journal article·2009-12Open access

Mechanical behavior of facial prosthetic elastomers after outdoor weathering

P.N. Eleni, I. Katsavou, M.K. Krokida, G.L. Polyzois, L. Gettleman

Dental Materials· Volume 25· Issue 12

Abstract

Objectives The degradation of maxillofacial prosthetic elastomers that occurs during physical weathering is usually responsible for the replacement of prostheses. In this study the mechanical behavior of 4 non-pigmented facial prosthetic elastomers, exposed to outdoor weathering for 1 year, was investigated. The hypothesis investigated was that irradiation time did not affect the properties measured. Methods The samples were exposed to solar radiation for 1 year in Thessaloniki (Greece). Three different types of polydimethyl siloxane (PDMS) and chlorinated polyethylene (CPE) samples were tested in this study. Mechanical tests (compressive-tensile) were performed using a universal type testing machine. Hardness tests were evaluated using a durometer tester. Simple mathematical models were developed to correlate the measured properties with irradiation time. The stress-strain data of compression and tensile tests were modeled using parameters such as maximum stress (sigma(max)), maximum strain (epsilon(max)), elasticity parameter (E), and non-linearity parameter (p), while the mathematical model used for hardness data involves initial hardness of materials (H(0)). Results Two of the silicone prosthetics (Elastomer 42, TechSil 25) seem to become harder and more brittle contrary to the other silicone (M 511) and chlorinated polyethylene (CPE) samples that become softer and more ductile. Duration of exposure increases these phenomena. Conclusion The effect of irradiation time on the mechanical behavior was introduced through its effect on the models' parameters. The hypothesis was rejected since changes were observed in the model parameters.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Reconstructive Facial Surgery Techniques · Dental materials and restorations · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Conference report: materials research in maxillofacial prosthetics10.1177/00220345920710081401 ↗
2. Designing a prosthesis to simulate the elastic properties of skin10.1177/0959298920050151-2004 ↗
3. Physical properties of a silicone prosthetic elastomer stored in simulated skin secretions10.1016/S0022-3913(00)70017-5 ↗
4. Comparison of mechanical properties of Cosmesil M511 and a-2186 maxillofacial silicone elastomers
5. Adhesive retention of silicone and chlorinated polyethylene for maxillofacial prostheses10.1016/S0022-3913(08)60113-4 ↗
6. Materials and techniques in maxillofacial prosthodontic rehabilitation10.1016/S1042-3699(02)00018-3 ↗
7. Facial prosthetic rehabilitation: preprosthetic surgical techniques and biomaterials10.1097/01.moo.0000172805.48758.0c ↗
8. Evaluation of mechanical properties of Zy-1 maxillofacial prosthetic materials
9. A study of some mechanical properties of an Rtv polydimethylsiloxane for extraoral maxillofacial prostheses10.1016/0267-6605(92)90006-F ↗
10. Thermo-mechanical analysis of dental silicone polymers10.1007/s10853-006-0852-7 ↗
11. Crystallization of Pdms: the effect of physical and chemical crosslinks10.1209/epl/i2002-00276-4 ↗
12. Modification of polysiloxane polymers for biomedical applications: a review10.1002/pi.783 ↗
13. Evaluation of cross-linking after accelerated photo-ageing of silicone rubber10.1002/pi.1329 ↗
14. Thermooxidative degradation of poly(vinyl chloride)/chlorinated polyethylene blends investigated by thermal analysis methods10.1016/j.polymdegradstab.2003.08.012 ↗
15. The use of optical microscopy to follow the degradation of isotactic polypropylene (Ipp) subjected to natural and accelerated ageing10.1016/j.polymertesting.2005.07.009 ↗
16. In vitro evaluation of color change in maxillofacial elastomer through the use of an ultraviolet light absorber and a hindered amine light stabilizer
17. The effects of [gamma]-radiation on the thermal, mechanical, and segmental dynamics of a silica filled. Room temperature vulcanized polysiloxane rubber10.1016/S0141-3910(03)00028-4 ↗
18. Comparison of UV degradation chemistry in accelerated (xenon) aging tests and outdoor tests (Ii)10.1016/0141-3910(94)90110-4 ↗
19. Physical properties of three maxillofacial materials as a function of accelerated aging10.1016/0022-3913(94)90098-1 ↗
20. Interactions of pigments and opacifiers on color stability of Mdx4-4210/type a maxillofacial elastomers subjected to artificial aging10.1016/j.prosdent.2005.12.006 ↗
21. Degradation profile of polyethylene after artificial accelerated weathering10.1016/S0141-3910(02)00338-5 ↗
22. Importance of weathering factors other than UV radiation and temperature in outdoor exposure10.1016/S0141-3910(02)00049-6 ↗
23. Factors affecting accelerated testing of polymer photostability10.1016/j.polymdegradstab.2005.01.049 ↗
24. An elastomeric material for facial prostheses: synthesis, experimental and numerical testing aspects10.1016/S0142-9612(03)00412-5 ↗
25. The uniaxial stress versus strain response of pig skin and silicone rubber at low and high strain rates10.1016/j.ijimpeng.2004.11.010 ↗
26. Polyurethane elastomers studied by the Mooney-Rivlin equation for rubbers10.1002/app.1991.070430323 ↗
27. Color stability of facial silicone prosthetic polymers after outdoor weathering10.1016/S0022-3913(99)70032-6 ↗
28. Color stability and colorant effect on maxillofacial elastomers. Part Iii. Weathering effect on color10.1016/S0022-3913(99)80010-9 ↗
29. Accelerated aging and lifetime prediction: review of non-Arrhenius behaviour due to two competing processes10.1016/j.polymdegradstab.2005.05.004 ↗
30. Weibull models for the statistical analysis of dental composite data: aged in physiologic media and cyclic-fatigued10.1016/0109-5641(91)90022-Q ↗
31. Statistical aspects of lifetime in the presence of UV radiation10.1115/1.1498263 ↗
32. Color stability of facial silicone prosthetic elastomers after artificial weathering
33. Structural damages of maxillofacial biopolymers under solar aging10.1007/s10856-007-3027-4 ↗
34. The effect of artificial accelerated weathering on the mechanical properties of maxillofacial polymers Pdms and Cpe10.1088/1748-6041/4/3/035001 ↗
35. ASTM. D395-03, Standard Test Methods for Rubber Property—Compression Set. 2003.
36. ASTM. D412-05, Tension Test for Vulcanized Rubber and Thermoplastic Elastomers.
37. ASTM. D2240-05, Standard Test Method for Rubber Property—Durometer Hardness.
38. Roesler · 2007
39. Krokida · 2000
40. Viscoelastic behaviour of dehydrated products during rehydration10.1016/S0260-8774(99)00063-1 ↗
41. Weathering of polymers: mechanisms of degradation and stabilization, testing strategies and modelling10.1007/BF00445969 ↗
42. Rabek · 1995
43. Aging processes in pharmaceutical polymers10.1016/S1461-5347(99)00210-2 ↗
44. An assessment of recent advances in external maxillofacial materials10.1016/0022-3913(80)90215-2 ↗
45. Dynamic mechanical thermal analysis of maxillofacial elastomers10.1016/S0022-3913(97)90000-7 ↗
46. Shah H, Munisamy S, Vaidyanathan TK. Artificial aging of chlorinated polyethylene and maxillofacial silicone elastomer. IADR 86th General Session & Exhibition 2008.
47. Kroschwitz · 2005