journal article·2010-01

Comparison of edge chipping resistance of PFM and veneered zirconia specimens

Janet B. Quinn, Veeraraghavan Sundar, Edward E. Parry, George D. Quinn

Dental Materials· Volume 26· Issue 1
Publisher page

Abstract

Objectives To investigate the chipping resistance of veneered zirconia specimens and compare it to the chipping resistance of porcelain fused to metal (PFM) specimens. Methods Veneered zirconia and PFM bar specimens were prepared in clinically relevant thicknesses. The specimen edges were chipped with different magnitude forces, producing chips of various sizes. The range of sizes included small chips that did not penetrate all the way through the veneers to the substrates, and also chips that were very large and reached the zirconia or metal substrates. The relationship between force magnitude and chip size (edge distance) was graphed. The resulting curves were compared for the veneered zirconia and PFM specimens. Knoop hardness vs. force graphs for the veneers and substrates were also obtained. Results The zirconia and PFM veneer chipping data followed a power law (coefficient of determination, R(2)>0.93) as expected from the literature. The curves overlapped within the combined data scatter, indicating similar resistance to chipping. The chips made in both types of specimens detached and did not penetrate into the substrate when they reached the veneer/substrate intersections. The hardness-load curves for the veneers and substrates all exhibited an indentation size effect (ISE) at low loads. The Knoop hardness values with uncertainties of +/-one standard deviation at 4N loads for the metal, zirconia, and the metal and zirconia veneers are: (2.02+/-0.08, 12.01+/-0.39, 4.24+/-0.16 and 4.36+/-0.02GPa), respectively, with no statistically significant difference between the veneers (Tukey pairwise comparison at 0.95 family confidence). Significance This work indicates that a similar resistance to chipping might be expected for veneered zirconia and PFM restorations, in spite of the large difference in substrate hardness. Differences in susceptibility to chip spalling were not detected, but the chips in both specimen types detached off the sides in a similar manner instead of extending into the substrates.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Research on bioceramics
2. Subbarao · 1981
3. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
4. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
5. Clinical behavior of zirconia based bridges: two-years results
6. Outcome of posterior FPDs of veneered zirconia ceramic (Cercon)
7. All-ceramic fixed partial dentures designed according to the DC-Zirkon® technique: a 2-year clinical study10.1111/j.1365-2842.2004.01437.x ↗
8. 5-Jahres-Ergebnisse—Bewährung von vollkeramischen Brücken aus DC-Zirkon®
9. Clinical long-term behavior of zirconia-based bridges (LAVA): five years results
10. 3-Year results of zirconia posterior fixed partial dentures made by Direct Ceramic Machining, (DCM)
11. Trends in materials science from the point of view of a practicing dentist10.1016/j.jeurceramsoc.2008.08.014 ↗
12. Resistance to fracture of two all-ceramic crown materials following endodontic access10.1016/j.prosdent.2005.11.003 ↗
13. Porcelain esthetics for the 21st century10.14219/jada.archive.2000.0402 ↗
14. ISO TC 106/SC 2, Dental Ceramic, ISO 6872, 1995.
15. Edge flaking of brittle materials
16. Edge flaking as a measure of material performance
17. Edge chipping of hard materials10.1016/S0263-4368(01)00030-0 ↗
18. How to design with brittle materials against edge flaking
19. “Edge toughness” and material properties related to the machining of dental ceramics10.1080/10940340008945711 ↗
20. Quinn · 2001
21. Flake and scratch size ratios in ceramics. Fractography of glasses and ceramics IV
22. Scratch hardness and chipping of dental ceramics under different environments10.1016/S0109-5641(03)00018-6 ↗
23. Geometry of edge chips formed at different angles10.1002/9780470291221.ch11 ↗
24. Edge strength of resin-composite margins10.1016/j.dental.2007.04.006 ↗
25. Edge-strength of flowable resin-composites10.1016/j.jdent.2007.10.006 ↗
26. Fractography of edge chipping. Fractography of glasses and ceramics IV, Varner JR, Quinn GD, editors. Ceramic transactions, vol. 122, Westerville, OH: American Ceramic Society; 2001. pp. 57–72.
27. Fracture barrier estimation by the edge fracture test method10.1016/j.ceramint.2008.10.026 ↗
28. A universal relation for edge chipping from sharp contacts in brittle materials: a simple means of toughness evaluation10.1016/j.actamat.2006.10.061 ↗
29. The influence of microstructure on the microhardness of ceramic materials
30. The indentation load/size effect and the measurement of the hardness of vitreous silica10.1016/S0022-3093(05)80492-2 ↗
31. Indentation brittleness of ceramics: a fresh approach10.1023/A:1018671823059 ↗
32. C1326 · 1999
33. Role of core support material in veneer failure of brittle layer structures10.1002/jbm.b.30712 ↗
34. Design maps for failure of all-ceramic layer structures in concentrated cyclic loading10.1016/j.actamat.2006.11.042 ↗
35. Influence of microstructure and chemistry on the fracture toughness of dental ceramics10.1016/S0109-5641(03)00002-2 ↗
36. Point of care: what measures can the clinician take to ensure the clinical success of metal-free (all-ceramic) crowns and bridges?
37. Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites10.1016/j.dental.2008.09.003 ↗
38. Unstable cracking (chipping) of veneer porcelain in all-ceramic crowns and fixed partial dentures10.1016/j.actbio.2008.12.016 ↗
39. Cracking and the indentation size effect for Knoop hardness of glasses10.1111/j.1151-2916.2003.tb03319.x ↗
40. Indentation size effects for glasses: yes, there is a fracture contribution
41. Evaluation of ISO9693 bond tests with zirconia ceramics
42. Bond strength of porcelain to yttria-stabilized tetragonal zirconia framework
43. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗