical preparation for veneering
30. Immediate dentin sealing improves bond strength of indirect restorations10.1016/j.prosdent.2005.10.010 ↗
31. Chiche · 1994 · 20
32. Naeije · 1998 · 39
33. Dental adhesion review: aging and stability of the bonded interface10.1016/j.dental.2007.02.009 ↗
34. Influence of the restorative technique and new adhesives on the dentin marginal seal and adaptation of resin composite Class II restorations: an in vitro evaluation
35. Effect of surface conditioning methods on the microtensile bond strength of resin composite to composite after aging conditions10.1016/j.dental.2006.11.007 ↗
36. Crack propensity of porcelain laminate veneers: a simulated operatory evaluation10.1016/S0022-3913(99)70277-5 ↗
37. Interactions between impression materials and immediate dentin sealing10.1016/S0022-3913(09)60178-5 ↗
38. The role of oxygen inhibition of a self-etch adhesive on self-cure resin composite bonding
39. Meta-analytical review of factors involved in dentin adherence10.1177/00220345010800070301 ↗
40. Thermal cycling procedures for laboratory testing of dental restorations10.1016/S0300-5712(98)00037-2 ↗
41. Meta-analytical review of parameters involved in dentin bonding10.1177/0022034511431251 ↗