Abstract

Objectives High-strength ceramics for dental restoration are used as an understructure (core) that subsequently is covered by veneering ceramic. The veneering process involves a firing procedure at high temperatures at least once, usually two to five times. The aim of this study was to investigate whether these firing procedures affect the mechanical properties of a zirconia ceramic. Methods Thirty-three specimens of an industrially sintered yttria-stabilized zirconia ceramic (DC Zircon, DCS Dental AG, Allschwil, Switzerland) were cut into bars (1.2mmx4mmx20mm). One set of specimens (n=13) remained untreated (controls). Another set of specimens (n=10) was heat-treated once, corresponding to the first step of the veneering process. The third set of specimens (n=10) was heat-treated five times to mimic the full veneering process. Flexural strength, microhardness, dimensions and surface roughness were measured. The fracture patterns were assessed by light microscopy. Results The untreated specimens showed a statistically significant higher flexural strength (20%) and microhardness (9%) than both of the test groups (p< or =0.001). No significant differences were found for fracture patterns, dimensions or surface roughness. Significance The heat treatment associated with the veneering procedure on a zirconia core material reduced the flexural strength of the core after the first firing. Subsequent firings were not detrimental to the properties measured.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Anatomy and Medical Technology · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Influence of firing cycles on the margin distortion of 3 all ceramic crown systems10.1016/j.prosdent.2005.02.003 ↗
2. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic10.1016/j.jdent.2004.07.001 ↗
3. The influence of multiple firing on thermal contraction of ceramic materials used for the fabrication of layered all-ceramic dental restorations10.1016/j.dental.2004.08.006 ↗
4. The effect of veneering and heat treatment on the flexural strength of Empress 2 ceramics10.1016/S0300-5712(02)00013-1 ↗
5. Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing10.1016/j.dental.2004.07.013 ↗
6. Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia10.1016/j.biomaterials.2005.11.021 ↗
7. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
8. International standard ISO 6872. Dental ceramics; 1995.
9. Hull · 1999
10. Fracture-surface analysis of dental ceramics10.1016/0022-3913(89)90075-9 ↗
11. Influence of grinding, sandblasting, polishing and heat treatment on the flexural strength of a glass-infiltrated alumina-reinforced dental ceramic10.1016/j.biomaterials.2003.08.056 ↗
12. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
13. Strength and reliability of surface treated Y-TZP dental ceramics10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
14. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗
15. Reliability and properties of ground Y-TZP-zirconia ceramics10.1177/154405910208100711 ↗
16. CAD/CAM-machining effects on Y-TZP zirconia10.1016/j.dental.2003.08.007 ↗
17. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic10.1016/j.jdent.2005.06.006 ↗
18. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
19. Prevention of low-temperature surface transformation by surface recrystallization in yttria-doped tetragonal zirconia10.1111/j.1151-2916.1989.tb06124.x ↗
20. Hummel · 2004
21. Grain-boundary resistivity in zirconia-based materials—effect of sintering temperatures and impurities10.1016/0167-2738(94)00236-L ↗
22. Fatigue and static crack propagation in yttria-stabilized tetragonal zirconia polycrystals: crack growth micromechanisms and precracking effects10.1111/j.1151-2916.1997.tb03192.x ↗
23. Instrumented micro-indentation of zirconia ceramics10.1111/j.1151-2916.2000.tb01500.x ↗
24. Cyclic fatigue in water of veneer-framework composites for all-ceramic dental bridges10.1016/j.dental.2006.01.011 ↗
25. Mechanical and fracture behavior of veneer-framework composites for all-ceramic dental bridges10.1016/j.dental.2005.12.009 ↗
26. Characterization of damage modes in dental ceramic bilayer structures10.1002/jbm.10091 ↗
27. The influence of interfacial surface roughness on bilayered ceramic specimen performance10.1016/S0109-5641(03)00085-X ↗
28. Strength, reliability, and mode of fracture of bilayered porcelain/core ceramics
29. The effect of core:dentin thickness ratio on the bi-axial flexure strength and fracture mode and origin of bilayered dental ceramic composites10.1016/j.dental.2004.01.005 ↗
30. The in vitro failure of all-ceramic crowns and the connector area of fixed partial dentures using bilayered ceramic specimens: the influence of core to dentine thickness ratio10.1016/j.dental.2005.11.005 ↗
31. Fractographic analyses of three ceramic whole crown restoration failures10.1016/j.dental.2005.01.006 ↗
32. Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling10.1177/00220345950740060301 ↗
33. Fracture surface analysis of clinically failed fixed partial dentures10.1177/154405910608500314 ↗